Influence of Mixture Proportions and Permeability- Reducing Admixtures on Concrete Fluid Transport

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Influence of Mixture Proportions and Permeability- Reducing Admixtures on Concrete Fluid Transport

Author(s): R. M. Ghantous, V. Bui, S. Schaef, B. Fronczek, C. B. Jablonski, S. R. Reese, and W. J. Weiss

Publication: Materials Journal

Volume: 120

Issue: 6

Appears on pages(s): 107-120

Keywords: concrete mixture design; degree of saturation (DOS); interfacial transition zone (ITZ); neutron radiography (NR); permeability; permeabilityreducing admixtures (PRAs); visual inspection

DOI: 10.14359/51739150

Date: 12/1/2023

Abstract:
This study uses neutron radiography (NR) and visual inspection to quantify water penetration in concrete samples exposed to water pressure on one face. It provides experimental data regarding the impact of mixture proportions on the hydraulic permeability of concrete. Specifically, it illustrates the influence of water-cement ratio (w/c), curing duration, entrained air content, and coarse aggregate (CA) size and volume on water transport. In addition, this paper quantifies the impact of permeability-reducing admixtures (PRAs) on water transport in concrete. It was observed that decreasing the w/c and/or increasing the curing duration reduced the fluid transport. Liquid and powder PRAs efficiently reduced fluid transport in concrete without impacting the compressive strength. The liquid PRA showed more consistent results, likely due to better dispersion than the powder PRA. Fluid ingress in concrete samples appears to increase with entrained air content due to a lower degree of saturation (DOS) at the start of the test. Increasing the CA volume fraction or decreasing the CA size will increase the fluid transport in concrete due to an increase in the connectivity of the interfacial transition zone. The influence of entrained air content, curing duration, CA volume fraction, and CA size was less noticeable on mixtures with PRAs due to the higher density and low permeability of these samples compared to control samples.

Related References:

1. Graveen, C.; Falker, E. M.; Beaver, M.; Neithalath, N.; Weiss, W. J.; Olek, J.; Nantung, T. E.; and Gallivan, V. L., “Performance Related Specifications (PRS) for Concrete Pavements in Indiana, Volume 1: Executive Summary,” Report No. FHWA/IN/JTRP-2004/13-1, Joint Transportation Research Program, Indiana Department of Transportation and Purdue University, West Lafayette, IN, 2009. doi: 10.5703/1288284314213

2. Graveen, C.; Falker, E. M.; Beaver, M.; Neithalath, N.; Weiss, W. J.; Olek, J.; Nantung, T. E.; and Gallivan, V. L., “Performance Related Specifications (PRS) for Concrete Pavements in Indiana, Volume 2: Technical Report,” Report No. FHWA/IN/JTRP-2004/13-2, Joint Transportation Research Program, Indiana Department of Transportation and Purdue University, West Lafayette, IN, 2009. doi: 10.5703/1288284314214

3. Weiss, W. J., “Concrete Pavement Joint Durability: A Sorption-Based Model for Saturation, the Role of Distributed Cracking, and Calcium Oxychloride Formation,” Concreep 10: Proceedings of the 10th International Conference on Mechanics and Physics of Creep, Shrinkage, and Durability of Concrete and Concrete Structures, C. Hellmich, B. Pichler, and J. Kollegger, eds., Vienna, Austria, 2015, pp. 211-218.

4. Mackechnie, J. R., and Alexander, M. G., “Using Durability to Enhance Concrete Sustainability,” Journal of Green Building, V. 4, No. 3, 2009, pp. 52-60. doi: 10.3992/jgb.4.3.52

5. Weiss, J., and Shields-Cook, S., “Relating Transport Properties to Performance in Concrete Pavements,” CP Road Map MAP Brief, National Concrete Pavement Technology Center, Iowa State University of Science and Technology, Ames, IA, 2014, 6 pp.

6. Chini, A. R.; Muszynski, L. C.; and Hicks, J. K., “Determination of Acceptance Permeability Characteristics for Performance-Related Specifications for Portland Cement Concrete,” final report, Florida Department of Transportation, Tallahassee, FL, 2003, 162 pp.

