Modeling of Concrete Printing Process with Frictional Interface

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Modeling of Concrete Printing Process with Frictional Interface

Author(s): Ignasius P. A. Wijaya, Eric Kreiger, and Arif Masud

Publication: Structural Journal

Volume: 121

Issue: 2

Appears on pages(s): 71-85

Keywords: concrete printing; geometric instability; material instability; printing-induced deformation; structural failure

DOI: 10.14359/51740243

Date: 3/1/2024

Abstract:
Three-dimensional (3-D) concrete printing is invariably accompanied by slippage between the printed structure and the platform, which affects the shape of the printed object. This study employs a physics-based friction model in a finite-deformation interfacial kinematic framework to model relative slipping between the bottom layer and the supporting surface. The constitutive model that is specialized for cementitious materials is based on an extension of the Drucker-Prager plasticity model. The evolution of material parameters due to thixotropy and hydration reaction results in increased stiffness that gives rise to the non-physical bounce-back phenomenon. A bounce-back control algorithm is presented and used in conjunction with the plasticity model as well as the interfacial frictional model. The printing process is simulated through an algorithm that controls the kinematics of the nozzle and links the material timescales of curing with the timescales of layered printing. The model and method are validated against experimental data, and several interesting test cases are presented.

Related References:

ACI Committee 347, 2004, “Guide to Formwork for Concrete (ACI 347-04),” American Concrete Institute, Farmington Hills, MI, 32 pp.

Bažant, Z. P., 1979, “Thermodynamics of Solidifying or Melting Viscoelastic Material,” Journal of the Engineering Mechanics Division, ASCE, V. 105, No. 6, pp. 933-952. doi: 10.1061/JMCEA3.0002555

Bažant, Z. P., ed., 1988, Mathematical Modeling of Creep and Shrinkage of Concrete, John Wiley & Sons, Inc., New York.

Comminal, R.; Leal da Silva, W. R.; Andersen, T. J.; Stang, H.; and Spangenberg, J., 2020, “Modelling of 3D Concrete Printing Based on Computational Fluid Dynamics,” Cement and Concrete Research, V. 138, Article No. 106256. doi: 10.1016/j.cemconres.2020.106256

de Miranda, L. R. M.; Marchesini, F. H.; Lesage, K.; and De Schutter, G., 2023, “The Evolution of the Rheological Behavior of Hydrating Cement Systems: Combining Constitutive Modeling with Rheometry, Calorimetry and Mechanical Analyses,” Cement and Concrete Research, V. 164, Article No. 107046. doi: 10.1016/j.cemconres.2022.107046

Diggs-McGee, B. N., and Kreiger, E. L., 2021, “Using Isolated Temporal Analysis to Aid in the Assessment of Structural Element Quality for Additive Construction,” Standards Development for Cement and Concrete for Use in Additive Construction, S. Z. Jones and E. L. Kreiger, eds., ASTM International, West Conshohocken, PA, pp. 117-143. doi: 10.1520/STP163620200105

Gawin, D.; Pesavento, F.; and Schrefler, B. A., 2006, “Hygro-Thermo-Chemo-Mechanical Modelling of Concrete at Early Ages and Beyond. Part I: Hydration and Hygro-Thermal Phenomena,” International Journal for Numerical Methods in Engineering, V. 67, No. 3, pp. 299-331. doi: 10.1002/nme.1615

Harbouz, I.; Yahia, A.; Roziere, E.; and Loukili, A., 2023, “Printing Quality Control of Cement-Based Materials under Flow and Rest Conditions,” Cement and Concrete Composites, V. 138, Article No. 104965. doi: 10.1016/j.cemconcomp.2023.104965

Jagoda, J. A., 2020, “An Analysis of the Viability of 3D-Printed Construction as an Alternative to Conventional Construction Methods in the Expeditionary Environment,” master’s thesis, Air Force Institute of Technology, Wright-Patterson AFB, OH, 121 pp.

