Thermal, Microstructural, and Mechanical Properties of Ternary Blended Geopolymers

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Thermal, Microstructural, and Mechanical Properties of Ternary Blended Geopolymers

Author(s): S. Sundar Kumar and S. Maheswaran

Publication: Materials Journal

Volume: 119

Issue: 4

Appears on pages(s): 103-115

Keywords: calcined lime sludge; characterization studies; fly ash; geopolymer; lime sludge; slag

DOI: 10.14359/51734728

Date: 7/1/2022

Abstract:
Geopolymer (GP) binders are an environmentally friendly alternative to ordinary portland cement (OPC). They can be produced from materials which otherwise would be considered waste and would result in environmental degradation. The objective of this study is to use industrial residues—namely, fly ash (FA), slag cement, and calcined lime sludge (CLS)—as raw materials for geopolymer binder synthesis and to investigate the thermal, microstructural, and mechanical properties of ternary blended geopolymers. This study also focused on replacing calcium-rich slag cement with CLS, a pulp and paper industry residue, the disposal of which is still a concern for the industry. Alkali activator solutions (AAS) responsible for the chemical reactions were used at two levels of concentration. Thermal analysis was carried out by using an isothermal conduction calorimeter and thermogravimetric-differential thermogravimetric analysis (TG-DTG). Microstructural characterization of raw materials and GP products were investigated by using X-ray diffraction (XRD), X-ray fluorescence (XRF), and scanning electron microscopy (SEM) with energy-dispersive X-ray analysis (EDAX). The results showed that the reaction characteristics of products formed and strength developed of GP mortars were as in conventional cement mortars, and also proved that CLS is a viable replacement for slag cement in geopolymer. Hence, in this novel work, slag cement and fly-ash-based geopolymers were produced by using CLS as a ternary blend partially replacing slag cement. With slag cement no longer being available free of cost, use of CLS in place of slag cement would not only reduce the cost of geopolymer but also result in a smaller carbon footprint of the product.

Related References:

1. Central Electricity Authority of India (CEA), “Report on Fly Ash Generation at Coal/Lignite Based Thermal Power Stations and Its Utilization in the Country for the Year 2014-15,” New Delhi, India, Oct. 2015.

2. Maheswaran, S.; Murthy, A. R.; and Priya, G. S., “Pozzolanic Effect of Fly Ash with Calcined Lime Sludge,” ACI Materials Journal, V. 115, No. 6, Nov. 2018, pp. 925-934. doi: 10.14359/51706847

3. IS 3812-1, “Pulverized Fuel Ash – Specification, Part – 1 For Use as Pozzolan in Cement, Mortar and Concrete,” Bureau of Indian Standards, New Delhi, India, 2003.

4. IS 12089, “Specification for Granulated Slag for the Manufacture of Portland Slag Cement,” Bureau of Indian Standards, New Delhi, India, 1987.

5. Singh, M., and Garg, M., “Utilization of Waste Lime Sludge as Building Materials,” Journal of Scientific and Industrial Research, V. 67, 2008, pp. 161-166.

6. Chandra, S.; Kumar, S.; and Kumar Anand R., “Soil Stabilization with Rice Husk Ash and Lime Sludge,” Indian Highways, V. 33, No. 5, 2005.

7. Maher, A.; Butziger, J. M.; and Oweis, I. S., “Lime Sludge Amended Fly Ash for Utilization as an Engineering Material,” ASCE Annual Convention and Exposition, Dallas, TX, 1993, pp. 73-88.

8. Sabat, A. K., “Utilization of Bagasse Ash and Lime Sludge for Construction of Flexible Pavements in Expansive Soil Areas,” The Electronic Journal of Geotechnical Engineering, V. 17, 2012, pp. 1037-1046.

9. Santa, R. A.; Bernardin, A. M.; Riella, H. G.; and Kuhnen, N. C., “Geopolymer Synthetized from Bottom Coal Ash and Calcined Paper Sludge,” Journal of Cleaner Production, V. 57, 2013, pp. 302-307. doi: 10.1016/j.jclepro.2013.05.017

10. Maheswaran, S.; Kalaiselvam, S.; Arunbalaji, S.; Palani, G. S.; and Iyer, N. R., “Low-Temperature Preparation of Belite from Lime Sludge and Nanosilica through Solid-State Reaction,” Journal of Thermal Analysis and Calorimetry, V. 119, No. 3, 2015, pp. 1845-1852. doi: 10.1007/s10973-014-4371-5

