Title: Shear Capacity of GFRP-Reinforced UHPC Beams without Stirrups

Author(s): Yail J. Kim and Haftom Gebrehiwot

Publication: Structural Journal

Volume: 120

Issue: 2

Appears on pages(s): 47-59

Keywords: fiber-reinforced polymer (FRP); nonmetallic reinforcement; shear; ultra-high-performance concrete (UHPC)

DOI: 10.14359/51734823

Date: 3/1/2023

Abstract:
This paper presents the behavior of glass fiber-reinforced polymer (GFRP)-reinforced ultra-high-performance concrete (UHPC) beams without shear stirrups. An experimental program is conducted to examine the implications of variable geometric, loading, and reinforcement configurations, particularly for the effective depth-to-height ratio (0.75 ≤ d/h ≤ 0.90), shear spandepth ratio (1.18 ≤ a/d ≤ 3.23), and GFRP reinforcement ratio (1.35% ≤ ρf ≤ 4.85%) of the beams. Also tested are UHPC cylinders and prisms under axial compression and three-point bending. The strength development of UHPC is remarkable during the first 3 days of casting, after which a gradual and asymptotic growth rate is associated because of saturated pores and the limited attractions of calcium-silicate-hydrate networks. Compared with the factors related to the placement of the GFRP reinforcing bars (d/h and ρf), the a/d is more influential in controlling the capacity and the postpeakdeformation of the beams by altering load-transfer mechanisms. The stress of a shear-compression zone is redistributed under arch action and results in supplementary cracks along the beam span. The horizontal splitting of UHPC at the reinforcing bar level caused by the dowel action of GFRP is dependent upon the reinforcement ratio. Analytical models are formulated, and design guidelines are recommended.


ALSO AVAILABLE IN:

Electronic Structural Journal



  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

Edit Module Settings to define Page Content Reviewer