Khan, M. S.; Sanchez, F.; and Zhou, H., 2020, “3-D Printing of Concrete: Beyond Horizons,” Cement and Concrete Research, V. 133, Article No. 106070. doi: 10.1016/j.cemconres.2020.106070

Kreiger, E.; Diggs-McGee, B.; Wood, T.; MacAllister, B.; and Kreiger, M., 2020, “Field Considerations for Deploying Additive Construction,” Second RILEM International Conference on Concrete and Digital Fabrication: Digital Concrete 2020, F. P. Bos, S. S. Lucas, R. J. M. Wolfs, and T. A. M. Salet, eds., Springer International Publishing, Cham, Switzerland, pp. 1147-1163. doi: 10.1007/978-3-030-49916-7_109

Kreiger, E. L.; Kreiger, M. A.; and Case, M. P., 2019, “Development of the Construction Processes for Reinforced Additively Constructed Concrete,” Additive Manufacturing, V. 28, pp. 39-49. doi: 10.1016/j.addma.2019.02.015

Kröner, E., 1959, “Allgemeine Kontinuumstheorie der Versetzungen und Eigenspannungen,” Archive for Rational Mechanics and Analysis, V. 4, No. 1, pp. 273-334. (in German) doi: 10.1007/BF00281393

Kupwade-Patil, K.; Tyagi, M.; Brown, C. M.; and Büyüköztürk, O., 2016, “Water Dynamics in Cement Paste at Early Age Prepared with Pozzolanic Volcanic Ash and Ordinary Portland Cement Using Quasielastic Neutron Scattering,” Cement and Concrete Research, V. 86, pp. 55-62. doi: 10.1016/j.cemconres.2016.04.011

Laursen, T. A., and Simo, J. C., 1993, “A Continuum-Based Finite Element Formulation for the Implicit Solution of Multibody, Large

Deformation-Frictional Contact Problems,” International Journal for Numerical Methods in Engineering, V. 36, No. 20, pp. 3451-3485. doi: 10.1002/nme.1620362005

Le, T. T.; Austin, S. A.; Lim, S.; Buswell, R. A.; Gibb, A. G. F.; and Thorpe, T., 2012a, “Mix Design and Fresh Properties for High-Performance Printing Concrete,” Materials and Structures, V. 45, No. 8, pp. 1221-1232. doi: 10.1617/s11527-012-9828-z

Le, T. T.; Austin, S. A.; Lim, S.; Buswell, R. A.; Law, R.; Gibb, A. G. F.; and Thorpe, T., 2012b, “Hardened Properties of High-Performance Printing Concrete,” Cement and Concrete Research, V. 42, No. 3, pp. 558-566. doi: 10.1016/j.cemconres.2011.12.003

Lee, E. H., 1969, “Elastic-Plastic Deformation at Finite Strains,” Journal of Applied Mechanics, V. 36, No. 1, pp. 1-6. doi: 10.1115/1.3564580

Masud, A., and Goraya, S., 2022, “Variational Embedding of Measured Data in Physics-Constrained Data-Driven Modeling,” Journal of Applied Mechanics, V. 89, No. 11, Article No. 111001. doi: 10.1115/1.4055256

Masud, A.; Truster, T. J.; and Bergman, L. A., 2012, “A Unified Formulation for Interface Coupling and Frictional Contact Modeling with Embedded Error Estimation,” International Journal for Numerical Methods in Engineering, V. 92, No. 2, pp. 141-177. doi: 10.1002/nme.4326

Nedjar, B., 2022, “Incremental Viscoelasticity at Finite Strains for the Modelling of 3D Concrete Printing,” Computational Mechanics, V. 69, No. 1, pp. 233-243. doi: 10.1007/s00466-021-02091-5

Ngo, T. D.; Kashani, A.; Imbalzano, G.; Nguyen, K. T. Q.; and Hui, D., 2018, “Additive Manufacturing (3D Printing): A Review of Materials, Methods, Applications and Challenges,” Composites Part B: Engineering, V. 143, pp. 172-196. doi: 10.1016/j.compositesb.2018.02.012

Paolini, A.; Kollmannsberger, S.; and Rank, E., 2019, “Additive Manufacturing in Construction: A Review on Processes, Applications, and Digital Planning Methods,” Additive Manufacturing, V. 30, Article No. 100894. doi: 10.1016/j.addma.2019.100894

Perrot, A.; Rangeard, D.; and Pierre, A., 2016, “Structural Built-Up of Cement-Based Materials Used for 3D-Printing Extrusion Techniques,” Materials and Structures, V. 49, No. 4, pp. 1213-1220. doi: 10.1617/s11527-015-0571-0

