Case Study: Garage Floor Renovation

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Case Study: Garage Floor Renovation

Author(s):

Publication: Concrete International

Volume: 46

Issue: 9

Appears on pages(s): 52-53

Keywords: repair, renovation, hydrodemolition, bond

DOI: 10.14359/51742215

Date: 9/1/2024

Abstract:
While it might seem that hydrodemolition is only appropriate for big projects, it can also be an economical choice for compact applications, such as the renovation of a residential garage floor. The floor had heavy damage that required recasting with new concrete. The floor was diamond ground, so the hydrodemolition method was well-suited to create a rough, consistent bonding surface for the new concrete.




  