Title: CPC Position Statement #6: Surface Repairs Prior to Polishing Concrete

Author(s): contractor, appearance, material, cost

Publication: Concrete International

Volume: 45

Issue: 7

Appears on pages(s): 47

Keywords:

DOI:

Date: 7/1/2023

Abstract:
Most floors to be polished require surface repairs due to concrete placement and finishing, as well as damage from continued use of the surface for construction operations. This position statement provides recommendations on repair materials selection, proper execution of a repair, and urges the owner to set aside time and money for possible repairs on a project.




  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

Edit Module Settings to define Page Content Reviewer