11. Maheswaran, S.; Kalaiselvam, S.; Karthikeyan, S. S.; Kokila, C.; and Palani, G. S., “β-Belite Cements (β-Dicalcium Silicate) Obtained from Calcined Lime Sludge and Silica Fume,” Cement and Concrete Composites, V. 66, 2016, pp. 57-65. doi: 10.1016/j.cemconcomp.2015.11.008

12. Shi, C.; Jiménez, A. F.; and Palomo, A., “New Cements for the 21st Century: The Pursuit of an Alternative to Portland Cement,” Cement and Concrete Research, V. 41, No. 7, 2011, pp. 750-763. doi: 10.1016/j.cemconres.2011.03.016

13. Provis, J. L., and Van Deventer, J. S., “Alkali Activated Materials: State-of-the-Art Report (RILEM TC 224-AAM),” Springer Science & Business Media, Dordrecht, the Netherlands, 2013.

14. Shi, C.; Krivenko, P. V.; and Roy, D., Alkali-Activated Cements and Concretes, Taylor & Francis, New York, 2006.

15. Huntzinger, D. N., and Eatmon, T. D., “A Life-Cycle Assessment of Portland Cement Manufacturing: Comparing the Traditional Process with Alternative Technologies,” Journal of Cleaner Production, V. 17, No. 7, 2009, pp. 668-675. doi: 10.1016/j.jclepro.2008.04.007

16. McLellan, B. C.; Williams, R. P.; Lay, J.; Van Riessen, A.; and Corder, G. D., “Costs and Carbon Emissions for Geopolymer Pastes in Comparison to Ordinary Portland Cement,” Journal of Cleaner Production, V. 19, No. 9-10, 2011, pp. 1080-1090. doi: 10.1016/j.jclepro.2011.02.010

17. Duxson, P.; Provis, J. L.; Lukey, G. C.; and Van Deventer, J. S., “The Role of Inorganic Polymer Technology in the Development of ‘Green Concrete’,” Cement and Concrete Research, V. 37, No. 12, 2007, pp. 1590-1597. doi: 10.1016/j.cemconres.2007.08.018

18. Jamieson, E.; McLellan, B.; Van Riessen, A.; and Nikraz, H., “Comparison of Embodied Energies of Ordinary Portland Cement with Bayer-Derived Geopolymer Products,” Journal of Cleaner Production, V. 99, 2015, pp. 112-118. doi: 10.1016/j.jclepro.2015.03.008

19. Hardjito, D., and Rangan, B. V., “Development and Properties of Low-Calcium Fly Ash-Based Geopolymer Concrete,” Research Report GC 1, Faculty of Engineering, Curtin University of Technology Perth, Perth, Australia, 2005.

20. Somna, K.; Jaturapitakkul, C.; Kajitvichyanukul, P.; and Chindaprasirt, P., “NaOH-Activated Ground Fly Ash Geopolymer Cured at Ambient Temperature,” Fuel, V. 90, No. 6, 2011, pp. 2118-2124. doi: 10.1016/j.fuel.2011.01.018

21. Yip, C. K.B, “The Role of Calcium in Geopolymerisation,” doctoral dissertation, University of Melbourne, Melbourne, Australia, 2004.

22. Puligilla, S., and Mondal, P., “Role of Slag in Microstructural Development and Hardening of Fly Ash-Slag Geopolymer,” Cement and Concrete Research, V. 43, 2013, pp. 70-80. doi: 10.1016/j.cemconres.2012.10.004

23. Li, Z., and Liu, S., “Influence of Slag as Additive on Compressive Strength of Fly Ash-Based Geopolymer,” Journal of Materials in Civil Engineering, ASCE, V. 19, No. 6, 2007, pp. 470-474. doi: 10.1061/(ASCE)0899-1561(2007)19:6(470)

24. Kumar, S.; Kumar, R.; and Mehrotra, S. P., “Influence of Granulated Blast Furnace Slag on the Reaction, Structure and Properties of Fly Ash Based Geopolymer,” Journal of Materials Science, V. 45, No. 3, 2010, pp. 607-615. doi: 10.1007/s10853-009-3934-5

25. Nath, P., and Sarker, P. K., “Use of OPC to Improve Setting and Early Strength Properties of Low Calcium Fly Ash Geopolymer Concrete Cured at Room Temperature,” Cement and Concrete Composites, V. 55, 2015, pp. 205-214. doi: 10.1016/j.cemconcomp.2014.08.008

26. Raheem, Z., and Kareem, A. A., “Wear and Friction of Polymer Fiber Composites Coated by Nicr Alloy,” Engineering Transactions, V. 65, 2017, pp. 307-318.

27. Kareem, A. A., “Enhanced Thermal and Electrical Properties of Epoxy/Carbon Fiber–Silicon Carbide Composites,” Advanced Composites Letters, V. 29, 2020, pp. 1-6. doi: 10.1177/2633366X19894598

28. Kareem, A. A., and Rasheed, H. K., “Electrical and Thermal Characteristics of MWCNTs Modified Carbon Fiber/Epoxy Composite Films,” Materials Science Poland, V. 37, No. 4, 2019, pp. 622-627. doi: 10.2478/msp-2019-0081

29. IS 383, “Specification for Course and Fine Aggregates from Natural Sources for Concrete,” Bureau of Indian Standards, New Delhi, India, 1970.

30. Kumar, S., and Kumar, R., “Mechanical Activation of Fly Ash: Effect on Reaction, Structure and Properties of Resulting Geopolymer,” Ceramics International, V. 37, No. 2, 2011, pp. 533-541. doi: 10.1016/j.ceramint.2010.09.038

31. Yao, X.; Zhang, Z.; Zhu, H.; and Chen, Y., “Geopolymerization Process of Alkali–Metakaolinite Characterized by Isothermal Calorimetry,” Thermochimica Acta, V. 493, No. 1-2, 2009, pp. 49-54. doi: 10.1016/j.tca.2009.04.002

32. Zhang, Z.; Wang, H.; Provis, J. L.; Bullen, F.; Reid, A.; and Zhu, Y., “Quantitative Kinetic and Structural Analysis of Geopolymers. Part 1. The Activation of Metakaolin with Sodium Hydroxide,” Thermochimica Acta, V. 539, 2012, pp. 23-33. doi: 10.1016/j.tca.2012.03.021

33. Kong, D. L., and Sanjayan, J. G., “Effect of Elevated Temperatures on Geopolymer Paste, Mortar and Concrete,” Cement and Concrete Research, V. 40, No. 2, 2010, pp. 334-339. doi: 10.1016/j.cemconres.2009.10.017

34. Billong, N.; Oti, J.; and Kinuthia, J., “Using Silica Fume-Based Activator in Sustainable Geopolymer Binder for Building Application,” Construction and Building Materials, V. 275, 2021, pp. 122-177. doi: 10.1016/j.conbuildmat.2020.122177

35. Cheng, Y.; Hongqiang, M.; Hongyu, C.; Jiaxin, W.; Jing, S.; Zonghui, L.; and Mingkai, Y., “Preparation and Characterization of Coal Gangue Geopolymers,” Construction and Building Materials, V. 187, 2018, pp. 318-326. doi: 10.1016/j.conbuildmat.2018.07.220

36. Hussin, M. W.; Bhutta, M. A.; Azreen, M.; Ramadhansyah, P. J.; and Mirza, J., “Performance of Blended Ash Geopolymer Concrete at Elevated Temperatures,” Materials and Structures, V. 48, No. 3, 2015, pp. 709-720. doi: 10.1617/s11527-014-0251-5

37. Whitfield, P. S., and Mitchell, L. D., “Quantitative Rietveld Analysis of the Amorphous Content in Cements and Clinkers,” Journal of Materials Science, V. 38, No. 21, 2003, pp. 4415-4421. doi: 10.1023/A:1026363906432

38. Nath, S. K.; Maitra, S.; Mukherjee, S.; and Kumar, S., “Microstructural and Morphological Evolution of Fly Ash Based Geopolymers,” Construction and Building Materials, V. 111, 2016, pp. 758-765. doi: 10.1016/j.conbuildmat.2016.02.106

39. Antiohos, S.; Papageorgiou, A.; and Tsimas, S., “Activation of Fly Ash Cementitious Systems in the Presence of Quicklime. Part II: Nature of Hydration Products, Porosity and Microstructure Development,” Cement and Concrete Research, V. 36, No. 12, 2006, pp. 2123-2131. doi: 10.1016/j.cemconres.2006.09.013

40. Yip, C. K.; Lukey, G. C.; and Van Deventer, J. S., “The Coexistence of Geopolymeric Gel and Calcium Silicate Hydrate at the Early Stage of Alkaline Activation,” Cement and Concrete Research, V. 35, No. 9, 2005, pp. 1688-1697. doi: 10.1016/j.cemconres.2004.10.042