7. Bentz, D. P.; Clifton, J. R.; Ferraris, C. F.; Garboczi, E. J.; and Torrents, J. M., “Transport Properties and Durability of Concrete: Literature Review and Research Plan,” NISTIR 6395, National Institute of Standards and Technology, Gaithersburg, MD, 1999.

8. Garboczi, E. J., “Permeability, Diffusivity, and Microstructural Parameters: A Critical Review,” Cement and Concrete Research, V. 20, No. 4, 1990, pp. 591-601. doi: 10.1016/0008-8846(90)90101-3

9. Meletiou, C. A.; Tia, M.; and Bloomquist, D., “Development of a Field Permeability Test Apparatus and Method for Concrete,” ACI Materials Journal, V. 89, No. 1, Jan.-Feb. 1992, pp. 83-89.

10. Saricimen, H.; Maslehuddin, M.; Al-Tayyib, A. J.; and Al-Mana, A. I., “Permeability and Durability of Plain and Blended Cement Concretes Cured in Field and Laboratory Conditions,” ACI Materials Journal, V. 92, No. 2, Mar.-Apr. 1995, pp. 111-116.

11. Shattaf, N. R.; Alshamsi, A. M.; and Swamy, R. N., “Curing/Environment Effect on Pore Structure of Blended Cement Concrete,” Journal of Materials in Civil Engineering, ASCE, V. 13, No. 5, 2001, pp. 380-388. doi: 10.1061/(ASCE)0899-1561(2001)13:5(380)

12. Philipose, K. E.; Feldman, R. F.; and Beaudoin, J. J., “Durability Predictions from Rate of Diffusion Testing of Normal Portland Cement, Fly Ash, and Slag Concrete,” AECL-10489, Atomic Energy of Canada Limited, Chalk River, ON, Canada, 1991, 24 pp.

13. Munn, R. L.; Chang, Z. T.; and Kao, G., “Performance of Australian Commercial Concretes Modified with a Permeability Reducing Admixture,” Proceedings of the 22nd Biennial Conference of the Concrete Institute of Australia, Melbourne, VIC, Australia, 2005, pp. 17-19.

14. Riding, K. A.; Tibbetts, C. M.; and Ferraro, C. C., “Testing Methods to Assess the Durability of Concrete Permeability Reducing Admixtures,” final report, Florida Department of Transportation, Tallahassee, FL, 2020, 69 pp.

15. Biparva, A., and Gupta, R., “Smart Waterproofing System: A Review,” Proceedings, International Conference on Future Concrete, Doha, Qatar, 2010, 10 pp.

16. Muhammad, N. Z.; Keyvanfar, A.; Majid, M. Z. A.; Shafaghat, A.; and Mirza, J., “Waterproof Performance of Concrete: A Critical Review on Implemented Approaches,” Construction and Building Materials, V. 101, Part 1, 2015, pp. 80-90. doi: 10.1016/j.conbuildmat.2015.10.048

17. Giannini, E. R.; Lindly, J. K.; and Dunn, J. R., “Comparative Evaluation of Concrete Bridge Deck Sealers,” ALDOT Report No. 930-861, Alabama Department of Transportation, Montgomery, AL, 2015, 103 pp.

18. ACI Committee 212, “Report on Chemical Admixtures for Concrete (ACI 212.3R-16),” American Concrete Institute, Farmington Hills, MI, 2016, 76 pp.

19. Pfeifer, D. W., and Scali, M. J., “Concrete Sealers for Protection of Bridge Structures,” NCHRP Report No. 244, Transportation Research Board, Washington, DC, 1981, 148 pp.

20. Pincheira, J. A., and Dorshorst, M. A., “Evaluation of Concrete Deck and Crack Sealers,” Report No. WHRP 06-09, Wisconsin Highway Research Program, Madison, WI, 2005, 164 pp.

21. Almusallam, A. A.; Khan, F. M.; Dulaijan, S. U.; and Al-Amoudi, O. S. B., “Effectiveness of Surface Coatings in Improving Concrete Durability,” Cement and Concrete Composites, V. 25, No. 4-5, 2003, pp. 473-481. doi: 10.1016/S0958-9465(02)00087-2

22. Tibbetts, C. M.; Riding, K. A.; and Ferraro, C. C., “A Critical Review of the Testing and Benefits of Permeability-Reducing Admixtures for Use in Concrete,” Cement, V. 6, 2021, Article No. 100016. doi: 10.1016/j.cement.2021.100016

23. Hooton, R. D., “What is Needed in a Permeability Test for Evaluation of Concrete Quality,” MRS Online Proceedings Library, V. 137, 1988, pp. 141-149. doi: 10.1557/PROC-137-141

24. Hassani Esgandani, M.; Vessalas, K.; Baweja, D.; and Schmidt, Z., “Effect of Chemical Admixtures on Water Penetration of Concrete,” RILEM International Workshop on Performance-Based Specification and Control of Concrete Durability, Paris, France, 2014.

