Hysteresis Behavior of Glass Fiber-Reinforced Polymer- Reinforced Precast Concrete Tunnel Segments under Cyclic Load

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Hysteresis Behavior of Glass Fiber-Reinforced Polymer- Reinforced Precast Concrete Tunnel Segments under Cyclic Load

Author(s): Basil Ibrahim, Salaheldin Mousa, Hamdy M. Mohamed, and Brahim Benmokrane

Publication: Structural Journal

Volume: 121

Issue: 3

Appears on pages(s): 83-96

Keywords: deformability; glass fiber-reinforced polymer (GFRP) bars; high-strength concrete (HSC); hysteresis behavior; normal-strength concrete (NSC); precast concrete tunnel lining (PCTL) segments; quasistatic cyclic flexural loading

DOI: 10.14359/51740480

Date: 5/1/2024

Abstract:
The hysteresis response of precast concrete tunnel lining (PCTL) segments reinforced internally with fiber-reinforced polymer (FRP) bars under quasi-static cyclic flexural loading is an area for which no experimental research results are available. This paper reports on an investigation on the hysteresis behavior of PCTL segments reinforced internally with glass fiber-reinforced polymer (GFRP) bars. Full-scale curvilinear GFRP-reinforced PCTL segments were designed, fabricated, and tested under quasi-static cyclic flexural loading. The segments measured 3100 mm (122 in.) in length, 1500 mm (59 in.) in width, and 250 mm (9.8 in.) in thickness. The test parameters were the longitudinal reinforcement ratio, the transverse reinforcement configuration, and the concrete compressive strength. The hysteresis response, cracking pattern, and ductility of the PCTL segments were identified and experimentally evaluated. The experimental results of the current study demonstrate that the hysteresis response of the curvilinear GFRP-reinforced PCTL segments had stable cyclic behavior with no or limited strength degradation until failure. In addition, analytical prediction of the load-carrying capacity, deflection, and unloading stiffness of the test segments was carried out. The segments’ analytically predicted responses were validated and compared to the experimental results. The segments’ analytically predicted models for the post-cracking loading tangent stiffness and unloading stiffness for the curvilinear GFRP-reinforced PCTL segments are proposed herein. The analytically predicted hysteresis response shows accurate predictions with comparable loading stiffness, unloading stiffness, and residual deformation at the end of each loading cycle.

Related References:

Abbas, S., 2014, “Structural and Durability Performance of Precast Segmental Tunnel Linings,” doctoral dissertation, Western University, London, ON, Canada.

Al-Saadi, N. T. K.; Mohammed, A.; Al-Mahaidi, R.; and Sanjayan, J., 2019, “A State-of-the-Art Review: Near-Surface Mounted FRP Composites for Reinforced Concrete Structures,” Construction and Building Materials, V. 209, pp. 748-769. doi: 10.1016/j.conbuildmat.2019.03.121

ACI Committee 374, 2013, “Guide for Testing Reinforced Concrete Structural Elements under Slowly Applied Simulated Seismic Loads (ACI 374.2R-13),” American Concrete Institute, Farmington Hills, MI, 18 pp.

ACI Committee 440, 2015, “Guide for the Design and Construction of Structural Concrete Reinforced with Fiber-Reinforced Polymer (FRP) Bars (ACI 440.1R-15),” American Concrete Institute, Farmington Hills, MI.

ACI Committee 440, 2022, “Building Code Requirements for Structural Concrete Reinforced with Glass Fiber-Reinforced Polymer (GFRP) Bars—Code and Commentary (ACI CODE-440.11-22),” American Concrete Institute, Farmington Hills, MI, 260 pp.

ACI Committee 544, 2016, “Report on Design and Construction of Fiber-Reinforced Precast Concrete Tunnel Segments (ACI 544.7R-16),” American Concrete Institute, Farmington Hills, MI, 36 pp.

ASTM D7205/D7205M-21, 2021, “Standard Test Method for Tensile Properties of Fiber Reinforced Polymer Matrix Composite Bars,” ASTM International, West Conshohocken, PA.

Benmokrane, B.; Mousa, S.; Mohamed, K.; and Sayed-Ahmed, M., 2021, “Physical, Mechanical, and Durability Characteristics of Newly Developed Thermoplastic GFRP Bars for Reinforcing Concrete Structures,” Construction and Building Materials, V. 276, p. 122200. doi: 10.1016/j.conbuildmat.2020.122200

Caratelli, A.; Meda, A.; Rinaldi, Z.; and Spagnuolo, S., 2016, “Precast Tunnel Segments with GFRP Reinforcement,” Tunnelling and Underground Space Technology, V. 60, pp. 10-20. doi: 10.1016/j.tust.2016.07.011

Caratelli, A.; Meda, A.; Rinaldi, Z.; Spagnuolo, S.; and Maddaluno, G., 2017, “Optimization of GFRP Reinforcement in Precast Segments for Metro Tunnel Lining,” Composite Structures, V. 181, pp. 336-346. doi: 10.1016/j.compstruct.2017.08.083

CAN/CSA-S806-12, 2012, “Design and Construction of Building Components with Fiber-Reinforced Polymers (Reapproved 2017),” CSA Group Toronto, ON, Canada.

