International Concrete Abstracts Portal

  


Title: GFRP Reinforcement for Concrete Facilities to Protect Against Mudflow

Author(s): Valery Hurynovich and Antonio Nanni

Publication: Concrete International

Volume: 46

Issue: 2

Appears on pages(s): 38-42

Keywords: bars, cost, channel, water

DOI:

Date: 2/1/2024

Abstract:
A unique complex of mudflow protection facilities was recently constructed to protect the city of Ashgabat, Turkmenistan, using concrete reinforced with glass fiber-reinforced polymer reinforcement (GFRP). The project’s specifications and design provisions followed current Russian standards for fiber-reinforced polymer reinforcement, and the project was completed on time and under budget.




  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

Edit Module Settings to define Page Content Reviewer