Performance of Lightweight Self-Consolidating Concrete Beams Reinforced with Glass Fiber-Reinforced Polymer Bars without Stirrups under Shear

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Performance of Lightweight Self-Consolidating Concrete Beams Reinforced with Glass Fiber-Reinforced Polymer Bars without Stirrups under Shear

Author(s): Shehab Mehany, Hamdy M. Mohamed, and Brahim Benmokrane

Publication: Structural Journal

Volume: 120

Issue: 1

Appears on pages(s): 17-30

Keywords: beams; design codes; glass fiber-reinforcing polymer (GFRP) bars; lightweight aggregate (LWA); lightweight self-consolidating concrete (LWSCC); load deflection; shear failure and cracking; shear strength; shear strength predictions; strain

DOI: 10.14359/51737229

Date: 1/1/2023

Abstract:
Integrating glass fiber-reinforced polymer (GFRP) bars into lightweight self-consolidating concrete (LWSCC) would effectively contribute to producing lighter and more durable reinforced concrete (RC) structures. Nonetheless, the shear behavior of GFRP RC structures cast with LWSCC has not yet been fully defined. This paper reports experimental results on the behavior and shear strength of LWSCC beams reinforced with GFRP bars. The beams measured 3100 mm (122.05 in.) long, 200 mm (7.87 in.) wide, and 400 mm (15.75 in.) deep. The test program included six beams reinforced with GFRP bars and one control beam reinforced with conventional steel bars for comparison purposes. The test variables were the reinforcement type and ratio and concrete density. The experimental results indicate that using LWSCC allowed for decreasing the self-weight of the RC beams (density of 1800 kg/m3 [112.4 lb/ft3]) compared to normalweight concrete (NWC). All beams failed as a result of diagonal tension cracking. Increasing the axial stiffness of the longitudinal GFRP reinforcing bars improved the concrete shear capacity of the LWSCC beams. The test results of this study and the results for 42 specimens in the literature were compared to the current fiber-reinforced polymer (FRP) shear design equations in the design guidelines, codes, and literature. Applying concrete density reduction factors of 0.8 and 0.75 in the ACI 440.1R-15 and CSA S806-12 shear design equations, respectively, to consider the influence of concrete density achieved an appropriate degree of conservatism equal to that of the equations for NWC beams.

Related References:

Abdelazim, W.; Mohamed, H. M.; Afifi, M. Z.; and Benmokrane, B., 2020, “Proposed Slenderness Limit for Glass Fiber-Reinforced Polymer-Reinforced Concrete Columns Based on Experiments and Buckling Analysis,” ACI Structural Journal, V. 117, No. 1, Jan., pp. 241-254. doi: 10.14359/51718073

ACI Committee 318, 2019, “Building Code Requirements for Structural Concrete (ACI 318-19) and Commentary (ACI 318R-19),” American Concrete Institute, Farmington Hills, MI, 623 pp.

ACI Committee 440, 2006, “Guide for the Design and Construction of Structural Concrete Reinforced with FRP Bars (ACI 440.1R-06),” American Concrete Institute, Farmington Hills, MI, 44 pp.

ACI Committee 440, 2015, “Guide for the Design and Construction of Structural Concrete Reinforced with FRP Bars (ACI 440.1R-15),” American Concrete Institute, Farmington Hills, MI, 88 pp.

Ali, A. H.; Mohamed, H. M.; and Benmokrane, B., 2016, “Shear Behavior of Circular Concrete Members Reinforced with GFRP Bars and Spirals at Shear Span-To-Depth Ratios Between 1.5 and 3.0,” Journal of Composites for Construction, ASCE, V. 20, No. 6, p. 04016055. doi: 10.1061/(ASCE)CC.1943-5614.0000707

Ali, A. H.; Mohamed, H. M.; and Benmokrane, B., 2017a, “Strength and Behavior of Circular FRP-Reinforced Concrete Sections Without Web Reinforcement in Shear,” Journal of Structural Engineering, ASCE, V. 143, No. 3, p. 04016196. doi: 10.1061/(ASCE)ST.1943-541X.0001684

Ali, A. H.; Mohamed, H. M.; and Benmokrane, B., 2017b, “Shear Strength of Circular Concrete Beams Reinforced with Glass Fiber-Reinforced Polymer Bars and Spirals,” ACI Structural Journal, V. 114, No. 1, Jan.-Feb., pp. 39-49. doi: 10.14359/51689423

ASTM C330/C330M-17a, 2017, “Standard Specification for Lightweight Aggregates for Structural Concrete,” ASTM International, West Conshohocken, PA.

ASTM C39/C39M-18, 2018, “Standard Test Method for Compressive Strength of Cylindrical Concrete Specimens,” ASTM International, West Conshohocken, PA.

ASTM C567/C567M-14, 2014, “Standard Test Method for Determining Density of Structural Lightweight Concrete,” ASTM International, West Conshohocken, PA.