CAN/CSA-S6-19, 2019, “Canadian Highway Bridge Design Code,” CSA Group, Toronto, ON, Canada.

Davis, J. R., 2000, “Corrosion: Understanding the Basics,” ASM International, The Materials Information Society, Materials Park, OH, 571 pp. 

Ding, L.; Wu, G.; Yang, S.; and Wu, Z., 2013, “Performance Advancement of RC Columns by Applying Basalt FRP Composites with NSM and Confinement System,” Journal of Earthquake and Tsunami, V. 7, No. 2, p. 1350007. doi: 10.1142/S1793431113500073

Dong, Z.; Zhang, P.; Zhu, H.; Wu, G.; and Wu, Z., 2016, “Study on Stiffness and Recoverability of Fiber Reinforced Polymers-Reinforced Concrete (FRP-RC) Composite T-Beams with Prefabricated Basalt Fiber-Reinforced Polymers Shell,” Journal of Reinforced Plastics and Composites, V. 35, No. 6, pp. 516-529. doi: 10.1177/0731684415618019

Fahmy, M. F.; Wu, Z.; and Wu, G., 2009, “Seismic Performance Assessment of Damage-Controlled FRP-Retrofitted RC Bridge Columns Using Residual Deformations,” Journal of Composites for Construction, ASCE, V. 13, No. 6, pp. 498-513. doi: 10.1061/(ASCE)CC.1943-5614.0000046

Faza, S. S., and Gangarao, H. V., 1993, “Theoretical and Experimental Correlation of Behavior of Concrete Beams Reinforced with Fiber Reinforced Plastic Rebars,” Fiber-Reinforced-Plastic Reinforcement for Concrete Structures—International Symposium, SP-138, A. Nanni and C. W. Dolan, eds., American Concrete Institute, Farmington Hills, MI, pp. 599-614.

Grace, N. F.; Soliman, A. K.; Abdel-Sayed, G.; and Saleh, K. R., 1998, “Behavior and Ductility of Simple and Continuous FRP Reinforced Beams,” Journal of Composites for Construction, ASCE, V. 2, No. 4, pp. 186-194. doi: 10.1061/(ASCE)1090-0268(1998)2:4(186)

Hosseini, S. M.; Mousa, S.; Mohamed, H. M.; and Benmokrane, B., 2022, “Structural Behavior of Precast RC Tunnel Segments with GFRP Bars and Ties under Bending Load,” ACI Structural Journal, V. 119, No. 1, Jan., pp. 1-13.

Hosseini, S. M.; Mousa, S.; Mohamed, H. M.; and Benmokrane, B., 2023a, “Development of Strength Interaction Diagrams for Designing Precast Concrete Tunnel Lining Segments Reinforced with GFRP Bars,” Engineering Structures, V. 284, p. 115976. doi: 10.1016/j.engstruct.2023.115976

Hosseini, S. M.; Mousa, S.; Mohamed, H. M.; Ferrier, E.; and Benmokrane, B., 2023b, “Experimental and Analytical Investigation of Precast Fiber-Reinforced Concrete (FRC) Tunnel Lining Segments Reinforced with Glass-FRP Bars,” Tunnelling and Underground Space Technology, V. 139, p. 105230. doi: 10.1016/j.tust.2023.105230

Ibrahim, B.; Mousa, S.; Mohamed, H. M.; and Benmokrane, B., 2022, “GFRP Reinforced Precast Concrete Tunnel Lining Segments under Flexural Cyclic Loading,” 8th International Conference on Advanced Composite Materials in Bridges and Structures, V. 2, pp. 149-156.

Ibrahim, B.; Mousa, S.; Mohamed, H. M.; and Benmokrane, B., 2023a, “Quasi-Static Cyclic Flexural Loading Behavior of Precast Reinforced Concrete Tunnel Segments with Glass Fiber-Reinforced Polymer Bars,” ACI Structural Journal, V. 120, No. 4, July, pp. 73-87.

Ibrahim, B.; Mousa, S.; Mohamed, H. M.; and Benmokrane, B., 2023b, “Quasi-Static Cyclic Behavior of Precast High-Strength Concrete Tunnel Segments Reinforced with GFRP Bars,” Engineering Structures, V. 286, p. 116159 doi: 10.1016/j.engstruct.2023.116159

Jaeger, L. G.; Mufti, A. A.; and Tadros, G., 1997, “The Concept of the Overall Performance Factor in Rectangular-Section Reinforced Concrete Members,” Proceedings, 3rd International Symposium on Non-Metallic (FRP) Reinforcement for Concrete Structures, FRPRCS-3, V. 2, Japan Concrete Institute, Tokyo, Japan, pp. 551-559.

