Shear Strengthening of Hollow-Core Slabs with Structural Openings

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Shear Strengthening of Hollow-Core Slabs with Structural Openings

Author(s): Ahmed F. Elkhouly, Mohammed H. Hedia, and George Morcous

Publication: Concrete International

Volume: 47

Issue: 3

Appears on pages(s): 55-59

Keywords: strength, test, load, capacity

DOI: 10.14359/51745651

Date: 3/1/2025

Abstract:
Hollow-core (HC) slabs are precast/prestressed concrete members with continuous voids oriented parallel to the span of the slabs. Openings in HC slabs are one of the most common challenges encountered during construction. This study experimentally evaluated the effectiveness of proposed strengthening methods for HC slabs with unforeseen structural openings.

Related References:

1. Hawkins, N.M., and Ghosh, S.K., “Shear Strength of Hollow-Core Slabs,” PCI Journal, V. 51, No. 1, Jan.-Feb. 2006, pp. 110-115.

2. MNL-126-15, PCI Manual for the Design of Hollow Core Slabs and Walls, third edition, Precast/Prestressed Concrete Institute, Chicago, IL, 2015.

3. Pajari, M., “Resistance of Prestressed Hollow Core Slabs Against Web Shear Failure,” VTT Research Notes 2292, VTT Technical Research Centre of Finland, Espoo, Finland, 2005, 68 pp.

4. Truderung, K.A.; El-Ragaby, A.; Mady, M.; and El-Salakawy, E., “Shear Capacity of Dry-Cast Extruded Precast, Prestressed Concrete Hollow-Core Slabs,” PCI Journal, V. 64, No. 4, July-Aug. 2019, pp. 71-83.

5. Palmer, K.D., and Schultz, A.E., “Experimental Investigation of the Web-Shear Strength of Deep Hollow-Core Units,” PCI Journal, V. 56, No. 4, Fall 2011, pp. 83-104.

6. Tawadrous, R., and Morcous, G., “Shear Strength of Deep Hollow-Core Slabs,” ACI Structural Journal, V. 115, No. 3, May 2018, pp. 699-709.

7. El-Khouly, A.F.; Meleka, N.N.; Tayel, M.A.; and Heiza, K.M., “Behavior of Precast Prestressed Hollow Core Slabs with Openings: Experimental Study,” Engineering Research Journal, V. 40, No. 4, Oct. 2017, pp. 325-329.

8. Pinheiro, G.; Júnior, A.M.; Schultz, A.; Silva, I.; Arroyo, F.N.; Aquino, V.; Ferreira, M.; Carvalho, R.; Santos, H.; Christoforo, A.; and Almeida Filho, F., “Shear Behavior of Prestressed Hollow Core One-Way Slabs with Openings: Experimental, Numerical, and Standard Formulation Verification,” Buildings, V. 13, No. 7, July 2023, 18 pp.

9. Pachalla, S.K.S., and Prakash, S.S., “Efficient Near Surface Mounting CFRP Strengthening of Pretensioned Hollowcore Slabs with Opening – An Experimental Study,” Composite Structures, V. 162, Feb. 2017, pp. 28-38.

10. Pachalla, S.K.S., and Prakash, S.S., “Experimental Evaluation on Effect of Openings on Behavior of Prestressed Precast Hollow-Core Slabs,” ACI Structural Journal, V. 114, No. 2, Mar.-Apr. 2017, pp. 427-436.

11. Pachalla, S.K.S., and Prakash, S.S., “Load Resistance and Failure Modes of Hollow-Core Slabs with Openings: A Finite Element Analysis,” PCI Journal, V. 63, No. 4, July-Aug. 2018, pp. 25-40.

12. ACI Committee 318, “Building Code Requirements for Structural Concrete and Commentary (ACI CODE-318-19) (Reapproved 2022),” American Concrete Institute, Farmington Hills, MI, 2019, 624 pp.