Proposition of Mixture Design Method for Ultra-High- Performance Concrete

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Proposition of Mixture Design Method for Ultra-High- Performance Concrete

Author(s): Roberto Christ, Bernardo Fonseca Tutikian, and Paulo Roberto do Lago Helene

Publication: Materials Journal

Volume: 119

Issue: 1

Appears on pages(s): 79-89

Keywords: fiber-reinforced concrete; mixture design; particle-size distribution; ultra-high-performance concrete

DOI: 10.14359/51734191

Date: 1/1/2022

Abstract:
The mechanical potential, the durability, and the most varied uses of structures have been studied and disclosed. However, there is still a gap regarding the determination of mixing ratios using a simple, accessible mixture design method that allows the determination of the ideal ratio of mixture constituents. Some studies on ultra-high-performance concrete (UHPC) mixtures did not present a method to define the mixing ratio with different materials and fiber contents, with high mechanical strength and no workability loss. To develop a method of mixing design from informational parameters of the materials, this paper presents a method of dosing UHPC. The proposed method is based on the packaging of particles through the previous evaluation of the percentages of each material according to its particle size distribution. Results showed that the proposed mixture design method can grant high potential compressive strength to the mixture. There was also a linear relation between higher matrix compacity and compressive strength. The composition with higher compacity—that is, the lowest void ratio of the mixture—presented an increase of 20% in compressive strength compared to the mixture with less compacity.

Related References:

1. Schmidt, M., and Fehling, E., “Ultra-High-Performance Concrete: Research, Development and Application in Europe,” Seventh International Symposium on the Utilization of High-Strength/High-Performance Concrete, SP-228, H. G. Russell, ed., American Concrete Institute, Farmington Hills, MI, 2015, pp. 51-78.

2. Tutikian, B. F.; Pacheco, F.; and Christ, R., “Analysis of the Mechanical Properties of Advanced Cementitious Composites of Reactive Powder Concretes with Hybridization of Metal and Polypropylene Microfibers,” Ciencia and Engenharia/Science and Engineering Journal, V. 25, No. 1, 2016, pp. 49-56.

3. Christ, R., “Proposição de um método de dosagem para concretos de ultra alto desempenho (UHPC),” Universidade do Vale do Rio dos Sinos, São Leopoldo, Brazil, 2019.

4. Perry, V., “Case Studies on Innovative Applications and Challenges of Introducing Break-through Technologies (UHPC) in the Construction Industry,” ACF Symposium on UHPC, Kolkata, India, 2015.

5. ASTM C1856/C1856M-17, “Standard Practice for Fabricating and Testing Specimens of Ultra-High Performance Concrete,” ASTM International, West Conshohocken, PA, 2017, 4 pp.

6. NF P 18-710, “Design of Concrete Structures: Specific Rules for Ultra-High Performance Fibre-Reinforced Concrete (UHPFRC),” Association Française de Normalisation, La Plaine Saint-Denis, France, 2016.

7. NF P 18-470, “Concrete Ultra-High-Performance Fibre-Reinforced Concrete (UPHFRC)—Specification, Performance, Production and Conformity,” Association Française de Normalisation, La Plaine Saint-Denis, France, 2017.

8. Toutlemonde, F., and Resplendino, J., Designing and Building with UHPFRC, Wiley, Hoboken, NJ, 2013.

9. Fehling, E.; Schmidt, M.; Walraven, J.; Leutbecher, T.; and Frohlich, S., Ultra-High-Performance Concrete UHPC: Fundamentals, Design, Examples, Wiley, Berlin, Germany, 2013.

10. Freytag, B.; Heinzle, G.; Reichel, M. M.; and Sparowitz, L., “Wild-Bridge Scientific Preparation for Smooth Realisation,” Symposium, Third International Symposium on UHPC and Nanotechnology for High Performance Construction Materials, Kassel, Germany, 2012.

11. Acker, P., and Behloul, M., “Ductal® Technology: A Large Spectrum of Properties, a Wide Range of Applications,” Symposium, Proceedings of the International Symposium on Ultra High Performance Concrete, Kassel, Germany, 2004.

12. Torregrosa, E. C., “Dosage Optimization and Bolted Connections for UHPFRC Ties,” PhD dissertation, Universitat Politècnica de València Dosage, Valencia, Spain, 2013.

13. Yu, R.; Spiesz, P.; and Brouwers, H. J. H., “Mix Design and Properties Assessment of Ultra-High Performance Fibre Reinforced Concrete (UHPFRC),” Cement and Concrete Research, V. 56, Feb. 2014, pp. 29-39. doi: 10.1016/j.cemconres.2013.11.002

14. Libya, L. A.; Peyvandi, A.; Abideen, S.; Weerasiri, R. R.; Balachandra, A. M.; and Soroushian, P., “Production Methods for Reliable Construction of Ultra-High-Performance Concrete (UHPC) Structures,” Materiaux et Constructions,” Materials and Structures, V. 50, No. 1, 2017, pp. 1-19.

15. Wang, X.; Yu, R.; Song, Q.; Shui, Z.; Liu, Z.; Wu, S.; and Hou, D., “Optimized Design of Ultra-High Performance Concrete (UHPC) with a High Wet Packing Density,” Cement and Concrete Research, V. 126, Dec. 2019, p. 105921. doi: 10.1016/j.cemconres.2019.105921

16. Ragalwar, K.; Heard, W. F.; Williams, B. A.; and Ranade, R., “Significance of the Particle Size Distribution Modulus for Strain-Hardening-Ultra-High Performance Concrete (SH-UHPC) Matrix Design,” Construction and Building Materials, V. 234, Feb. 2020, p. 117423. doi: 10.1016/j.conbuildmat.2019.117423

17. Christ, R.; Pacheco, F.; Ehrenbring, H.; Quinino, U.; Mancio, M.; and Tutikian, B. F., “Study of Mechanical Behavior of Ultra—High Performance Concrete (UHPC) Reinforced with Hybrid Fibers and with Reduced Cement Consumption,” Revista de Ingeniería de Construcción, V. 34, No. 2, 2019, pp. 159-168. doi: 10.4067/S0718-50732019000200159

18. Yunsheng, Z.; Wei, S.; Sifeng, L.; Chujie, J.; and Jianzhong, L., “Preparation of C200 Green Reactive Powder Concrete and Its Static–Dynamic Behaviors,” Cement and Concrete Composites, V. 30, No. 9, 2008, pp. 831-838. doi: 10.1016/j.cemconcomp.2008.06.008

19. Christ, R., and Tutikian, B., “Study of Pressure and Curing Temperature in Reactive Powder Concretes (RPC) with Different Amounts of Metallic Microfibers,” Revista de la Construcción, V. 12, No. 2, 2013, pp. 1-9. doi: 10.4067/S0718-915X2013000200003

20. Sun, Y.; Yu, R.; Shui, Z.; Wang, X.; Qian, D.; Rao, B.; Huang, J.; and He, Y., “Understanding the Porous Aggregates Carrier Effect on Reducing Autogenous Shrinkage of Ultra-High Performance Concrete (UHPC) Based on Response Surface Method,” Construction and Building Materials, V. 222, Oct. 2019, pp. 130-141. doi: 10.1016/j.conbuildmat.2019.06.151

21. Fennis, S. A. A. M., and Walraven, J. C., “Using Particle Packing Technology for Sustainable Concrete Mixture Design,” Heron, V. 57, No. 2, 2012, pp. 73-101.

22. Spiesz, P. R., and Hunger, M., “Towards a More Common Use of Ultra-High Performance Concrete (UHPC)—Development of UHPC for Ready-Mix and Prefabrication Concrete Plants,” Proceedings of Eleventh High Performance Concrete Conference, HPC Tromso, H. Justnes and H. Braarud, eds., University of Technology, Eindhoven, Netherlands, 2017, pp. 1-10, https://pure.tue.nl/ws/files/58624276/46_UHPC_Przemek_Spiesz.pdf. (last accessed Dec. 28, 2021)

23. Martinie, L.; Rossi, P.; and Roussel, N., “Rheology of Fiber Reinforced Cementitious Materials: Classification and Prediction,” Cement and Concrete Research, V. 40, No. 2, 2010, pp. 226-234. doi: 10.1016/j.cemconres.2009.08.032

24. ASTM C1611/C1611M-18, “Standard Test Method for Slump Flow of Self-Consolidating Concrete,” ASTM International, West Conshohocken, PA, 2018.

25. ASTM C1231/C1231M-15, “Standard Practice for Use of Unbonded Caps in Determination of Compressive Strength of Hardened Cylindrical Concrete Specimens,” ASTM International, West Conshohocken, PA, 2015.

26. ASTM C1609-12, “Standard Test Method for Flexural Performance of Fiber-Reinforced Concrete (Using Beam with Third-Point Loading),” ASTM International, West Conshohocken, PA, 2012.

27. Choi, M. S.; Lee, J. S.; Ryu, K. S.; Koh, K.-T.; and Kwon, S. H., “Estimation of Rheological Properties of UHPC Using Mini Slump Test,” Construction and Building Materials, V. 106, Mar. 2016, pp. 632-639. doi: 10.1016/j.conbuildmat.2015.12.106

28. Pyo, S., and Kim, H. K., “Fresh and Hardened Properties of Ultra-High Performance Concrete Incorporating Coal Bottom Ash and Slag Powder,” Construction and Building Materials, V. 131, Jan. 2017, pp. 459-466. doi: 10.1016/j.conbuildmat.2016.10.109

29. Fehling, E.; Schmidt, M.; and Stürwald, S., Ultra-High-Performance Concrete (UHPC), Kassel University Press, Kassel, Germany, 2015.

