Modified Shear Design Model for Steel- and Fiber-Reinforced Polymer-Reinforced Concrete Beams

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Modified Shear Design Model for Steel- and Fiber-Reinforced Polymer-Reinforced Concrete Beams

Author(s): A. N. Tarawneh, E. F. Saleh, A. M Alghossoon, G. S. Almasabha, O. S. Alajarmeh, A. Manalo, and B. Benmokrane

Publication: Structural Journal

Volume: 121

Issue: 1

Appears on pages(s): 147-158

Keywords: ACI 440; axial stiffness; code evaluation; fiber-reinforced polymer (FRP)-reinforced concrete (RC) beams; fiber-reinforced polymer (FRP) reinforcement; reliability analysis; shear strength; steel-reinforced concrete beams; steel reinforcement

DOI: 10.14359/51739191

Date: 1/1/2024

Abstract:
This study proposes a unified shear design provision for slender steel- and fiber-reinforced polymer (FRP)-reinforced concrete (RC) members. The proposed model is a modification of the ACI 318-19 model to include the axial stiffness of the longitudinal reinforcement by introducing a new modification term, nc, representing the elastic modular ratio of the longitudinal reinforcement to the concrete. The new relation is Vc = (0.4 [nc ρfl]1/3 λ s√fcꞌ + Nu/[6Ag])bwd. The unified shear model was assessed with five experimental data sets: FRP-RC beams without shear reinforcement (288 beams), steel-RC beams without shear reinforcement (759 beams), FRP-RC beams with shear reinforcement (56 beams), steel-RC beams with shear reinforcement (157 beams), and steel-RC beams with axial force (prestressed) but without shear reinforcement (209 beams). The unified shear model provided better performance than the ACI 318-19 and ACI CODE-440.11-22 provisions in terms of mean, coefficient of variation, standard deviation (SD), and absolute average error (AAE). The unified model also showed improved performance over a wider range of material properties. In addition, reliability analysis using Monte Carlo simulation indicated that the unified shear model provides a consistent satisfactory safety level with a reliability index between 3.5 and 4.0 for both steel- and FRP-RC members. The reliability index provided by the unified model is similar to the reliability index provided by the ACI 318-19 shear provision. In contrast, the ACI CODE-440.11-22 results in highly conservative estimates with a reliability index between 4.5 and 5.0.

Related References:

1. Regan, P. E., “Shear in Reinforced Concrete: An Analytical Study,” Construction Industry Research and Information Association, Department of Civil Engineering, Imperial College, London, UK, 1971.

2. Kupfer, H.; Hilsdorf, H. K.; and Rusch, H., “Behavior of Concrete Under Biaxial Stresses,” ACI Journal Proceedings, V. 66, No. 8, Aug. 1969, pp. 656-666.

3. Taylor, H. P. J., “Investigation of the Forces Carried Across Cracks in Reinforced Concrete Beams in Shear by Interlock of Aggregate,” 1970.

4. Reineck, K. H., “Ultimate Shear Force of Structural Concrete Members without Transverse Reinforcement Derived from a Mechanical Model,” ACI Structural Journal, V. 88, No. 5, Sept.-Oct. 1991, pp. 592-602.

5. Nielsen, M. P., and Hoang, L. C., Limit Analysis and Concrete Plasticity, CRC Press, Boca Raton, FL, 2016.

6. Mitchell, D., and Collins, M. P., “Diagonal Compression Field Theory – A Rational Model for Structural Concrete in Pure Torsion,” ACI Journal Proceedings, V. 71, No. 8, Aug. 1974, pp. 396-408.

7. Vecchio, F. J., and Collins, M. P., “The Modified Compression-Field Theory for Reinforced Concrete Elements Subjected to Shear,” ACI Journal Proceedings, V. 83, No. 2, Mar.-Apr. 1986, pp. 219-231.

8. Kotsovos, M. D., “Compressive Force Path Concept: Basis for Reinforced Concrete Ultimate Limit State Design,” ACI Structural Journal, V. 85, No. 1, Jan.-Feb. 1988, pp. 68-75.