25. Hassani, M.; Vessalas, K.; Sirivivatnanon, V.; and Baweja, D., “Influence of Permeability-Reducing Admixtures on Water Penetration in Concrete,” ACI Materials Journal, V. 114, No. 6, Nov.-Dec. 2017, pp. 911-922.

26. Pazderka, J., and Hájková, E., “Crystalline Admixtures and Their Effect on Selected Properties of Concrete,” Acta Polytechnica, V. 56, No. 4, 2016, pp. 306-311. doi: 10.14311/AP.2016.56.0306

27. Silva, E. F.; Moreira, M.; Manzano, M. A. R.; and Blanco, R., “Case Study of Permeability-Reducing Admixture Use in Anti-Flotation Slabs: Building in Brasilia, Brazil,” Journal of Building Pathology and Rehabilitation, V. 2, No. 1, 2017, Article No. 1. doi: 10.1007/s41024-016-0014-5

28. Kapustin, F. L., and Pomazkin, E. P., “Effect of Waterproofing Penetrating Capillary Mixture on Concrete Waterproofness and Cement Stone Microstructure,” Power Technology and Engineering, V. 52, No. 2, 2018, pp. 168-171. doi: 10.1007/s10749-018-0927-z

29. Mačanovskis, A.; Krasņikovs, A.; Spruģe, I.; Šahmenko, G.; and Lukašenoks, A., “Mechanical Properties and Self-Healing Effect of Concrete Containing Capillary Hydro Insulation Admixture,” Rīgas Tehniskās Universitātes Zinātniskie Raksti, V. 18, No. 1, 2016, pp. 17-21. doi: 10.1515/cons-2016-0003

30. Teng, L.-W.; Huang, R.; Chen, J.; Cheng, A.; and Hsu, H.-M., “A Study of Crystalline Mechanism of Penetration Sealer Materials,” Materials (Basel), V. 7, No. 1, 2014, pp. 399-412. doi: 10.3390/ma7010399

31. DIN 1048-5:1991, “Testing of Hardened Concrete,” Deutsches Institut für Normung, Berlin, Germany, 1991.

32. Ghantous, R. M.; Fronczek, B.; Jablonski, C. B.; Bui, V.; Schaef, S.; Reese, S. R.; and Weiss, W. J., “Using Neutron Radiography to Assess Parameters Associated with Water Permeability Testing,” Advances in Civil Engineering Materials, V. 12, No. 1, 2023, 21 pp. doi: 10.1520/ACEM20220061

33. Moradllo, M. K.; Montanari, L.; Suraneni, P.; Reese, S. R.; and Weiss, J., “Examining Curing Efficiency Using Neutron Radiography,” Transportation Research Record: Journal of the Transportation Research Board, V. 2672, No. 27, 2018, pp. 13-23. doi: 10.1177/0361198118773571

34. Gadd, M. S., “Characterization of the Oregon State University Neutron Radiography Facility,” LA-UR-07–5375, Los Alamos National Laboratory, Los Alamos, NM, 2007.

35. Ghantous, R. M.; Valadez-Carranza, Y.; Reese, S. R.; and Weiss, W. J., “Drying Behavior of 3D Printed Cementitious Pastes Containing Cellulose Nanocrystals,” Cement, V. 9, 2022, Article No. 100035. doi: 10.1016/j.cement.2022.100035

36. Hussey, D. S.; Spernjak, D.; Weber, A. Z.; Mukundan, R.; Fairweather, J.; Brosha, E. L.; Davey, J.; Spendelow, J. S.; Jacobson, D. L.; and Borup, R. L., “Accurate Measurement of the Through-Plane Water Content of Proton-Exchange Membranes Using Neutron Radiography,” Journal of Applied Physics, V. 112, No. 10, 2012, Article No. 104906. doi: 10.1063/1.4767118

37. Schneider, C. A.; Rasband, W. S.; and Eliceiri, K. W., “NIH Image to ImageJ: 25 Years of Image Analysis,” Nature Methods, V. 9, No. 7, 2012, pp. 671-675. doi: 10.1038/nmeth.2089

38. AASHTO TP 135-20, “Standard Method of Test for Determining the Total Pore Volume in Hardened Concrete Using Vacuum Saturation,” American Association of State Highway and Transportation Officials, Washington, DC, 2020, 7 pp.

