Study on Pore Characteristics of Microfoam Concrete Based on Different Mixing Ratios

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Study on Pore Characteristics of Microfoam Concrete Based on Different Mixing Ratios

Author(s): C. Jin, N. Jiang, H. Li, C. Liu, A. Cao, J. Wang, and X. Wen

Publication: Materials Journal

Volume: 121

Issue: 3

Appears on pages(s): 17-28

Keywords: fractal dimension; porosity; recycled micro powder

DOI: 10.14359/51740703

Date: 5/1/2024

Abstract:
The use of construction waste to prepare recycled micro powder can improve the use of construction waste resources and effectively reduce carbon emissions. In this paper, researchers used waste concrete processing micro powder to prepare foam concrete (FC) and quantitatively characterized the performance and pore structure of FC by scanning electron microscopy (SEM), pore and fissure image recognition and analysis system (PCAS), and mechanical property testing methods with different mixing ratios of micro powder. The results showed that the effect of single mixing of micro powder or fly ash is better than the composite mixing test, and the optimal proportion of compressive strength of single mixing of micro powder is higher than that of single mixing of fly ash. The optimum mixing ratio is 6:4 between cement and micro powder, and the best effect is achieved when the micro powder mixing amount is 40%. Single or double mixing can fill the pores between the foam and strengthen the performance of the substrate. The tests of single-mixed or compound-mixed micro powder showed that the fractal dimension decreased with the increase of porosity; when the fractal dimension of the specimen increased, the average shape factor became smaller, the compressive strength decreased, and the water absorption rate increased.

Related References:

1. Tingting, X.; Ningshan, J.; Lianxin, L.; Lin, G.; and Peng, W., “Study on the Effect of External Additives on the Strength and Dry Density of Foam Concrete,” Journal of Qinghai University, V. 31, No. 6, 2013, pp. 19-23.

2. Othuman Mydin, M. A., and Wang, Y. C., “Structural Performance of Lightweight Steel-Foamed Concrete-Steel Composite Walling System under Compression,” Thin Wall Structures, V. 49, No. 1, 2011, pp. 66-76. doi: 10.1016/j.tws.2010.08.007

3. British Cement Association, “Foam Concrete – Composition and Properties,” Camberley, UK, 1994, 4 pp.

4. Dransfield, J. M., “Foam Concrete: Properties, Applications and Potential,” Foam Concrete: An Introduction to the Product and Its Properties, One Day Awareness Seminar, University of Dundee, Dundee, UK, 2000, pp. 1-11.

5. Jones, M. R., and McCarthy, A., “Preliminary Views on the Potential of Foamed Concrete as a Structural Material,” Magazine of Concrete Research, V. 57, No. 1, 2005, pp. 21-31. doi: 10.1680/macr.2005.57.1.21

6. Huang, H.; Gong, N.; Mu, C.; Zhou, H.; and Liu, W., “Dynamic Mechanical Properties and Constitutive Relationship of Foam Concrete,” Jianzhu Cailiao Xuebao, V. 23, No. 2, 2020, pp. 466-472. (in Chinese)

7. Visagie, M., and Kearsly, E. P., “Properties of Foamed Concrete as Influenced by Air-Void Parameters,” Concrete Beton, V. 101, 2002, pp. 8-14.

8. Nambiar, E. K. K., and Ramamurthy, K., “Air-Void Characterisation of Foam Concrete,” Cement and Concrete Research, V. 37, No. 2, 2007, pp. 221-230. doi: 10.1016/j.cemconres.2006.10.009

9. Pang, C. M., and Wang, S., “Void Characterization and Effect on Properties of Foam Concrete,” Journal of Building Materials, V. 20, No. 1, 2017, pp. 93-98. (in Chinese)

10. Zhang, X.; Wang, W.; Yang, D.; and Zhang, L., “Characteristic on Pore Structure of Foamed Concrete and Study Development of its Effecting Factors,” China Concrete and Cement Products, No. 7, 2018, pp. 63-68. (in Chinese)

11. Hilal, A. A.; Thom, N. H.; and Dawson, A. R., “On Entrained Pore Size Distribution of Foamed Concrete,” Construction and Building Materials, V. 75, 2015, pp. 227-233. doi: 10.1016/j.conbuildmat.2014.09.117

12. Fang, Y.; Wang, R.; Pang, E.; and Yue, Z., “Relationship Between Compressive Strength and Pore Structure of Cement-Fly Ash Foam Concrete,” Journal of Silicates, V. 38, No. 4, 2010, pp. 621-626. (in Chinese)

13. Liu, M., “Research on the Performance of Recycled Powder Foam Concrete,” dissertation, Yangzhou University, Yangzhou, China, 2021. (in Chinese)

14. Nan, H., “Application of Fly Ash Concrete and its Long-Term Significance,” Building Materials Technology and Application, No. 4, 2010, pp. 23-24. (in Chinese)

15. JC/T 2199-2013, “Foam Agent for Foam Concrete,” Standardization Administration of China, Beijing, China, 2013. (in Chinese)

16. GB/T 17671-2021, “Test Method for Strength of Cementitious Sand (ISO Method),” Standardization Administration of China, Beijing, China, 2021. (in Chinese)

17. Zhang, J., “Research on the Preparation and Performance of Recycled Micronized Foam Concrete,” Qinghai University, Qinghai, China, 2020. (in Chinese)

18. JG/T 266-2011, “Foam Concrete,” Standardization Administration of China, Beijing, China, 2011. (in Chinese)

19. JGJ/T 341-2014, “Technical Specification for Application of Foam Concrete,” Standardization Administration of China, Beijing, China, 2014. (in Chinese)

20. Wang, Q., “Fractal Theory and its Application in Hydrology,” Shanxi Water Resources Science and Technology, No. 3, 2003, pp. 21-23. (in Chinese)

21. Liu, P.; Liu, W.; and Xu, H., “Quantitative Evaluation of Dolomite Dissolution Pore Structure Based on SEM and PCAS,” Geological Hazards and Environmental Protection, V. 34, No. 1, 2023, pp. 59-63. (in Chinese)

22. Wei, J.; Yu, Q.; Zeng, X.; and Bai, R., “Study on the Fractal Dimension of Pore Structure in Concrete,” Journal of South China University of Technology, No. 2, 2007, pp. 121-124.


ALSO AVAILABLE IN:

Electronic Materials Journal