9. Mrsch, E., Concrete Steel Construction, McGraw Hill, New York, NY, 1909.

10. Guadagnini, M.; Pilakoutas, K.; and Waldron, P., “Shear Resistance of FRP RC Beams: Experimental Study,” Journal of Composites for Construction, ASCE, V. 10, No. 6, 2006, pp. 464-473. doi: 10.1061/(ASCE)1090-0268(2006)10:6(464)

11. Tarawneh, A. N.; Dwairi, H. M.; Almasabha, G. S.; and Majdalaweyh, S. A., “Effect of Fiber-Reinforced Polymer-Compression Reinforcement in Columns Subjected to Concentric and Eccentric Loading,” ACI Structural Journal, V. 118, No. 3, May 2021, pp. 187-197

12. Bentz, E. C.; Massam, L.; and Collins, M. P., “Shear Strength of Large Concrete Members with FRP Reinforcement,” Journal of Composites for Construction, ASCE, V. 14, No. 6, 2010, pp. 637-646. doi: 10.1061/(ASCE)CC.1943-5614.0000108

13. Farghaly, A., and Benmokrane, B., “Shear Behavior of FRP-Reinforced Concrete Deep Beams without Web Reinforcement,” Journal of Composites for Construction, ASCE, V. 17, No. 6, 2013, p. 04013015. doi: 10.1061/(ASCE)CC.1943-5614.0000385

14. Tureyen, A. K., and Frosch, R. J., “Shear Tests of FRP-Reinforced Concrete Beams without Stirrups,” ACI Structural Journal, V. 99, No. 4, July-Aug. 2002, pp. 427-434.

15. Kanakubo, T., and Shindo, M., “Shear Behavior of Fiber-Mesh Reinforced Plates,” Non-­Metallic (FRP) Reinforcement for Concrete Structures: Proceedings of the Third International Symposium (FRPRCS-3), Sapporo, Japan, 1997, pp. 317-324.

16. Peng, F.; Xue, W.; and Xue, W., “Database Evaluation of Shear Strength of Slender Fiber-Reinforced Polymer-Reinforced Concrete Members,” ACI Structural Journal, V. 117, No. 3, May 2020, pp. 273-281.

17. Kuchma, D. A.; Wei, S.; Sanders, D. H.; Belarbi, A.; and Novak, L. C., “Development of the One-Way Shear Design Provisions of ACI 318-19 for Reinforced Concrete,” ACI Structural Journal, V. 116, No. 4, July 2019, pp. 285-296. doi: 10.14359/51716739

18. ACI Committee 318, “Building Code Requirements for Structural Concrete (ACI 318-19) and Commentary (ACI 318R-19) (Reapproved 2022),” American Concrete Institute, Farmington Hills, MI, 2019, 624 pp.

19. ACI Committee 440, “Guide for the Design and Construction of Structural Concrete Reinforced with Fiber-Reinforced Polymer Bars (ACI 440.1R-15),” American Concrete Institute, Farmington Hills, MI, 2015, 88 pp.

20. ACI Committee 440, “Building Code Requirements for Structural Concrete Reinforced with Glass Fiber-Reinforced Polymer (GFRP) Bars—Code and Commentary (ACI CODE-440.11-22),” American Concrete Institute, Farmington Hills, MI, 2022, 260 pp.

21. Nanni, A.; De Luca, A.; and Zadeh, J. H., FRP Reinforced Concrete Structures—Theory, Design and Practice, CRC Press, Boca Raton, FL, 2014, 400 pp.

22. Reineck, K. H.; Bentz, E. C.; Fitik, B.; Kuchma, D. A.; and Bayrak, O., “ACI-DAfStb Databases for Shear Tests on Slender Reinforced Concrete Beams without Stirrups,” ACI Structural Journal, V. 110, No. 5, Sept.-Oct. 2013, pp. 867-876. doi: 10.14359/51685839

23. Reineck, K. H.; Bentz, E. C.; Fitik, B.; Kuchma, D. A.; and Bayrak, O., “ACI-DAfStb Databases for Shear Tests on Slender Reinforced Concrete Beams with Stirrups,” ACI Structural Journal, V. 111, No. 5, Sept.-Oct. 2014, pp. 1147-1156. doi: 10.14359/51686819

24. Kaszubska, M.; Kotynia, R.; Barros, J. A.; and Baghi, H., “Shear Behavior of Concrete Beams Reinforced Exclusively with Longitudinal Glass Fiber Reinforced Polymer Bars: Experimental Research,” Structural Concrete, V. 19, No. 1, 2018, pp. 152-161. doi: 10.1002/suco.201700174

25. Razaqpur, A. G.; Shedid, M.; and Isgor, B., “Shear Strength of Fiber-Reinforced Polymer Reinforced Concrete Beams Subject to Unsymmetric Loading,” Journal of Composites for Construction, ASCE, V. 15, No. 4, 2011, pp. 500-512. doi: 10.1061/(ASCE)CC.1943-5614.0000184