Mohamed, H. M.; Ali, A. H.; and Benmokrane, B., 2017, “Behavior of Circular Concrete Members Reinforced with Carbon-FRP Bars and Spirals Under Shear,” Journal of Composites for Construction, ASCE, V. 21, No. 2, p. 04016090. doi: 10.1061/(ASCE)CC.1943-5614.0000746

Mohamed, H. M.; Ali, A. H.; and Benmokrane, B., 2019, “Mechanism of Distributed Composite GFRP Bars in Circular Concrete Members with and without Spirals under Shear,” Composites. Part B, Engineering, V. 162, pp. 62-72. doi: 10.1016/j.compositesb.2018.10.083

Mohamed, H. M.; Ali, A. H.; Hadhood, A.; Mousa, S.; Abdelazim, W.; and Benmokrane, B., 2020, “Testing, Design, and Field Implementation of GFRP RC Soft-Eyes for Tunnel Construction,” Tunnelling and Underground Space Technology, V. 106, p. 103626. doi: 10.1016/j.tust.2020.103626

Mohamed, H. M., and Benmokrane, B., 2015, “Torsion Behavior of Concrete Beams Reinforced with Glass Fiber-Reinforced Polymer Bars and Stirrups,” ACI Structural Journal, V. 112, No. 5, Sept.-Oct., pp. 543-552. doi: 10.14359/51687824

Mohamed, H. M., and Benmokrane, B., 2016, “Reinforced Concrete Beams with and without FRP Web Reinforcement under Pure Torsion,” Journal of Bridge Engineering, ASCE, V. 21, No. 3, p. 04015070. doi: 10.1061/(ASCE)BE.1943-5592.0000839

Mousa, S.; Mohamed, H. M.; and Benmokrane, B., 2018, “Flexural Strength and Design Analysis of Circular Reinforced Concrete Members with Glass Fiber-Reinforced Polymer Bars and Spirals,” ACI Structural Journal, V. 115, No. 5, Sept.-Oct., pp. 1353-1357. doi: 10.14359/51702282

Mousa, S.; Mohamed, H. M.; and Benmokrane, B., 2019, “Strength and Deformability Aspects of Circular Concrete Members Reinforced with Hybrid Carbon-FRP and Glass-FRP Under Flexure,” Journal of Composites for Construction, ASCE, V. 23, No. 2, p. 04019005. doi: 10.1061/(ASCE)CC.1943-5614.0000931

Mousa, S.; Mohamed, H. M.; Benmokrane, B.; and Nanni, A., 2020, “Flexural Behavior of Long-Span Square Reinforced Concrete Members with Uniformly Distributed Fiber-Reinforced Polymer Bars,” ACI Structural Journal, V. 117, No. 4, July, pp. 209-222.

Naaman, A. E., and Jeong, S. M., 1995, “Structural Ductility of Concrete Beams Prestressed with FRP Tendons,” Proceedings of the 2nd International RILEM Symp. on Non-Metallic (FRP) Reinforcement for Concrete Structures, RILEM, Bagneux, France, pp. 379-386.

Pan, Y., and Yan, D., 2021, “Study on the Durability of GFRP Bars and Carbon/Glass Hybrid Fiber Reinforced Polymer (HFRP) Bars Aged in Alkaline Solution,” Composite Structures, V. 261, p. 113285. doi: 10.1016/j.compstruct.2020.113285

Rancourt, A., 2016, “Analysis of the Costs of a Tunnel Drilled between Beauport and Lévis,” Report, Géosys, pp. 35.

Solyom, S., and Balázs, G. L., 2020, “Bond of FRP Bars with Different Surface Characteristics,” Construction and Building Materials, V. 264, p. 119839. doi: 10.1016/j.conbuildmat.2020.119839

Spagnuolo, S.; Meda, A.; Rinaldi, Z.; and Nanni, A., 2017, “Precast Concrete Tunnel Segments with GFRP Reinforcement,” Journal of Composites for Construction, ASCE, V. 21, No. 5, p. 04017020. doi: 10.1061/(ASCE)CC.1943-5614.0000803

Wang, Z.; Zhao, X. L.; Xian, G.; Wu, G.; Raman, R. S.; Al-Saadi, S.; and Haque, A., 2017, “Long-Term Durability of Basalt-and Glass-Fibre Reinforced Polymer (BFRP/GFRP) Bars in Seawater and Sea Sand Concrete Environment,” Construction and Building Materials, V. 139, pp. 467-489. doi: 10.1016/j.conbuildmat.2017.02.038

Whitmore, D. W., and Ball, J. C., 2004, “Corrosion Management,” Concrete International, V. 26, No. 12, Dec., pp. 82-85.

Xiao, S.; Li, J.; and Mo, Y. L., 2018, “Effect of Loading Rate on Cyclic Behavior of Reinforced Concrete Beams,” Advances in Structural Engineering, V. 21, No. 7, pp. 990-1001. doi: 10.1177/1369433217737114

Zhiqiang, Z., and Mansoor, Y. A., 2013, “Evaluating the Strength of Corroded Tunnel Lining under Limiting Corrosion Conditions,” Tunnelling and Underground Space Technology, V. 38, pp. 464-475. doi: 10.1016/j.tust.2013.08.003


ALSO AVAILABLE IN:

Electronic Structural Journal



  

Edit Module Settings to define Page Content Reviewer