Lab-Mixed versus Truck-Mixed UHPC—What’s the Difference?

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Lab-Mixed versus Truck-Mixed UHPC—What’s the Difference?

Author(s): Sherif El-Tawil, M.A. Saqif, Dewayne Rogers, and Yuh-Shiou Tai

Publication: Concrete International

Volume: 45

Issue: 1

Appears on pages(s): 40-45

Keywords: mixer, mixture, strength, spread

DOI: 10.14359/51738465

Date: 1/1/2023

Abstract:
One of the hurdles to adoption of ultra-high-performance concrete (UHPC) technology is the widespread belief that UHPC is difficult to mix. This article presents a study on mixing UHPC in common concrete field mixers and ready mixed concrete trucks and compares fresh and hardened properties of UHPC produced using these systems with laboratory mixtures.

Related References:

1. Wille, K.; El-Tawil, S.; and Naaman, A.E., “Properties of Strain Hardening Ultra High Performance Fiber Reinforced Concrete (UHP-FRC) Under Direct Tensile Loading,” Cement and Concrete Composites, V. 48, Apr. 2014, pp.53-66.

2. Wille, K.; Naaman, A.E.; and El-Tawil, S., “Optimizing Ultra-High-Performance Fiber-Reinforced Concrete,” Concrete International, V. 33, No. 9, Sept. 2011, pp. 35-41.

3. “Ultra High Performance Concrete,” keyword search, Google Scholar, 2021 https://scholar.google.com/scholar?hl=en&as_sdt=0,23&q=%22ultra-high+performance+concrete%22&scisbd=1.

4. “Every Day Counts,” Federal Highway Administration, McLean, VA, 2021, www.fhwa.dot.gov/innovation/everydaycounts/about-edc.cfm. Accessed Jun. 23, 2022.

5. ASTM C1856/C1856M-17, “Standard Practice for Fabricating and Testing Specimens of Ultra-High Performance Concrete,” ASTM International, West Conshohocken, PA, 2017, 4 pp.

6. ACI Committee 239, “Ultra-High-Performance Concrete: An Emerging Technology Report (ACI 239R-18),” American Concrete Institute, Farmington Hills, MI, 2018, 21 pp.

7. El-Tawil, S.; Tai, Y.-S.; and Belcher II, J.A., “Field Application of Nonproprietary Ultra-High-Performance Concrete,” Concrete International, V. 40, No. 1, Jan. 2018, pp. 30-36.

8. Alkaysi, M., and El-Tawil, S., “Effects of Variations in the Mix Constituents of Ultra High Performance Concrete (UHPC) on Cost and Performance,” Materials and Structures, V. 49, No. 10, Oct. 2016, pp. 4185-4200.

9. El-Tawil, S.; Tai, Y.-S.; Meng, B.; Hansen, W.; and Liu, Z., “Commerical Production of Non-Proprietary Ultra High Performance Concrete,” RC-1670, Michigan Department of Transportation, Lansing, MI, 2018, 162 pp.

10. Tai, Y.-S., and El-Tawil, S., “Effect of Component Materials and Mixing Protocol on the Short-Term Performance of Generic Ultra-High-Performance Concrete,” Construction and Building Materials, V. 238, Mar. 2020.

11. ASTM C1437-15, “Standard Test Method for Flow of Hydraulic Cement Mortar,” ASTM International, West Conshohocken, PA, 2015, 2 pp.

12. ASTM C1611/C1611M-21, “Standard Test Method for Slump Flow of Self-Consolidating Concrete,” ASTM International, West Conshohocken, PA, 2021, 6 pp.

13. Graybeal, B.A., “Material Property Characterization of Ultra-High Performance Concrete,” FHWA-HRT-06-103, Federal Highway Administration, McLean, VA, Aug. 2006, 176 pp.

14. Graybeal, B.A., and Baby, F., “Tension Testing of Ultra-High Performance Concrete,” FHWA-HRT-17-053, Federal Highway Administration, McLean, VA, Feb. 2019, 206 pp.

15. Park, S.; Wu, S.; Liu, Z.; and Pyo, S., “The Role of Supplementary Cementitious Materials (SCMs) in Ultra High Performance Concrete (UHPC): A Review,” Materials, V. 14, No. 6, Mar. 2021, p. 1472.

16. El-Tawil, S.; Tai, Y-S.; Belcher II, J.A.; and Rogers, D., “Open-Recipe Ultra-High-Performance Concrete,” Concrete International, V. 42, No. 6, June 2020, pp. 33-38.