26. El-Sayed, A.; El-Salakawy, E.; and Benmokrane, B., “Shear Strength of One-Way Concrete Slabs Reinforced with Fiber-Reinforced Polymer Composite Bars,” Journal of Composites for Construction, ASCE, V. 9, No. 2, 2005, pp. 147-157. doi: 10.1061/(ASCE)1090-0268(2005)9:2(147)

27. Issa, M. A.; Ovitigala, T.; and Ibrahim, M., “Shear Behavior of Basalt Fiber Reinforced Concrete Beams with and without Basalt FRP Stirrups,” Journal of Composites for Construction, ASCE, V. 20, No. 4, 2016, p. 04015083. doi: 10.1061/(ASCE)CC.1943-5614.0000638

28. El Refai, A., and Abed, F., “Concrete Contribution to Shear Strength of Beams Reinforced with Basalt Fiber-Reinforced Bars,” Journal of Composites for Construction, ASCE, V. 20, No. 4, 2016, p. 04015082. doi: 10.1061/(ASCE)CC.1943-5614.0000648

29. Tomlinson, D., and Fam, A., “Performance of Concrete Beams Reinforced with Basalt FRP for Flexure and Shear,” Journal of Composites for Construction, ASCE, V. 19, No. 2, 2015, p. 04014036. doi: 10.1061/(ASCE)CC.1943-5614.0000491

30. Khaja, M. N., and Sherwood, E. G., “Does the Shear Strength of Reinforced Concrete Beams and Slabs Depend Upon the Flexural Reinforcement Ratio or the Reinforcement Strain?” Canadian Journal of Civil Engineering, V. 40, No. 11, 2013, pp. 1068-1081. doi: 10.1139/cjce-2012-0459

31. Abdul-Salam, B., “Behaviour of Shear Critical FRP Reinforced Concrete One-Way Slabs,” doctoral dissertation, Université de Sherbrooke, Sherbrooke, QC, Canada, 2014.

32. Chang, K., and Seo, D., “Behavior of One-Way Concrete Slabs Reinforced with GFRP Bars,” Journal of Asian Architecture and Building Engineering, V. 11, No. 2, 2012, pp. 351-358. doi: 10.3130/jaabe.11.351

33. Ashour, A. F., and Kara, I. F., “Size Effect on Shear Strength of FRP Reinforced Concrete Beams,” Composites Part B: Engineering, V. 60, 2014, pp. 612-620. doi: 10.1016/j.compositesb.2013.12.002

34. Ashour, A. F., “Flexural and Shear Capacities of Concrete Beams Reinforced with GFRP Bars,” Construction and Building Materials, V. 20, No. 10, 2006, pp. 1005-1015. doi: 10.1016/j.conbuildmat.2005.06.023

35. Tariq, M., and Newhook, J. P., “Shear Testing of FRP Reinforced Concrete without Transverse Reinforcement,” Proceedings, Annual Conference of the Canadian Society for Civil Engineering, Moncton, NB, Canada, June 2003, pp. 1330-1339.

36. Kim, C. H., and Jang, H. S., “Concrete Shear Strength of Normal and Lightweight Concrete Beams Reinforced with FRP Bars,” Journal of Composites for Construction, ASCE, V. 18, No. 2, 2014, p. 04013038. doi: 10.1061/(ASCE)CC.1943-5614.0000440

37. El-Sayed, A. K.; Soudki, K.; and Kling, E., “Flexural Behaviour of Self-Consolidating Concrete Slabs Reinforced with GFRP Bars,” Proceedings of the 9th International Symposium on Fiber Reinforced Polymer Reinforcement for Reinforced Concrete Structures (FRPRCS-9), D. Oehlers, M. Griffith, and R. Seracino, eds., Sydney, NSW, Australia, July 2009, pp. 13-15.

38. Zhao, W.; Maruyama, K.; and Suzuki, H., “Shear Behavior of Concrete Beams Reinforced by FRP Rods as Longitudinal and Shear Reinforcement,” Non-metallic (FRP) Reinforcement for Concrete Structures: Proceedings of the Second International RILEM Symposium (FRPRCS-2), L. Taerwe, ed., Ghent, Belgium, Aug. 1995, pp. 352-359.

39. Alkhrdaji, T.; Wideman, M.; Belarbi, A.; and Nanni, A., “Shear Strength of GFRP RC Beams and Slabs,” Proceedings of the International Conference, Oct. 2001, pp. 409-414.

40. Deitz, D. H.; Harik, I. E.; and Gesund, H., “One-Way Slabs Reinforced with Glass Fiber Reinforced Polymer Reinforcing Bars,” Fourth International Symposium—Fiber Reinforced Polymer Reinforcement for Reinforced Concrete Structures, SP-188, C. W. Dolan, S. H. Rizkalla, and A. Nanni, eds., American Concrete Institute, Farmington Hills, MI, 1999, pp. 279-286.