30. Soliman, N. A., and Tagnit-Hamou, A., “Development of Ultra-High-Performance Concrete Using Glass Powder—Towards Ecofriendly Concrete,” Construction and Building Materials, V. 125, Oct. 2016, pp. 600-612. doi: 10.1016/j.conbuildmat.2016.08.073

31. Toutlemonde, F., and Resplendino, J., Designing and Building with UHPFRC, Wiley, Hoboken, NJ, 2011.

32. Alsalman, A.; Dang, C. N.; and Hale, W. M., “Development of Ultra-High Performance Concrete with Locally Available Materials,” Construction and Building Materials, V. 133, Feb. 2017, pp. 135-145. doi: 10.1016/j.conbuildmat.2016.12.040

33. Kang, S.-T.; Choi, J.-I. I.; Koh, K.-T.; Lee, K. S.; and Lee, B. Y., “Hybrid Effects of Steel Fiber and Microfiber on the Tensile Behavior of Ultra-High Performance Concrete,” Composite Structures, V. 145, June 2016, pp. 37-42. doi: 10.1016/j.compstruct.2016.02.075

34. Soroushian, P., and Bayasi, Z., “Fiber Type Effects on the Performance of Steel Fiber Reinforced Concrete,” ACI Materials Journal, V. 88, No. 2, Mar.-Apr. 1991, pp. 129-134.

35. Banfill, P. F. G.; Starrs, G.; Derruau, G.; McCarter, W. J.; and Chrisp, T. M., “Rheology of Low Carbon Fibre Content Reinforced Cement Mortar,” Cement and Concrete Composites, V. 28, No. 9, 2006, pp. 773-780. doi: 10.1016/j.cemconcomp.2006.06.004

36. Figueiredo, A. D., “Concreto reforçado com fibras,” Universidade de São Paulo, São Paulo, Brazil, 2011.

37. Hüsken, G., and Brouwers, H. J. H., “A New Mix Design Concept for Earth-Moist Concrete: A Theoretical and Experimental Study,” Cement and Concrete Research, V. 38, No. 10, 2008, pp. 1246-1259. doi: 10.1016/j.cemconres.2008.04.002

38. Khan, M. I.; Abbas, Y. M.; and Fares, G., “Review of High and Ultrahigh Performance Cementitious Composites Incorporating Various Combinations of Fibers and Ultrafines,” Journal of King Saud University Engineering and Science, V. 29, No. 4, 2017, pp. 339-347. doi: 10.1016/j.jksues.2017.03.006

39. Park, S. H.; Kim, D. J.; Ryu, G. S.; and Koh, K. T., “Tensile Behavior of Ultra High Performance Hybrid Fiber Reinforced Concrete,” Cement and Concrete Composites, V. 34, No. 2, 2012, pp. 172-184. doi: 10.1016/j.cemconcomp.2011.09.009

40. Yoo, D. Y.; Banthia, N.; Kang, S.-T.; and Yoon, Y.-S., “Effect of Fiber Orientation on the Rate-Dependent Flexural Behavior of Ultra-High-Performance Fiber-Reinforced Concrete,” Composite Structures, V. 157, Dec. 2016, pp. 62-70. doi: 10.1016/j.compstruct.2016.08.023

41. Yoo, D. Y.; Kim, S.; Park, G.-J.; Park, J.-J.; and Kim, S.-W., “Effects of Fiber Shape, Aspect Ratio, and Volume Fraction on Flexural Behavior of Ultra-High-Performance Fiber-Reinforced Cement Composites,” Composite Structures, V. 174, Aug. 2017, pp. 375-388. doi: 10.1016/j.compstruct.2017.04.069

42. Abbas, S.; Soliman, A. M.; and Nehdi, M. L., “Exploring Mechanical and Durability Properties of Ultra-High Performance Concrete Incorporating Various Steel Fiber Lengths and Dosages,” Construction and Building Materials, V. 75, Jan. 2015, pp. 429-441. doi: 10.1016/j.conbuildmat.2014.11.017

43. Yu, R.; Spiesz, P.; and Brouwers, H. J. H., “Development of an Eco-Friendly Ultra-High-Performance Concrete (UHPC) with Efficient Cement and Mineral Admixtures Uses,” Cement and Concrete Composites, V. 55, Jan. 2015, pp. 383-394. doi: 10.1016/j.cemconcomp.2014.09.024

44. Mehta, P. K., and Monteriro, P. J., Concreto: Microestrutura, Propriedades e Materiais, second edition, Ibracon, São Paulo, Brazil, 2014.

45. Neville, A. M., and Brooks, J. J., Concrete Technology, Pearson, 2010.

46. Ferrara, L.; Park, Y. D.; and Shah, S. P., “A Method for Mix-Design of Fiber-Reinforced Self-Compacting Concrete,” Cement and Concrete Research, V. 37, No. 6, 2007, pp. 957-971. doi: 10.1016/j.cemconres.2007.03.014

47. Park, J. J.; Kang, S.-T.; and Koh, K. T., “Influence of the Ingredients on the Compressive Strength of UHPC as a Fundamental Study to Optimize the Mixing Proportion,” Proceedings, Second International Symposium on Ultra High Performance Concrete, Albany, NY, 2008.


ALSO AVAILABLE IN:

Electronic Materials Journal



  

Edit Module Settings to define Page Content Reviewer