41. Miranda, J. M.; Fernández-Jiménez, A.; González, J. A.; and Palomo, A., “Corrosion Resistance in Activated Fly Ash Mortars,” Cement and Concrete Research, V. 35, No. 6, 2005, pp. 1210-1217. doi: 10.1016/j.cemconres.2004.07.030

42. Xu, H., and Van Deventer, J. S., “Microstructural Characterization of Geopolymers Synthesized from Kaolinite/Stilbite Mixtures Using XRD, MAS-NMR, SEM/EDX, TEM/EDX, and HREM,” Cement and Concrete Research, V. 32, No. 11, 2002, pp. 1705-1716. doi: 10.1016/S0008-8846(02)00859-1

43. Aziz, I. H.; Abdullah, M. M. A. B.; Salleh, M. M.; Azimi, E. A.; Chaiprapa, J.; and Sandu, A. V., “Strength Development of Solely Ground Granulated Blast Furnace Slag Geopolymers,” Construction and Building Materials, V. 250, 2020, pp. 118-720. doi: 10.1016/j.conbuildmat.2020.118720

44. Temuujin, J., and Van Riessen, A., “Effect of Fly Ash Preliminary Calcination on the Properties of Geopolymer,” Journal of Hazardous Materials, V. 164, No. 2-3, 2009, pp. 634-639. doi: 10.1016/j.jhazmat.2008.08.065

45. Gunasekara, C.; Law, D. W.; Setunge, S.; Burgar, I.; and Brkljaca, R., “Effect of Element Distribution on Strength in Fly Ash Geopolymers,” ACI Materials Journal, V. 114, No. 5, Sept.-Oct. 2017, pp. 795-808. doi: 10.14359/51689779

46. Kani, E. N.; Allahverdi, A.; and Provis, J. L., “Calorimetric Study of Geopolymer Binders Based on Natural Pozzolan,” Journal of Thermal Analysis and Calorimetry, V. 127, No. 3, 2017, pp. 2181-2190. doi: 10.1007/s10973-016-5850-7

47. Gadkar, A., and Subramaniam, K. V., “Self-Leveling Geopolymer Concrete Using Alkali-Activated Fly Ash,” ACI Materials Journal, V. 118, No. 2, Mar. 2021, pp. 21-30.

48. Bhagath Singh, G. V. P. and Subramaniam, K. V., “Evaluation of Total Reactive Oxide Ratios and Working Solution Ratios on Strength Development in Fly Ash Based Geopolymers,” Journal of Materials in Civil Engineering, ASCE, V. 32, No. 4, 2020, pp. 04020051-1-8.

49. Ryu, G. S.; Lee, Y. B.; Koh, K. T.; and Chung, Y. S., “The Mechanical Properties of Fly Ash-Based Geopolymer Concrete with Alkaline Activators,” Construction and Building Materials, V. 47, 2013, pp. 409-418. doi: 10.1016/j.conbuildmat.2013.05.069

50. Xu, H., and Van Deventer, J. S., “The Geopolymerization of Alumino-silicate Minerals,” International Journal of Mineral Processing, V. 59, No. 3, 2000, pp. 247-266. doi: 10.1016/S0301-7516(99)00074-5

51. Yip, C. K., and Van Deventer, J. S., “Microanalysis of Calcium Silicate Hydrate Gel Formed Within a Geopolymeric Binder,” Journal of Materials Science, V. 38, No. 18, 2003, pp. 3851-3860. doi: 10.1023/A:1025904905176

52. Van Deventer, J. S.; Provis, J. L.; Duxson, P.; and Lukey, G. C., “Reaction Mechanisms in the Geopolymeric Conversion of Inorganic Waste to Useful Products,” Journal of Hazardous Materials, V. 139, No. 3, 2007, pp. 506-513. doi: 10.1016/j.jhazmat.2006.02.044

53. Lee, W. K., and Van Deventer, J. S., “The Effect of Ionic Contaminants on the Early-Age Properties of Alkali-Activated Fly Ash-Based Cements,” Cement and Concrete Research, V. 32, No. 4, 2002, pp. 577-584. doi: 10.1016/S0008-8846(01)00724-4

54. Temuujin, J. V.; Van Riessen, A.; and Williams, R., “Influence of Calcium Compounds on the Mechanical Properties of Fly Ash Geopolymer Pastes,” Journal of Hazardous Materials, V. 167, No. 1-3, 2009, pp. 82-88. doi: 10.1016/j.jhazmat.2008.12.121


ALSO AVAILABLE IN:

Electronic Materials Journal