Title: GFRP Reinforced Concrete Slabs under Restrained Shrinkage

Author(s): Bryan E. Barragan, Antonio Mudadu, Giuseppe Tiberti, and Giovanni A. Plizzari

Publication: Concrete International

Volume: 45

Issue: 7

Appears on pages(s): 39-45

Keywords: bar, reinforcement, cracking, steel

DOI:

Date: 7/1/2023

Abstract:
The article presents results from an experimental study on the effectiveness of glass fiber-reinforced polymer (GFRP) bars as shrinkage reinforcement for slabs-on-ground. Slabs reinforced with steel and GFRP bars were cast inside steel frames providing a high degree of restraint to shrinkage deformations and allowing for a better evaluation of different reinforcement solutions.




  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

Edit Module Settings to define Page Content Reviewer