ASTM D7205-11, 2011, “Tensile Properties of Fiber Reinforced Polymer Matrix Composite Bars,” ASTM International, West Conshohocken, PA.

Bakouregui, A. S.; Mohamed, H. M.; Yahia, A.; and Benmokrane, B., 2021, “Axial Load–Moment Interaction Diagram of Full-Scale Circular LWSCC Columns Reinforced with BFRP and GFRP Bars and Spirals: Experimental and Theoretical Investigations,” Engineering Structures, V. 242, p. 112538. doi: 10.1016/j.engstruct.2021.112538

BS 8110-85, 1985, “Structural Use of Concrete: Code of Practice for Design and Construction,” British Standards Institution, London, UK.

CAN/CSAS806-12, 2012, “Design and Construction of Building Components with Fiber Reinforced Polymers,” Canadian Standards Association, Toronto, ON, Canada.

CAN/CSA-S6-19, 2019, “Canadian Highway Bridge Design Code,” Canadian Standards Association, Toronto, ON, Canada.

CAN/CSA A23.3-19, 2019, “Design of Concrete Structures,” Canadian Standards Association, Toronto, ON, Canada.

El-Sayed, A. K.; El-Salakawy, E. F.; and Benmokrane, B., 2006, “Shear Strength of FRP-Reinforced Concrete Beams Without Transverse Reinforcement,” ACI Structural Journal, V. 103, No. 2, Mar.-Apr., pp. 235-243.

Gerritse, A., 1981, “Design Considerations for Reinforced Lightweight Concrete,” International Journal of Cement Composites and Lightweight Concrete, V. 3, No. 1, pp. 57-69. doi: 10.1016/0262-5075(81)90031-2

Hadhood, A.; Mohamed, H. M.; and Benmokrane, B., 2018, “Flexural Stiffness of GFRP-and CFRP-RC Circular Members Under Eccentric Loads Based on Experimental and Curvature Analysis,” ACI Structural Journal, V. 115, No. 4, July, pp. 1185-1198. doi: 10.14359/51702235

Hadhood, A.; Mohamed, H. M.; Benmokrane, B.; Nanni, A.; and Shield, C. K., 2019, “Assessment of Design Guidelines of Concrete Columns Reinforced with Glass Fiber-Reinforced Polymer Bars,” ACI Structural Journal, V. 116, No. 4, July, pp. 193-207. doi: 10.14359/51715663

Hadhood, A.; Mohamed, H. M.; Ghrib, F.; and Benmokrane, B., 2017, “Efficiency of Glass-Fiber Reinforced-Polymer (GFRP) Discrete Hoops and Bars in Concrete Columns Under Combined Axial and Flexural Loads,” Composites. Part B, Engineering, V. 114, pp. 223-236. doi: 10.1016/j.compositesb.2017.01.063

Hossain, K. M. A.; Sathiyamoorthy, K.; Manzur, T.; and Lotfy, A., 2020, “Shear Behavior of Lightweight Slag Aggregate Self-Consolidating Concrete Beams,” ACI Structural Journal, V. 117, No. 5, Sept., pp. 259-268.

Hoult, N. A.; Sherwood, E. G.; Bentz, E. C.; and Collins, M. P., 2008, “Does the Use of FRP Reinforcement Change the One-Way Shear Behavior of Reinforced Concrete Slabs?” Journal of Composites for Construction, ASCE, V. 12, No. 2, pp. 125-133. doi: 10.1061/(ASCE)1090-0268(2008)12:2(125)

Hwang, C. L., and Hung, M. F., 2005, “Durability Design and Performance of Self-Consolidating Lightweight Concrete,” Construction and Building Materials, V. 19, No. 8, pp. 619-626. doi: 10.1016/j.conbuildmat.2005.01.003

Issa, M. A.; Ovitigala, T.; and Ibrahim, M., 2016, “Shear Behavior of Basalt Fiber Reinforced Concrete Beams With and Without Basalt FRP Stirrups,” Journal of Composites for Construction, ASCE, V. 20, No. 4, p. 04015083. doi: 10.1061/(ASCE)CC.1943-5614.0000638

Japan Society of Civil Engineers (JSCE), 1997, “Recommendations for Design and Construction of Concrete Structures Using Continuous Fiber Reinforced Materials.” Research Committee on Continuous Fiber Reinforced Materials, A. Machida, ed., Tokyo, Japan.

Kim, C. H., and Jang, H. S., 2014, “Concrete Shear Strength of Normal and Lightweight Concrete Beams Reinforced With FRP Bars,” Journal of Composites for Construction, ASCE, V. 18, No. 2, p. 04013038. doi: 10.1061/(ASCE)CC.1943-5614.0000440

Liu, R., and Pantelides, C. P., 2013, “Shear Strength of GFRP Reinforced Precast Lightweight Concrete Panels,” Construction and Building Materials, V. 48, pp. 51-58. doi: 10.1016/j.conbuildmat.2013.06.057

Mehany, S.; Mohamed, H. M.; and Benmokrane, B., 2019, “Strength and Behavior of HSC Concrete Beams Reinforced With Sand-Coated Basalt FRP Bars,” Proceedings of the Canadian Society for Civil Engineering (CSCE), Annual Conference, QC, Canada.

Mehany, S.; Mohamed, H. M.; and Benmokrane, B., 2021, “Contribution of Lightweight Self-Consolidated Concrete (LWSCC) to Shear Strength of Beams Reinforced With Basalt FRP Bars,” Engineering Structures, V. 231, p. 111758. doi: 10.1016/j.engstruct.2020.111758

Mohamed, H. M., and Benmokrane, B., 2014, “Design and Performance of Reinforced Concrete Water Chlorination Tank Totally Reinforced With GFRP Bars: Case Study,” Journal of Composites for Construction, ASCE, V. 18, No. 1, p. 05013001. doi: 10.1061/(ASCE)CC.1943-5614.0000429

Mousa, S.; Mohamed, H. M.; and Benmokrane, B., 2018, “Flexural Strength and Design Analysis of Circular Reinforced Concrete Members With Glass Fiber-Reinforced Polymer Bars and Spirals,” ACI Structural Journal, V. 115, No. 5, Sept., pp. 1353-1357. doi: 10.14359/51702282

Mousa, S.; Mohamed, H. M.; and Benmokrane, B., 2019, “Strength and Deformability Aspects of Circular Concrete Members Reinforced With Hybrid Carbon-FRP and Glass-FRP Under Flexure,” Journal of Composites for Construction, ASCE, V. 23, No. 2, p. 04019005. doi: 10.1061/(ASCE)CC.1943-5614.0000931

Naaman, A. E.; and Jeong, M., 1995, “Structural Ductility of Concrete Beams Prestressed with FRP Tendons,” Non-Metallic (FRP) Reinforcement for Concrete Structures: Proceedings of the Second International RILEM Symposium, CRC Press, Boca Raton, FL.

Okamura, H., and Ouchi, M., 2003, “Self-Compacting Concrete,” Journal of Advanced Concrete Technology, V. 1, No. 1, pp. 5-15. doi: 10.3151/jact.1.5

Pantelides, C. P.; Besser, B. T.; and Liu, R., 2012a, “One-Way Shear Behavior of Lightweight Concrete Panels Reinforced with GFRP Bars,” Journal of Composites for Construction, ASCE, V. 16, No. 1, pp. 2-9. doi: 10.1061/(ASCE)CC.1943-5614.0000240

Pantelides, C. P.; Liu, R.; and Reaveley, L. D., 2012b, “Lightweight Concrete Precast Bridge Deck Panels Reinforced with Glass Fiber-Reinforced Polymer Bars,” ACI Structural Journal, V. 109, No. 6, Nov.-Dec., pp. 879-888

Razaqpur, A. G., and Isgor, O. B., 2006, “Proposed Shear Design Method for FRP-Reinforced Concrete Members Without Stirrups,” ACI Structural Journal, V. 103, No. 1, pp. 93-102

Sanni, B. A.; Mohamed, H. M.; Yahia, A.; and Benmokrane, B., 2021, “Behavior of Lightweight Self-Consolidating Concrete Columns Reinforced with Glass Fiber-Reinforced Polymer Bars and Spirals under Axial and Eccentric Loads,” ACI Structural Journal, V. 118, No. 3, May, pp. 241-254.

Soltanzadeh, F.; Edalat-Behbahani, A.; Barros, J. A.; and Mazaheripour, H., 2016, “Effect of Fiber Dosage and Prestress Level on Shear Behavior of Hybrid GFRP-Steel Reinforced Concrete I-Shape Beams Without Stirrups,” Composites. Part B, Engineering, V. 102, pp. 57-77. doi: 10.1016/j.compositesb.2016.07.003

Tureyen, A. K., and Frosch, R. J., 2002, “Shear Tests of FRP-Reinforced Concrete Beams Without Stirrups,” ACI Structural Journal, V. 99, No. 4, July-Aug., pp. 427-434.

Vecchio, F. J., and Collins, M. P., 1986, “The Modified Compression Field Theory for Reinforced Concrete Elements Subjected to Shear,” ACI Journal Proceedings, V. 82, No. 2, Mar.-Apr., pp. 219-231.

Yost, J. R.; Gross, S. P.; and Dinehart, D. W., 2001, “Shear Strength of Normal Strength Concrete Beams Reinforced with Deformed GFRP Bars,” Journal of Composites for Construction, ASCE, V. 5, No. 4, pp. 268-275. doi: 10.1061/(ASCE)1090-0268(2001)5:4(268)


ALSO AVAILABLE IN: