Durability Performance of Blended Cement with Calcined Illitic Shale

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Durability Performance of Blended Cement with Calcined Illitic Shale

Author(s): G. P. Cordoba, A. Rossetti, S. V. Zito, V. F. Rahhal, D. Falcone, and E. F. Irassar

Publication: Materials Journal

Volume: 119

Issue: 1

Appears on pages(s): 134-144

Keywords: alkali-silica reaction; calcined clays; calcined shale; chloride penetration; durability; illite; sulfate attack

DOI: 10.14359/51734192

Date: 1/1/2022

Abstract:
The use of calcined clays in cement (kaolinitic and common calcined clays) introduces challenges due to the high alumina content, large specific surface area, and high-alkali content. This paper examines the performance against sulfate attacks, alkali-silica reactions, and chloride penetration in mixtures with calcined illitic shale (CIS). Replacement of high and moderate alkali content cement with 25% CIS significantly reduces the expansion in the alkali-silica reaction (ASR) test, as the pozzolanic reaction contributes to the combination of alkalis. Replacing 20% white portland cement with CIS allows the formulation of sulfate-resistant cement by limiting the formation of gypsum and ettringite. The incorporation of 25% CIS in concrete does not significantly increase chloride ingress. Therefore, blended cements with replacement levels of 20 to 25% of portland cement by CIS reduce or maintain the performance against ASR, sulfate attack, and chloride penetration.

Related References:

1. Fernandez, R.; Martirena, F.; and Scrivener, K. L., “The Origin of the Pozzolanic Activity of Calcined Clay Minerals: A Comparison between Kaolinite, Illite and Montmorillonite,” Cement and Concrete Research, V. 41, No. 1, 2011, pp. 113-122. doi: 10.1016/j.cemconres.2010.09.013

2. Tironi, A.; Trezza, M. A.; Scian, A. N.; and Irassar, E. F., “Assessment of Pozzolanic Activity of Different Calcined Clays,” Cement and Concrete Composites, V. 37, No. 1, 2013, pp. 319-327. doi: 10.1016/j.cemconcomp.2013.01.002

3. Marchetti, G.; Rahhal, V. F.; Pavlík, Z.; Pavlíková, M.; and Irassar, E. F., “Assessment of Packing, Flowability, Hydration Kinetics, and Strength of Blended Cements with Illitic Calcined Shale,” Construction and Building Materials, V. 254, Sept. 2020, p. 119042. doi: 10.1016/j.conbuildmat.2020.119042

4. Diaz-Loya, I.; Juenger, M.; Seraj, S.; and Minkara, R., “Extending Supplementary Cementitious Material Resources: Reclaimed and Remediated Fly Ash and Natural Pozzolans,” Cement and Concrete Composites, V. 101, Aug. 2019, pp. 44-51. doi: 10.1016/j.cemconcomp.2017.06.011

5. Juenger, M., and Siddique, R., “Recent Advances in Understanding the Role of Supplementary Cementitious Materials in Concrete,” Cement and Concrete Research, V. 78, Dec. 2015, pp. 71-80. doi: 10.1016/j.cemconres.2015.03.018

6. Plank, J.; Sakai, E.; Miao, C. W.; Yu, C.; and Hong, J. X., “Chemical Admixtures—Chemistry, Applications and Their Impact on Concrete Microstructure and Durability,” Cement and Concrete Research, V. 78, Dec. 2015, pp. 81-99. doi: 10.1016/j.cemconres.2015.05.016

7. Ferreiro, S.; Herfort, D.; and Damtoft, J. S., “Effect of Raw Clay Type, Fineness, Water-to-Cement Ratio and Fly Ash Addition on Workability and Strength Performance of Calcined Clay—Limestone Portland Cements,” Cement and Concrete Research, V. 101, Nov. 2017, pp. 1-12. doi: 10.1016/j.cemconres.2017.08.003

8. Dhandapani, Y., and Santhanam, M., “Assessment of Pore Structure Evolution in the Limestone Calcined Clay Cementitious System and Its Implications for Performance,” Cement and Concrete Composites, V. 84, Nov. 2017, pp. 36-47. doi: 10.1016/j.cemconcomp.2017.08.012

9. Malhotra, S., and Dave, N., “Investigations into the Effect of Addition of Flyash and Burnt Clay Pozzolana on Certain Engineering Properties of Cement Composites,” Cement and Concrete Composites, V. 21, No. 4, 1999, pp. 285-291. doi: 10.1016/S0958-9465(99)00006-2

10. Irassar, E. F.; Tironi, A.; Bonavetti, V. L.; Trezza, M. A.; Castellano, C. C.; Rahhal, V. F.; Donza, H. A.; and Scian, A. N., “Thermal Treatment and Pozzolanic Activity of Calcined Clay and Shale,” ACI Materials Journal, V. 116, No. 4, July 2019, pp. 133-143. doi: 10.14359/51716717

11. Seraj, S.; Cano, R.; Ferron, R. P.; and Juenger, M. C. G., “Calcined Shale as Low Cost Supplementary Cementitious Material,” Calcined Clays for Sustainable Concrete, RILEM Bookseries, V. 10, K. Scrivener and A. Favier, eds., Springer, Dordrecht, 2015, pp. 531-537.

12. Habert, G.; Choupay, N.; Escadeillas, G.; Guillaume, D.; and Montel, J. M., “Clay Content of Argillites: Influence on Cement Based Mortars,” Applied Clay Science, V. 43, No. 3-4, 2009, pp. 322-330. doi: 10.1016/j.clay.2008.09.009

13. Trümer, A.; Ludwig, H. M.; Schellhorn, M.; and Diedel, R., “Effect of a Calcined Westerwald Bentonite as Supplementary Cementitious Material on the Long-Term Performance of Concrete,” Applied Clay Science, V. 168, Feb. 2019, pp. 36-42. doi: 10.1016/j.clay.2018.10.015

14. Li, C.; Ideker, J. H.; and Drimalas, T., “The Efficacy of Calcined Clays on Mitigating Alakli-Silica Reaction (ASR) in Mortar and Its Influence on Microstructure,” Proceedings, First International Conference on Calcined Clays for Sustainable Concrete, V. 10, Lausanne, Switzerland, 2015, pp. 211-217.

15. Trümer, A., and Ludwig, H. M., “Sulphate and ASR Resistance of Concrete Made with Calcined Clay Blended Cements,” Calcined Clays for Sustainable Concrete, RILEM Bookseries, V. 10, K. Scrivener and A. Favier, eds., Springer, Dordrecht, 2015, pp. 3-9.

16. Scrivener, K. L.; Juilland, P.; and Monteiro, P. J. M., “Advances in Understanding Hydration of Portland Cement,” Cement and Concrete Research, V. 78, Dec. 2015, pp. 38-56. doi: 10.1016/j.cemconres.2015.05.025

17. Irassar, E. F., “Sulfate Attack on Cementitious Materials Containing Limestone Filler—A Review,” Cement and Concrete Research, V. 39, No. 3, 2009, pp. 241-254. doi: 10.1016/j.cemconres.2008.11.007

18. Bonavetti, V. L.; Rahhal, V. F.; and Irassar, E. F., “Studies on the Carboaluminate Formation in Limestone Filler-Blended Cements,” Cement and Concrete Research, V. 31, No. 6, 2001, pp. 853-859. doi: 10.1016/S0008-8846(01)00491-4

19. Mather, B., “How to Make Concrete That Will Not Suffer Deleterious Alkali-Silica Reaction,” Cement and Concrete Research, V. 29, No. 8, 1999, pp. 1277-1280. doi: 10.1016/S0008-8846(98)00240-3

20. Schulze, S. E., and Rickert, J., “Suitability of Natural Calcined Clays as Supplementary Cementitious Material,” Cement and Concrete Composites, V. 95, Jan. 2019, pp. 92-97. doi: 10.1016/j.cemconcomp.2018.07.006

21. Irassar, E. F.; Di Maio, A. A.; and Batic, O. R., “Sulfate Attack on Concrete with Mineral Admixtures,” Cement and Concrete Research, V. 26, No. 1, 1996, pp. 113-123. doi: 10.1016/0008-8846(95)00195-6

22. Gettu, R.; Patel, A.; Rathi, V.; Prakasan, S.; Basavaraj, A. S.; and Maity, S., “Sustainability Assessment of Cements and Concretes in the Indian Context: Influence of Supplementary Cementitious Materials,” Fourth International Conference on Sustainable Construction Materials and Technologies, P. Claisse, E. Ganjian, and T. Naik, eds., Coventry University, Las Vegas, NV, 2016. pp. 1142-1150.

