New ACI Document on Statistical Techniques for Assessment of Existing Concrete Structures

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: New ACI Document on Statistical Techniques for Assessment of Existing Concrete Structures

Author(s): Peter Barlow, Nicholas R. Triandafilou, and F. Michael Bartlett

Publication: Concrete International

Volume: 47

Issue: 4

Appears on pages(s): 41-46

Keywords: method, strength, test, example

DOI: 10.14359/51746693

Date: 4/1/2025

Abstract:
In August 2024, ACI published ACI PRC-ITG-11-24: Statistical Techniques for Assessment of Existing Concrete Structures—Report. This document, prepared by Innovation Task Group 11, which was created by the ACI Technical Activities Committee, provides information on using statistical techniques to evaluate condition and reliability of concrete structures and assessing possible repair options.

Related References:

1. ACI Committee 562, “Assessment, Repair, and Rehabilitation of Existing Concrete Structures—Code and Commentary (ACI CODE-562-25),” American Concrete Institute, Farmington Hills, MI, 2025, 133 pp.

2. ACI Innovation Task Group 11 website, www.concrete.org/committees/directoryofcommittees/acommitteehome.aspx?committee_code=C0009311, accessed Nov. 6, 2024.

3. ACI Innovation Task Group 11, “Statistical Techniques for Assessment of Existing Concrete Structures—Report (ACI PRC-ITG-11-24),” American Concrete Institute, Farmington Hills, MI, 2024, 47 pp.

4. Larsen, R.J., and Marx, M.L., An Introduction to Mathematical Statistics and Its Applications, sixth edition, Prentice Hall, Upper Saddle River, NJ, 2017, 752 pp.

5. ASTM E122-17(2022), “Standard Practice for Calculating Sample Size to Estimate, with Specified Precision, the Average for a Characteristic of a Lot or Process,” ASTM International, West Conshohocken, PA, 2022, 5 pp.