39. Bu, Y.; Spragg, R.; and Weiss, W. J., “Comparison of the Pore Volume in Concrete as Determined Using ASTM C642 and Vacuum Saturation,” Advances in Civil Engineering Materials, V. 3, No. 1, 2014, pp. 308-315. doi: 10.1520/ACEM20130090

40. Goodwin, M. N.; Ghantous, R. M.; Weiss, W. J.; and Reese, S. R., “Neutron Radiography of Cement Paste Made with Light and Heavy Water,” Journal of Radioanalytical and Nuclear Chemistry, V. 331, No. 12, 2022, pp. 5113-5121. doi: 10.1007/s10967-022-08493-w

41. Rangaraju, P. R., “Development of Some Performance-Based Material Specifications for High-Performance Concrete Pavement,” Transportation Research Record: Journal of the Transportation Research Board, V. 1834, No. 1, 2003, pp. 69-76. doi: 10.3141/1834-09

42. Neville, A. M., Properties of Concrete, fourth edition, Addison Wesley Longman Limited, Boston, MA, 1995.

43. Powers, T. C., “A Discussion of Cement Hydration in Relation to the Curing of Concrete,” Proceedings of the 27th Annual Meeting of the Highway Research Board, V. 27, 1948, pp. 178-188.

44. Bharadwaj, K.; Glosser, D.; Moradllo, M. K.; Isgor, O. B.; and Weiss, W. J., “Toward the Prediction of Pore Volumes and Freeze-Thaw Performance of Concrete Using Thermodynamic Modelling,” Cement and Concrete Research, V. 124, 2019, Article No. 105820. doi: 10.1016/j.cemconres.2019.105820

45. Breton, D.; Carles-Gibergues, A.; Ballivy, G.; and Grandet, J., “Contribution to the Formation Mechanism of the Transition Zone between Rock-Cement Paste,” Cement and Concrete Research, V. 23, No. 2, 1993, pp. 335-346. doi: 10.1016/0008-8846(93)90099-U

46. Scrivener, K. L., and Nemati, K. M., “The Percolation of Pore Space in the Cement Paste/Aggregate Interfacial Zone of Concrete,” Cement and Concrete Research, V. 26, No. 1, 1996, pp. 35-40. doi: 10.1016/0008-8846(95)00185-9

47. Shane, J. D.; Mason, T. O.; Jennings, H. M.; Garboczi, E. J.; and Bentz, D. P., “Effect of the Interfacial Transition Zone on the Conductivity of Portland Cement Mortars,” Journal of the American Ceramic Society, V. 83, No. 5, 2000, pp. 1137-1144. doi: 10.1111/j.1151-2916.2000.tb01344.x

48. Halamickova, P.; Detwiler, R. J.; Bentz, D. P.; and Garboczi, E. J., “Water Permeability and Chloride Ion Diffusion in Portland Cement Mortars: Relationship to Sand Content and Critical Pore Diameter,” Cement and Concrete Research, V. 25, No. 4, 1995, pp. 790-802. doi: 10.1016/0008-8846(95)00069-O

49. Pope, A. W., and Jennings, H. M., “The Influence of Mixing on the Microstructure of the Cement Paste/Aggregate Interfacial Zone and on the Strength of Mortar,” Journal of Materials Science, V. 27, No. 23, 1992, pp. 6452-6462. doi: 10.1007/BF00576298

50. Alexander, M. G.; Mindess, S.; Diamond, S.; and Qu, L., “Properties of Paste-Rock Interfaces and Their Influence on Composite Behaviour,” Materials and Structures, V. 28, No. 9, 1995, pp. 497-506. doi: 10.1007/BF02473154


ALSO AVAILABLE IN:

Electronic Materials Journal