23. González, M., and Irassar, E. F., “Effect of Limestone Filler on the Sulfate Resistance of Low C3A Portland Cement,” Cement and Concrete Research, V. 28, No. 11, 1998, pp. 1655-1667. doi: 10.1016/S0008-8846(98)00144-6

24. Wild, S.; Khatib, J. M.; and O’Farrell, M., “Sulphate Resistance of Mortar, Containing Ground Brick Clay Calcined at Different Temperatures,” Cement and Concrete Research, V. 27, No. 5, 1997, pp. 697-709. doi: 10.1016/S0008-8846(97)00059-8

25. Taylor-Lange, S. C.; Lamon, E. L.; Riding, K. A.; and Juenger, M. C. G., “Calcined Kaolinite—Bentonite Clay Blends as Supplementary Cementitious Materials,” Applied Clay Science, V. 108, May 2015, pp. 84-93. doi: 10.1016/j.clay.2015.01.025

26. Al-Zahrani, M. M.; Al-Sodani, K. A.; Maslehuddin, M.; Al-Amoudi, O. S. B.; and Al-Dulaijan, S. U., “Chloride Diffusion Models for Type V and Silica Fume Cement Concretes,” ACI Materials Journal, V. 117, No. 3, May 2020, pp. 11-20.

27. Al-Sodani, K. A. A.; Maslehuddin, M.; Al-Amoudi, O. S. B.; Saleh, T. A.; and Shameem, M., “Performance of Corrosion Inhibitors in Cracked and Uncracked Silica Fume Cement Concrete Beams,” European Journal of Environmental and Civil Engineering, V. 24, No. 10, 2020, pp. 1573-1588. doi: 10.1080/19648189.2018.1475306

28. Marsavina, L.; Audenaert, K.; De Schutter, G.; Faur, N.; and Marsavina, D., “Experimental and Numerical Determination of the Chloride Penetration in Cracked Concrete,” Construction and Building Materials, V. 23, No. 1, 2009, pp. 264-274. doi: 10.1016/j.conbuildmat.2007.12.015

29. Loser, R.; Lothenbach, B.; Leemann, A.; and Tuchschmid, M., “Chloride Resistance of Concrete and Its Binding Capacity—Comparison between Experimental Results and Thermodynamic Modeling,” Cement and Concrete Composites, V. 32, No. 1, 2010, pp. 34-42. doi: 10.1016/j.cemconcomp.2009.08.001

30. Shehata, M.; Adhikari, G.; and Radomski, S., “Long-Term Durability of Blended Cement against Sulfate Attack,” ACI Materials Journal, V. 105, No. 6, Nov.-Dec. 2008, pp. 594-602.

31. Dhole, R.; Thomas, M.; Folliard, K. J.; and Drimalas, T., “Chemical and Physical Sulfate Attack on Fly Ash Concrete Mixtures,” ACI Materials Journal, V. 116, No. 4, July 2019, pp. 31-42. doi: 10.14359/51716678

32. ASTM C618-15, “Standard Specification for Coal Fly Ash and Raw or Calcined Natural Pozzolan for Use in Concrete,” ASTM International, West Conshohocken, PA, 2015.

33. Snellings, R., “X-Ray Powder Diffraction Applied to Cement,” A Practical Guide to Microstructural Analysis of Cementitious Materials,

V. 2, K. L. Scrivener, R. Snellings, and B. Lothenbach, eds., Taylor & Francis Group, Boca Raton, FL, 2018, pp. 104-176.

34. ASTM C188-17, “Standard Test Method for Density of Hydraulic Cement,” ASTM International, West Conshohocken, PA, 2017.

35. ASTM D422-63(2007), “Standard Test Method for Particle-Size Analysis of Soils,” ASTM International, West Conshohocken, PA, 2007.

36. ASTM C204-18, “Standard Test Methods for Fineness of Hydraulic Cement by Air-Permeability Apparatus,” ASTM International, West Conshohocken, PA, 2018.

37. EN 196-5:2011, “Methods of Testing Cement—Part 5: Pozzolanicity Test for Pozzolanic Cement,” European Committee for Standardization, Brussels, Belgium, 2011.

38. ASTM C187-16, “Standard Test Method for Amount of Water Required for Normal Consistency of Hydraulic Cement Paste,” ASTM International, West Conshohocken, PA, 2016.

39. ASTM C191-19, “Standard Test Methods for Time of Setting of Hydraulic Cement by Vicat Needle,” ASTM International, West Conshohocken, PA, 2019.

40. ASTM C230/C230M-21, “Standard Specification for Flow Table for Use in Tests of Hydraulic Cement,” ASTM International, West Conshohocken, PA, 2021.

41. EN 196-1:2016, “Methods of Testing Cement—Part 1: Determination of Strength,” European Committee for Standardization, Brussels, Belgium, 2016.

42. ASTM C143/C143M-20, “Standard Test Method for Slump of Hydraulic-Cement Concrete,” ASTM International, West Conshohocken, PA, 2020.

43. ASTM C39/C39M-21, “Standard Test Method for Compressive Strength of Cylindrical Concrete Specimens,” ASTM International, West Conshohocken, PA, 2021.

44. ASTM C642-13, “Standard Test Method for Density, Absorption, and Voids in Hardened Concrete,” ASTM International, West Conshohocken, PA, 2013.

45. ASTM C441/C441M-17, “Standard Test Method for Effectiveness of Pozzolans or Ground Blast-Furnace Slag in Preventing Excessive Expansion of Concrete due to the Alkali-Silica Reaction,” ASTM International, West Conshohocken, PA, 2017.

46. ASTM C311/C311M-18, “Standard Test Methods for Sampling and Testing Fly Ash or Natural Pozzolans for Use in Portland-Cement Concrete,” ASTM International, West Conshohocken, PA, 2018.

47. ASTM C227-10, “Standard Test Method for Potential Alkali Reactivity of Cement-Aggregate Combinations (Mortar-Bar Method) (Withdrawn 2018) ,” ASTM International, West Conshohocken, PA, 2010.

48. Thomas, M.; Fournier, B.; Folliard, K.; Ideker, J.; and Shehata, M., “Test Methods for Evaluating Preventive Measures for Controlling Expansion due to Alkali–Silica Reaction in Concrete,” Cement and Concrete Research, V. 36, No. 10, 2006, pp. 1842-1856. doi: 10.1016/j.cemconres.2006.01.014

49. ASTM C1567-13, “Standard Test Method for Determining the Potential Alkali-Silica Reactivity of Combinations of Cementitious Materials and Aggregate (Accelerated Mortar-Bar Method),” ASTM International, West Conshohocken, PA, 2013.

50. ASTM C1260-21, “Standard Test Method for Potential Alkali Reactivity of Aggregates (Mortar-Bar Method),” ASTM International, West Conshohocken, PA, 2021.

51. Rossetti, A.; Cohelo dos Santos, G.; Falcone, D.; and Irassar, E. F., “Studies on Illitic Calcined Clays as Possible Inhibitors of the Alkali-Silica Reaction (ASR),” Proceedings, Sixteenth International Conference on Alkali-Aggregate Reaction in Concrete (16th ICAAR LISBOA 2020-2022). Lisbon, Portugal, 2021.

52. ACI Committee 201, “Guide to Durable Concrete (ACI 201.2R-16),” American Concrete Institute, Farmington Hills, MI, 2016.

53. ASTM C1012/C1012M-18, “Standard Test Method for Length Change of Hydraulic-Cement Mortars Exposed to a Sulfate Solution,” ASTM International, West Conshohocken, PA, 2018.

54. ASTM C157/C157M-17, “Standard Test Method for Length Change of Hardened Hydraulic-Cement Mortar and Concrete,” ASTM International, West Conshohocken, PA, 2017.

55. ASTM C109/C109M-20, “Standard Test Method for Compressive Strength of Hydraulic Cement Mortars (Using 2-in. or [50 mm] Cube Specimens),” ASTM International, West Conshohocken, PA, 2020.

56. ASTM C1556-11a(2016), “Standard Test Method for Determining the Apparent Chloride Diffusion Coefficient of Cementitious Mixtures by Bulk Diffusion,” ASTM International, West Conshohocken, PA, 2016.

57. Andrade Perdrix, C., “Testing and Modelling Chloride Penetration in Concrete: Analysis of Total Chloride Content in Concrete (RILEM TC 178-TMC),” Materials and Structures, V. 35, Nov, 2002, pp. 583-585.

58. EN 14629:2007, “Test Methods—Determination of Chloride Content in Hardened Concrete,” European Committee for Standardization, Brussels, Belgium, 2007.

59. He, C.; Osbæck, B.; and Makovicky, E., “Pozzolanic Reactions of Six Principal Clay Minerals: Activation, Reactivity Assessments and Technological Effects,” Cement and Concrete Research, V. 25, No. 8, 1995, pp. 1691-1702. doi: 10.1016/0008-8846(95)00165-4

60. Tironi, A.; Castellano, C.; Bonavetti, V. L.; Trezza, M. A.; Scian, A. N.; and Irassar, E. F., “Kaolinitic Calcined Clays—Portland Cement System: Hydration and Properties,” Construction and Building Materials, V. 64, Aug. 2014, pp. 215-221. doi: 10.1016/j.conbuildmat.2014.04.065

61. Msinjili, N. S.; Vogler, N.; Sturm, P.; Neubert, M.; Schroeder, H. J.; Kuehne, H.-C.; Huenger, K.-J.; and Gluth, G. J. G., “Calcined Brick Clays and Mixed Clays as Supplementary Cementitious Materials: Effects on the Performance of Blended Cement Mortars,” Construction and Building Materials, V. 266, No. 9, 2021, p. 120990. doi: 10.1016/j.conbuildmat.2020.120990

62. He, C.; Makovicky, E.; and Osbæck, B., “Thermal Stability and Pozzolanic Activity of Raw and Calcined Mixed-Layer Mica/Smectite,” Applied Clay Science, V. 17, No. 3-4, 2000, pp. 141-161. doi: 10.1016/S0169-1317(00)00011-9

63. Trümer, A., and Ludwig, H. M., “Assessment of Calcined Clays According to the Main Criterions of Concrete Durability,” Calcined Clays for Sustainable Concrete, RILEM Bookseries, V. 16, F. Martirena, A. Favier, and K. Scrivener, Springer, Dordrecht, 2018, pp. 475-481.

64. Paiva, H.; Velosa, A.; Cachim, P.; and Ferreira, V. M., “Effect of Metakaolin Dispersion on the Fresh and Hardened State Properties of Concrete,” Cement and Concrete Research, V. 42, No. 4, 2012, pp. 607-612. doi: 10.1016/j.cemconres.2012.01.005

65. Dhandapani, Y.; Sakthivel, T.; Santhanam, M.; Gettu, R.; and Pillai, R. G., “Mechanical Properties and Durability Performance of Concretes with Limestone Calcined Clay Cement (LC3),” Cement and Concrete Research, V. 107, May 2018, pp. 136-151. doi: 10.1016/j.cemconres.2018.02.005

66. Taha, B., and Nounu, G., “Using Lithium Nitrate and Pozzolanic Glass Powder in Concrete as ASR Suppressors,” Cement and Concrete Composites, V. 30, No. 6, 2008, pp. 497-505. doi: 10.1016/j.cemconcomp.2007.08.010

67. Bokern, J., “Concrete Tests for ASR Assessment: Effects of Testing Environment on Preconditions for an ASR and Transferability of Test Results,” Thirteenth International Conference on Alkali–Aggregate Reaction in Concrete, M. A. Broekmans and B. J. Wigum, eds. ICAAR, Trondheim, Norway, 2008. pp. 511-520.

68. ASTM C1293-20, “Standard Test Method for Determination of Length Change of Concrete due to Alkali-Silica Reaction,” ASTM International, West Conshohocken, PA, 2020.

69. Patzias, T., “The Development of ASTM Method C 1012 with Recommended Acceptance Limits for Sulfate Resistance of Hydraulic Cements,” Cement, Concrete and Aggregates, V. 13, No. 1, 1991, pp. 50-57. doi: 10.1520/CCA10549J

70. Monteiro, P. J. M., and Kurtis, K. E., “Time to Failure for Concrete Exposed to Severe Sulfate Attack,” Cement and Concrete Research, V. 33, No. 7, 2003, pp. 987-993. doi: 10.1016/S0008-8846(02)01097-9

71. Mehta, P. K., “Sulfate Attack on Concrete: A Critical Review,” Materials Science of Concrete, V. III, American Ceramic Society, Westerville, OH, 1992, pp. 105-130.

72. Sabir, B. B.; Wild, S.; and Bai, J., “Metakaolin and Calcined Clays as Pozzolans for Concrete: A Review,” Cement and Concrete Composites, V. 23, No. 6, 2001, pp. 441-454. doi: 10.1016/S0958-9465(00)00092-5


ALSO AVAILABLE IN: