Concrete Q&A: Leveled versus Manual Straightedge

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Concrete Q&A: Leveled versus Manual Straightedge

Author(s):

Publication: Concrete International

Volume: 46

Issue: 12

Appears on pages(s): 96

Keywords: test, floor, type, requirements

DOI: 10.14359/51744365

Date: 12/1/2024

Abstract:
This Q&A focuses on comparison of a level straightedge used when performing ASTM E1155 or ASTM E1486 testing versus a manual straightedge used in the manual straightedge method described in ACI 117-10(15). Additional information on requirements related to performing the manual straightedge method is also provided.

Related References:

1. ASTM E1155-23, “Standard Test Method for Determining FF Floor Flatness and FL Floor Levelness Numbers,” ASTM International, West Conshohocken, PA, 2023, 8 pp.

2. ASTM E1486-14 (Reapproved 2022), “Standard Test Method for Determining Floor Tolerances Using Waviness, Wheel Path and Levelness Criteria (Metric),” ASTM International, West Conshohocken, PA, 2014, 12 pp.

3. ACI Committee 117, “Specification for Tolerances for Concrete Construction and Materials (ACI 117-10) and Commentary (ACI 117R-10) (Reapproved 2015),” American Concrete Institute, Farmington Hills, MI, 76 pp.




  