Reinold, J.; Nerella, V. N.; Mechtcherine, V.; and Meschke, G., 2022, “Extrusion Process Simulation and Layer Shape Prediction during 3D-Concrete-Printing Using the Particle Finite Element Method,” Automation in Construction, V. 136, Article No. 104173. doi: 10.1016/j.autcon.2022.104173

Reiter, L.; Wangler, T.; Roussel, N.; and Flatt, R. J., 2018, “The Role of Early Age Structural Build-Up in Digital Fabrication with Concrete,” Cement and Concrete Research, V. 112, pp. 86-95. doi: 10.1016/j.cemconres.2018.05.011

Roussel, N., 2006, “A Thixotropy Model for Fresh Fluid Concretes: Theory, Validation and Applications,” Cement and Concrete Research, V. 36, No. 10, pp. 1797-1806. doi: 10.1016/j.cemconres.2006.05.025

Roussel, N., 2018, “Rheological Requirements for Printable Concretes,” Cement and Concrete Research, V. 112, pp. 76-85. doi: 10.1016/j.cemconres.2018.04.005

Roussel, N.; Spangenberg, J.; Wallevik, J.; and Wolfs, R., 2020, “Numerical Simulations of Concrete Processing: From Standard Formative Casting to Additive Manufacturing,” Cement and Concrete Research, V. 135, Article No. 106075. doi: 10.1016/j.cemconres.2020.106075

Simo, J. C., and Hughes, T. J. R., 1998, Computational Inelasticity, Springer-Verlag New York, Inc., New York.

Simo, J. C., and Laursen, T. A., 1992, “An Augmented Lagrangian Treatment of Contact Problems Involving Friction,” Computers & Structures, V. 42, No. 1, pp. 97-116. doi: 10.1016/0045-7949(92)90540-G

Spangenberg, J.; Leal da Silva, W. R.; Comminal, R.; Mollah, M. T.; Andersen, T. J.; and Stang, H., 2021, “Numerical Simulation of Multi-Layer 3D Concrete Printing,” RILEM Technical Letters, V. 6, pp. 119-123. doi: 10.21809/rilemtechlett.2021.142

Suiker, A. S. J., 2018, “Mechanical Performance of Wall Structures in 3D Printing Processes: Theory, Design Tools and Experiments,” International Journal of Mechanical Sciences, V. 137, pp. 145-170. doi: 10.1016/j.ijmecsci.2018.01.010

Suiker, A. S. J.; Wolfs, R. J. M.; Lucas, S. M.; and Salet, T. A. M., 2020, “Elastic Buckling and Plastic Collapse during 3D Concrete Printing,” Cement and Concrete Research, V. 135, Article No. 106016. doi: 10.1016/j.cemconres.2020.106016

Tripathi, A.; Nair, S. A. O.; and Neithalath, N., 2022, “A Comprehensive Analysis of Buildability of 3D-Printed Concrete and the Use of Bi-Linear Stress-Strain Criterion-Based Failure Curves towards Their Prediction,” Cement and Concrete Composites, V. 128, Article No. 104424. doi: 10.1016/j.cemconcomp.2022.104424

Wangler, T.; Roussel, N.; Bos, F. P.; Salet, T. A. M.; and Flatt, R. J., 2019, “Digital Concrete: A Review,” Cement and Concrete Research, V. 123, Article No. 105780. doi: 10.1016/j.cemconres.2019.105780

Wijaya, I. P. A.; Kreiger, E.; and Masud, A., 2022, “An Elastic-Inelastic Model and Embedded Bounce‐Back Control for Layered Printing with Cementitious Materials,” International Journal for Numerical Methods in Engineering, V. 123, No. 21, pp. 5098-5125. doi: 10.1002/nme.7044

Wolfs, R. J. M., and Suiker, A. S. J., 2019, “Structural Failure during Extrusion-Based 3D Printing Processes,” International Journal of Advanced Manufacturing Technology, V. 104, No. 1-4, pp. 565-584. doi: 10.1007/s00170-019-03844-6

Wolfs, R. J. M.; Bos, F. P.; and Salet, T. A. M., 2018, “Early Age Mechanical Behaviour of 3D Printed Concrete: Numerical Modelling and Experimental Testing,” Cement and Concrete Research, V. 106, pp. 103-116. doi: 10.1016/j.cemconres.2018.02.001


ALSO AVAILABLE IN:

Electronic Structural Journal