Title: DCC Best Practices in Decorative Concrete: Sealing Stamped Concrete

Author(s):

Publication: Concrete International

Volume: 47

Issue: 3

Appears on pages(s): 60-61

Keywords:

DOI: 10.14359/51745650

Date: 3/1/2025

Abstract:
The American Society of Concrete Contractors (ASCC) Decorative Concrete Council (DCC) provides best practices for sealing stamped concrete, including sealer types, surface preparation, application, and maintenance.