41. Duranovic, N.; Pilakoutas, K.; and Waldron, P., “Tests on Concrete Beams Reinforced with Glass Fibre Reinforced Plastic Bars,” Non-Metallic (FRP) Reinforcement for Concrete Structures: Proceedings of the Third International Symposium (FRPRCS-3), Sapporo, Japan, Oct. 14-16, 1997, pp. 479-486.

42. Matta, F.; El-Sayed, A. K.; Nanni, A.; and Benmokrane, B., “Size Effect on Concrete Shear Strength in Beams Reinforced with Fiber-Reinforced Polymer Bars,” ACI Structural Journal, V. 110, No. 4, July-Aug. 2013, pp. 617-628.

43. Yost, J. R.; Gross, S. P.; and Dinehart, D. W., “Shear Strength of Normal Strength Concrete Beams Reinforced with Deformed GFRP Bars,” Journal of Composites for Construction, ASCE, V. 5, No. 4, 2001, pp. 268-275. doi: 10.1061/(ASCE)1090-0268(2001)5:4(268)

44. Alam, M. S., “Influence of Different Parameters on Shear Strength of FRP Reinforced Concrete Beams without Web Reinforcement,” doctoral dissertation, Memorial University of Newfoundland, St. Johns, NL, Canada, 2010.

45. Olivito, R. S., and Zuccarello, F. A., “On the Shear Behaviour of Concrete Beams Reinforced by Carbon Fibre‐Reinforced Polymer Bars: An Experimental Investigation by Means of Acoustic Emission Technique,” Strain, V. 46, No. 5, 2010, pp. 470-481. doi: 10.1111/j.1475-1305.2009.00699.x

46. Gross, S. P.; Yost, J. R.; Dinehart, D. W.; Svensen, E.; and Liu, N., “Shear Strength of Normal and High Strength Concrete Beams Reinforced with GFRP Bars,” High Performance Materials in Bridges, A. Azizinamini, A. Yakel, and M. Abdelrahman, eds., 2003, pp. 426-437.

47. Ali, I.; Thamrin, R.; Abdul, A. A. S.; and Noridah, M., “Diagonal Shear Cracks and Size Effect in Concrete Beams Reinforced with Glass Fiber Reinforced Polymer (GFRP) Bars,” Applied Mechanics and Materials, V. 621, 2014, pp. 113-119. doi: 10.4028/www.scientific.net/AMM.621.113

48. Nakamura, H., and Higai, T., “Evaluation of Shear Strength of Concrete Beams Reinforced with FRP,” Proceedings of the Japan Society of Civil Engineers, V. 508, 1995, pp. 89-100.

49. Swamy, N., and Aburawi, M., “Structural Implications of Using GFRP Bars as Concrete Reinforcement,” Non-Metallic (FRP) Reinforcement for Concrete Structures: Proceedings of the Third International Symposium (FRPRCS-3), Sapporo, Japan, Oct. 14-16, 1997, pp. 503-510.

50. Liu, R., “Precast Concrete Bridge Deck Panels Reinforced with Glass Fiber Reinforced Polymer Bars,” doctoral dissertation, The University of Utah, Salt Lake City, UT, 2011.

51. Farahmand, F., “Shear Behaviour of Concrete Beams Reinforced with Glass Fibre Reinforced Plastic,” thesis, Department of Civil & Geological Engineering, University of Manitoba, Winnipeg, MB, Canada, 1996, pp. 234-345.

52. Gross, S. P.; Dinehart, D. W.; Yost, J. R.; and Theisz, P. M., “Experimental Tests of High-Strength Concrete Beams Reinforced with CFRP Bars,” Proceedings of the 4th International Conference on Advanced Composite Materials in Bridges and Structures (ACMBS-4), Calgary, AB, Canada, July 2004.

53. Maruyama, K., and Zhao, W. J., “Flexural and Shear Behaviour of Concrete Beams Reinforced with FRP Rods,” Corrosion and Corrosion Protection of Steel in Concrete, 1994, pp. 1330-1339.

54. Caporale, A., and Luciano, R., “Indagine Sperimentale e Numerica sulla Resistenza a Taglio di Travi di Calcestruzzo Armate con Barre di GFRP,” Proceedings of XXXVIII Convegno Nazionale AIAS, Turin, Italy, 2009. (in Italian)

57. Kilpatrick, A. E., and Easden, L., “Shear Capacity of GFRP Reinforced High Strength Concrete Slabs,” Developments in Mechanics of Structures and Materials, V. 1, 2005, pp. 119-124.

56. Kilpatrick, A. E., and Dawborn, R., “Flexural Shear Capacity of High Strength Concrete Slabs Reinforced with Longitudinal GFRP Bars,” Proceedings, Second International fib Congress, Naples, Italy, 2006, pp. 1-10.

57. Johnson, D. T. C., “Investigation of Glass Fibre Reinforced Polymer (GFRP) Bars as Internal Reinforcement for Concrete Structures,” PhD dissertation, University of Toronto, Toronto, ON, Canada, 2014.

58. Maranan, G. B.; Manalo, A. C.; Benmokrane, B.; Karunasena, W.; Mendis, P.; and Nguyen, T. Q., “Shear Behaviour of Geopolymer-Concrete Beams Transversely Reinforced with Continuous Rectangular GFRP Composite Spirals,” Composite Structures, V. 187, 2018, pp. 454-465. doi: 10.1016/j.compstruct.2017.12.080

59. Shehata, E.; Morphy, R.; and Rizkalla, S., “Fibre Reinforced Polymer Shear Reinforcement for Concrete Members: Behaviour and Design Guidelines,” Canadian Journal of Civil Engineering, V. 27, No. 5, 2000, pp. 859-872. doi: 10.1139/l00-004

60. Niewels, J., 2008, “Zum tragverhalten von botonbauteilen mit faserverbundkunststoffbewerhung,” PhD dissertation, Aachen University, Aachen, Germany, 164 pp. (in German)

61. Imjai, T., “Design and Analysis of Curved FRP Composites as Shear Reinforcement for Concrete Structures,” PhD dissertation, University of Sheffield, Sheffield, UK, 264 pp.

62. Yang, F., “Deformation Behaviour of Beams Reinforced with Fibre Reinforced Polymer Bars under Bending and Shear,” PhD dissertation, University of Sheffield, Sheffield, UK, 2014, 138 pp.

63. Ascione, F., “A Preliminary Numerical and Experimental Investigation on the Shear Stress Distribution on Multi-Row Bolted FRP Joints,” Mechanics Research Communications, V. 37, No. 2, 2010, pp. 164-168. doi: 10.1016/j.mechrescom.2010.01.006

64. Alsayed, S. H., “Flexural Behavior of Concrete Beams Reinforced with GFRP Bars,” Cement and Concrete Composites, V. 20, No. 1, 1998, pp. 1-11. doi: 10.1016/S0958-9465(97)00061-9

65. Reineck, K. H.; Kuchma, D. A.; and Fitik, B., “Extended Databases with Shear Tests on Structural Concrete Beams without and with Stirrups for the Assessment of Shear Design Procedures,” Nuclear Regulatory Commission, Rockville, MD, 2010.

69. Nehdi, M.; El Chabib, H.; and Saïd, A. A., “Proposed Shear Design Equations for FRP-Reinforced Concrete Beams Based on Genetic Algorithms Approach,” Journal of Materials in Civil Engineering, ASCE, V. 19, No. 12, 2007, pp. 1033-1042. doi: 10.1061/(ASCE)0899-1561(2007)19:12(1033)

66. Kara, I. F., “Prediction of Shear Strength of FRP-Reinforced Concrete Beams Without Stirrups Based on Genetic Programming,” Advances in Engineering Software, V. 42, No. 6, 2011, pp. 295-304. doi: 10.1016/j.advengsoft.2011.02.002

68. MacGregor, J. G., “Safety and Limit States Design for Reinforced Concrete,” Canadian Journal of Civil Engineering, V. 3, No. 4, 1976, pp. 484-513. doi: 10.1139/l76-055

69. Ellingwood, B.; Galambos, T.; MacGregor, J.; and Cornell, C. A., “Development of a Probability Based Load Criterion for American National Standard A58,” NBS Special Publication 577, National Bureau of Standards, U.S. Department of Commerce, Washington, DC, June 1980, 222 pp.

70. Farrow, C. B.; Frigui, I.; and Klingner, R. E., “Tensile Capacity of Single Anchors in Concrete: Evaluation of Existing Formulas on an LRFD Basis,” ACI Structural Journal, V. 93, No. 1, Jan.-Feb. 1996, pp. 128-137.

71. Szerszen, M. M., and Nowak, A. S., “Calibration of Design Code for Buildings (ACI 318): Part 2—Reliability Analysis and Resistance Factors,” ACI Structural Journal, V. 100, No. 3, May-June 2003, pp. 383-391.


ALSO AVAILABLE IN: