International Concrete Abstracts Portal

  


Title: Concrete Q&A: Standing Water and Concrete Placement

Author(s): Bruce A. Suprenant

Publication: Concrete International

Volume: 44

Issue: 6

Appears on pages(s): 76

Keywords: footing, tremie, form, exit

DOI:

Date: 6/1/2022

Abstract:

A 5 ft (1.5 m) thick foundation mat slab has been prepared for concrete placement. Reinforcing steel was installed over a 3 in. (76 mm) thick mud (or working) slab with an area of approximately 25,000 ft2 (2320 m2) finished flat (that is, no slopes or contours). There are puddles of standing rainwater deposited yesterday on top of the mud slab in random locations that range in depth up to 1/2 in. (13 mm). Are there any ACI requirements for placing concrete in such conditions?




  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

Edit Module Settings to define Page Content Reviewer