Title: Carbon-Negative Pilot

Author(s): Yao Wang, Mija Hubler, Rakshita Ramesh Bhat, Wil V. Srubar III, Shane Frazier, Loren Burnett, Linfei Li, Ben Stanley, Ryan Dick, and Sean James

Publication: Concrete International

Volume: 45

Issue: 8

Appears on pages(s): 49-53

Keywords: wall, biogenic, limestone, algae

DOI: 10.14359/51739101

Date: 8/1/2023

Abstract:
The article discusses testing of a system designed to achieve overall carbon negativity. The system comprises a concrete slab supporting a wall constructed using concrete masonry units (CMUs). The concrete slab was made of alkali-activated cement containing algae-derived carbon-storing, biogenic limestone. The CMUs contain biomineralizing microalgae and a proprietary hydrogel binder as cement replacement.

Related References:

1. Nanayakkara, O.; Gunasekara, C.; Sandanayake, M.; Law, D.W.; Nguyen, K.; Xia, J.; and Setunge, S., “Alkali-Activated Slag Concrete Incorporating Recycled Aggregate Concrete: Long-Term Performance and Sustainability Aspect,” Construction and Building Materials, V. 271, Feb. 2021.

2. Weil, M.; Dombrowski-Daube, K.; and Buchwald, A., “Life-Cycle Analysis of Geopolymers,” Geopolymers, J. Provis and J. Deventer, eds., Woodhead Publishing Ltd., Sawston, UK, 2009, pp. 194-210.

3. Heveran, C.M.; Williams, S.L.; Qiu, J.; Artier, J.; Hubler, M.H.; Cook, S.M.; Cameron, J.C.; and Srubar III, W.V., “Biomineralization and Successive Regeneration of Engineered Living Building Materials,” Matter, V. 2, No. 2, Feb. 2020, pp. 481-494.

4. Qiu J.; Artier J.; Cook S.; Srubar W.; Cameron J.; and Hubler M., “Engineering Living Building Materials for Enhanced Bacterial Viability and Mechanical Properties,” IScience, V. 24, No. 2, Feb. 2021.

5. “ISO 14040:2006: Environmental Management — Life Cycle Assessment — Principles and Framework,” International Organization for Standardization, Geneva, Switzerland, 2006, 20 pp.