Assessment of Sustainability and Self-Healing Performances of Recycled Ultra-High-Performance Concrete

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Assessment of Sustainability and Self-Healing Performances of Recycled Ultra-High-Performance Concrete

Author(s): N. P. Kannikachalam, D. di Summa, R. P. Borg, E. Cuenca, M. Parpanesi, N. De Belie, and L. Ferrara

Publication: Materials Journal

Volume: 120

Issue: 1

Appears on pages(s): 117-132

Keywords: life cycle assessment; recycled aggregate; self-healing; sustainability; ultra-high-performance concrete (UHPC)

DOI: 10.14359/51737336

Date: 1/1/2023

Abstract:
This research focuses on the evaluation of the sustainability of recycled ultra-high-performance concrete (R-UHPC) in a life cycle analysis (LCA) perspective, and with reference to a case study example dealing with structures exposed to extremely aggressive environments. This involves the assessment of the self-healing capacity of R-UHPC, as guaranteed by the R-UHPC aggregates themselves. Recycled aggregates (RA) were created by crushing 4-month-old UHPC specimens with an average compressive strength of 150 MPa. Different fractions of recycled aggregates (0 to 2 mm) and two different percentages (50 and 100%) were used as a substitute for natural aggregates in the production of R-UHPC. Notched beam specimens were pre-cracked to 150 μm using a three-point flexural test. The autogenous self-healing potential of R-UHPC, stimulated by the addition of a crystalline admixture, was explored using water absorption tests and microscopic crack healing at a pre-determined time (0 days, 1 month, 3 months, and 6 months) following pre-cracking. Continuous wet/ dry healing conditions were maintained throughout the experimental campaign. The specimens using R-UHPC aggregates demonstrated improved self-healing properties to those containing natural aggregates, especially from the second to the sixth month. To address the potential environmental benefits of this novel material in comparison to the conventional ones, an LCA analysis was conducted adopting the 10 CML-IA baseline impact categories, together with a life cycle cost (LCC) analysis to determine the related economic viability. Both LCA and LCC methodologies are integrated into a holistic design approach to address not only the sustainability concerns but also to promote the spread of innovative solutions for the concrete construction industry. As a case study unit, a basin for collection and cooling of geothermal waters was selected. This is representative of both the possibility offered, in terms of structural design optimization and reduction of resource consumption, and of reduced maintenance guaranteed by the retained mechanical performance and durability realized by the self-healing capacity of R-UHPC.

Related References:

Agustí-Juan, I.; Müller, F.; Hack, N.; Wangler, T.; and Habert, G., 2017, “Potential Benefits of Digital Fabrication for Complex Structures: Environmental Assessment of a Robotically Fabricated Concrete Wall,” Journal of Cleaner Production, V. 154, pp. 330-340. doi: 10.1016/j.jclepro.2017.04.002

Akhtar, A., and Sarmah, A. K., 2018, “Construction and Demolition Waste Generation and Properties of Recycled Aggregate Concrete: A Global Perspective,” Journal of Cleaner Production, V. 186, pp. 262-281. doi: 10.1016/j.jclepro.2018.03.085

Al-Obaidi, S.; Bamonte, P.; Animato, F.; Lo Monte, F.; Mazzantini, I.; Luchini, M.; Scalari, S.; and Ferrara, L., 2021, “Innovative Design Concept of Cooling Water Tanks/Basins in Geothermal Power Plants using Ultra High Performance Fiber Reinforced Concrete with Enhanced Durability,” Sustainability, V. 13, No. 17, pp. 1-26. doi: 10.3390/su13179826

Al-Obaidi, S.; Bamonte, P.; Luchini, M.; Mazzantini, I.; and Ferrara, L., 2020, “Durability-Based Design of Structures Made with UHP/UHDC in Extremely Aggressive Scenarios: Application to a Geothermal Water Basin Case Study,” Infrastructures, V. 5, No. 11, pp. 1-44. doi: 10.3390/infrastructures5110102

Alonso, M. C.; Gimenez, M.; Menendez, E.; Serna, P.; Valcuende, M.; Soto, J.; Suesta, C.; Fort, L.; Camacho, E.; Scalari, S.; Borg, R. P.; and Deegan, P., 2018, “Definition of Key Durability Parameters for Each Scenario,” ReSHEALience Project Deliverable D3.2.

Alonso, M. C., and Sanchez, M., 2009, “Analysis of the Variability of Chloride Threshold Values in the Literature,” Materials and Corrosion, V. 60, No. 8, pp. 631-637. doi: 10.1002/maco.200905296

Bai, G.; Zhu, C.; Liu, C.; and Liu, B., 2020, “An Evaluation of the Recycled Aggregate Characteristics and the Recycled Aggregate Concrete Mechanical Properties,” Construction and Building Materials, V. 240, Apr., p. 117978.

Behera, M.; Bhattacharyya, S. K.; Minocha, A. K.; Deoliya, R.; and Maiti, S., 2014, “Recycled Aggregate from C&D Waste & its Use in Concrete – A Breakthrough Towards Sustainability in Construction Sector: A Review,” Construction and Building Materials, V. 68, pp. 501-516. doi: 10.1016/j.conbuildmat.2014.07.003

Bertolini, L.; Elsener, B.; and Pedeferri, P., 2004, Corrosion of Steel in Concrete, McGraw Hill, New York.

Blengini, G. A., and Garbarino, E., 2010, “Resources and Waste Management in Turin (Italy): The Role of Recycled Aggregates in the Sustainable Supply Mix,” Journal of Cleaner Production, V. 18, No. 10-11, pp. 1021-1030. doi: 10.1016/j.jclepro.2010.01.027

Borg, R. P.; Cuenca, E.; Garofalo, R.; Schillani, F.; Lozano-Nasner, M.; and Ferrara, L., 2021, “Performance Assessment of Ultra High Durability Concrete Produced from Recycled Ultra High Durability Concrete,” Frontiers in Built Environment, pp. 1-20. doi: 10.3389/fbuil.2021.648220

Borg, R. P.; Hajek, P.; and Fernandez Ordonez, D., 2018, “Sustainable Concrete: Materials and Structures,” Proceedings of fib Conference: Sustainable Concrete: Materials and Structures, Materials Science and Engineering, IOP Conf. Series, 442 pp. doi:10.1088/1757-899X/442/1/011001

Bossio, A.; Lignola, G. P.; Fabbrocino, F.; Monetta, T.; Prota, A.; Bellucci, F.; and Manfredi, G., 2017, “Nondestructive Assessment of Corrosion of Reinforcing Bars Through Surface Concrete Cracks,” Structural Concrete, V. 18, No. 1, pp. 104-117. doi: 10.1002/suco.201600034

Caruso, M. C.; Pascale, C.; Camacho, E.; and Ferrara, L., 2022, “Comparative Environmental and Social Life Cycle Assessments of Off-Shore Aquaculture Rafts Made in Ultra-High-Performance Concrete (UHPC),” The International Journal of Life Cycle Assessment, V. 27, No. 2, pp. 281-300. doi: 10.1007/s11367-021-02017-6

Chen, W.; Jin, R.; Xu, Y.; Wanatowski, D.; Li, B.; Yan, L.; Pan, Z.; and Yang, Y., 2019, “Adopting Recycled Aggregates as Sustainable Construction Materials: A Review of the Scientific Literature,” Construction and Building Materials, V. 218, pp. 483-496. doi: 10.1016/j.conbuildmat.2019.05.130

Commission Delegated Regulation, 2012, Commission Delegated Regulation (EU), 2012 No 244/2012 of 16 January 2012 supplementing Directive 2010/31/EU of the European Parliament and of the Council on the energy performance of buildings by establishing a comparative methodology framework for calculation.

Cuenca, E.; Criado, M.; Gimenez, M.; Alonso, M. C.; and Ferrara, L., 2022, “Effects of Alumina Nanofibers and Cellulose Nanocrystals on Durability and Self-Healing Capacity of Ultrahigh-Performance Fiber-Reinforced Concretes,” Journal of Materials in Civil Engineering, ASCE, V. 34, No. 8, pp. 8-17. doi: 10.1061/(ASCE)MT.1943-5533.0004375

Cuenca, E.; Lo Monte, F.; Moro, M.; Schiona, A.; and Ferrara, L., 2021, “Effects of Autogenous and Stimulated Self-Healing on Durability and Mechanical Performance of UHPFRC: Validation of Tailored Test Method Through Multi-Performance Healing-Induced Recovery Indices,” MDPI Sustainability, V. 13, pp. 1-24. doi: 10.3390/su132011386

di Summa, D.; Tenorio Filho, J. R.; Snoeck, D.; Van den Heede, P.; Van Vlierberghe, S.; Ferrara, L.; and De Belie, N., 2022, “Environmental and Economic Sustainability of Crack Mitigation in Reinforced Concrete with SuperAbsorbent Polymers (SAPs),” Journal of Cleaner Production, V. 358, p. 131998. doi: 10.1016/j.jclepro.2022.131998

Emilia-Romagna, “Provveditorato interregionale alle Opere Pubbliche di Lombardia,” C.D.M., PREZZARIO REGIONALE delle opere pubbliche, https://territorio.regione.emilia-romagna.it/osservatorio/Elenco-regionale-prezzi. (last accessed Jan. 19, 2023)

EN 15804:2012, 2012, “Sustainability of Construction Works, Environmental Product Declarations, Core Rules for the Product Category of Construction Products,” European Committee for Standardization, Brussels, Belgium.

EN 16627:2015, 2015, “Sustainability of Construction Works – Assessment of Economic Performance of Buildings – Calculation Methods,” European Committee for Standardization, Brussels, Belgium.

EN 1990:2002, 2002, “Eurocode – Basis of Structural Design,” European Committee for Standardization, Brussels, Belgium.

FEICA, 2015, “Environmental Product Declaration – Reactive Resins Based on Epoxy Resin, Filled and/or Aqueous with Low Content of Filler,” Association of the European Adhesive and Sealant Industry, Brussels, Belgium.

Ferrara, L.; Krelani, V.; and Moretti, F., 2016, “Autogenous Healing on the Recovery of Mechanical Performance of High-Performance Fibre Reinforced Cementitious Composites (HPFRCCS): Part 2 – Correlation Between Healing of Mechanical Performance and Crack Sealing,” Cement and Concrete Composites, V. 73, pp. 299-315. doi: 10.1016/j.cemconcomp.2016.08.003

Ferrara, L.; Krelani, V.; Moretti, F.; Roig Flores, M.; and Serna Ros, P., 2017, “Effects of Autogenous Healing on the Recovery of Mechanical Performance of High-Performance Fibre Reinforced Cementitious Composites (HPFRCCS): Part,” Cement and Concrete Composites, V. 83, pp. 76-100. doi: 10.1016/j.cemconcomp.2017.07.010

Fraj, A. B., and Idir, R., 2017, “Concrete Based on Recycled Aggregates – Recycling and Environmental Analysis: A Case Study of Paris’ Region,” Construction and Building Materials, V. 157, pp. 952-964. doi: 10.1016/j.conbuildmat.2017.09.059

Hu, M.; Di Maio, F.; Lin, X.; and Van Roekel, E., 2012, “Fates of End-of-Life Concrete and Their Economic Implications,” 27th International Conference on Solid Waste Technology and Management, pp. 1-9.

Knoeri, C.; Sanyé-Mengual, E.; and Althaus, H.-J., 2013, “Comparative LCA of Recycled and Conventional Concrete for Structural Applications,” The International Journal of Life Cycle Assessment, V. 18, pp. 909-918.

Lehne, J., and Preston, F., 2018, “Making Concrete Change: Innovation in Low-Carbon Cement and Concrete,” Chatham House, The Royal Institute of International Affairs, London, UK.

Lo Monte, F., and Ferrara, L., 2020, “Tensile Behaviour Identification in Ultra-High-Performance Fibre Reinforced Cementitious Composites: Indirect Tension Tests and Back Analysis of Flexural Test Results,” Materials and Structures, V. 53, pp. 1-12. doi: 10.1617/s11527-020-01576-8

Lo Monte, F., and Ferrara, L., 2021, “Self-Healing Characterization of UHPFRCC with Crystalline Admixture: Experimental Assessment via Multi-Test/Multi-Parameter Approach,” Construction and Building Materials, V. 283, pp. 1-12. doi: 10.1016/j.conbuildmat.2021.122579

López Ruiz, L. A.; Roca Ramón, X.; and Gassó Domingo, S., 2020, “The Circular Economy in the Construction and Demolition Waste Sector – A Review and an Integrative Model Approach,” Journal of Cleaner Production, V. 248, p. 119238. doi: 10.1016/j.jclepro.2019.119238

Lotfi, S.; Eggimann, M.; Wagner, E.; Mróz, R.; and Deja, J., 2015, “Performance of Recycled Aggregate Concrete Based on a New Concrete Recycling Technology,” Construction and Building Materials, V. 95, pp. 243-256. doi: 10.1016/j.conbuildmat.2015.07.021

Lotfi, S., and Rem, P., 2016, “Recycling of End-of-Life Concrete Fines into Hardened Cement and Clean Sand,” Journal of Environmental Protection, V. 7, No. 6, pp. 934-950. doi: 10.4236/jep.2016.76083

Lotfi, S.; Rem, P.; Deja, J.; and Mróz, R., 2017, “An Experimental Study on the Relation Between Input Variables and Output Quality of a New Concrete Recycling Process,” Construction and Building Materials, V. 137, pp. 128-140. doi: 10.1016/j.conbuildmat.2017.01.085

Ministero dell’Ambiente, 2018, “DECRETO 1 febbraio 2018,” https://www.gazzettaufficiale.it/atto/serie_generale/caricaDettaglioAtto/originario?atto.dataPubblicazioneGazzetta=2018-02-08&atto.codiceRedazionale=18A00818. (last accessed Jan. 19, 2023)

Nováková, I., and Mikulica, K., 2016, “Properties of Concrete with Partial Replacement of Natural Aggregate by Recycled Concrete Aggregates from Precast Production,” Procedia Engineering, V. 151, pp. 360-367. doi: 10.1016/j.proeng.2016.07.387

Parpanesi, M., 2021, “A Holistic Life-Cycle Design Approach to Structures with Advanced Cement-Based Materials,” MSc thesis, Department of Civil and Environmental Engineering, Politecnico di Milano, Milan, Italy.

Penetron, 2020, “Environmental Product Declaration—Penetron Products,” https://www.penetron.it/public/allegati_news/S-P-02038%20EPD.pdf. (last accessed Jan. 19, 2023)

Qian, D.; Yu, R.; Shui, Z.; Sun, Y.; Jiang, C.; Zhou, F.; Ding, M.; Tong, X.; and He, Y., 2020, “A Novel Development of Green Ultra-High-Performance Concrete (UHPC) Based on Appropriate Application of Recycled Cementitious Material,” Journal of Cleaner Production, V. 261, p. 121231. doi: 10.1016/j.jclepro.2020.121231

Regione Toscana, 2021, Prezzario dei Lavori della Toscana 2021 –Provincia di Siena. Prezzario, Regione Toscana, Italia.

Serna, P.; Roig, M.; Mezquida, E.; Peled, A.; Regev, O.; Ferrara, L.; Lo Monte, F.; Cuenca, E.; Reichardt, M.; Schröfl, C.; Mechtcherine, V.; Borg, R. P.; Camacho, E.; Lopez, J.A.; and Coll, H., 2019, “Guidelines for Mix Design Formulation of Functionalized UHDC and Adaption to Different Application Technologies,” ReSHEALience Project Deliverable D4.2.

Shi, C., and Chen. B., 2018, “Ultra-High-Performance Concrete Materials and Structures,” UHPC 2018, Proceedings of the 2nd International Conference, Fuzhou, China, Nov. 7-10, RILEM pubs. PRO 129.

Sabău, M., and Remolina Duran, J., “Prediction of Compressive Strength of General-Use Concrete Mixes with Recycled Concrete Aggregate,” International Journal of Pavement Research and Technology, V. 15, pp. 73-85. doi: 10.1007/s42947-021-00012-6

Silva, R. V.; de Brito, J.; and Dhir, R. K., 2019, “Use of Recycled Aggregates Arising from Construction and Demolition Waste in New Construction Applications,” Journal of Cleaner Production, V. 236, p. 117629.

Singh, V. K.; Shukla, A.; Sahani, R. K.; Shekhar, A. R.; and Singh, R., 2022, “Structural Application of Concrete Made of Recycled Aggregate Sourced from Construction and Demolition Waste,” Proceedings of SECON’21, pp. 863–872. doi: 10.1007/978-3-030-80312-4_74

Thomas, J.; Thaickavil, N. N.; and Wilson, P. M., 2018, “Strength and Durability of Concrete Containing Recycled Concrete Aggregates,” Journal of Building Engineering, V. 19, pp. 349-365. doi: 10.1016/j.jobe.2018.05.007

UNI EN 206:2016, 2016, “Concrete – Specification, Performance, Production and Conformity,” European Committee for Standardization, Brussels, Belgium.

UNEP, 2021, “Global Status Report for Buildings and Construction,” UN Environment Programme, Nairobi, Kenya.

USGS, 2021, “Mineral Commodity Summaries 2021,” U.S. Geological Survey, https://pubs.er.usgs.gov/publication/mcs2021. (last accessed Jan. 19, 2023)

Vandamme, M.; Ulm, F.-J.; and Fonollosa, P., 2010, “Nanogranular Packing of C–S–H at Substochiometric Conditions,” Cement and Concrete Research, V. 40, No. 1, pp. 14-26. doi: 10.1016/j.cemconres.2009.09.017

Villoria Sáez, P., and Osmani, M., 2019, “A Diagnosis of Construction and Demolition Waste Generation and Recovery Practice in the European Union,” Journal of Cleaner Production, V. 241, p. 118400. doi: 10.1016/j.jclepro.2019.118400

Wang, X.; Yu, R.; Shui, Z.; Song, Q.; Liu, Z.; Bao, M.; Liu, Z.; and Wu, S., 2019, “Optimized Treatment of Recycled Construction and Demolition Waste in Developing Sustainable Ultra-High-Performance Concrete,” Journal of Cleaner Production, V. 221, pp. 805-816. doi: 10.1016/j.jclepro.2019.02.201

Zhang, H.; Ji, T.; Zeng, X.; Yang, Z.; Lin, X.; and Liang, Y., 2018, “Mechanical Behavior of Ultra-High-Performance Concrete (UHPC) Using Recycled Fine Aggregate Cured Under Different Conditions and the Mechanism Based on Integrated Microstructural Parameters,” Construction and Building Materials, V. 192, pp. 489-507. doi: 10.1016/j.conbuildmat.2018.10.117

Zhang, L.; Liu, B.; Du, J.; Liu, C.; and Wang, S., 2019, “CO2 Emission Linkage Analysis in Global Construction Sectors: Alarming Trends from 1995 to 2009 and Possible Repercussions,” Journal of Cleaner Production, V. 221, pp. 863-877. doi: 10.1016/j.jclepro.2019.02.231


ALSO AVAILABLE IN:

Electronic Materials Journal