Title: Case Study: Measuring Flow and Setting Time for Three-Dimensionally Printed Mortar

Author(s): Emily Xu, Karin Vanessa Tejada, David Walker, Sasa Zivkovic, and Kenneth C. Hover

Publication: Materials Journal

Volume: 118

Issue: 6

Appears on pages(s): 395-405

Keywords: additive manufacturing; mortar; mortar flow; setting; threedimensional (3D) printing

DOI: 10.14359/51734152

Date: 11/1/2021

Abstract:
The authors explored the influence of ingredients on fluid consistency and setting behavior of mortars for three-dimensional (3D) printing using standard test methods typically employed to monitor post-depositional flow and setting time of pastes and mortar from one to several hours after batching. With minor modifications in method and reanalysis of results, readily available standard tests can characterize some behaviors of plastic mortar as early as half an hour or sooner following printing. The work also showed the behavioral sensitivity of the 3D-printed mortar to changes in ingredients, including conversion of a prebagged commercial mortar mixture to a sand, cement, and lime mixture and isolating the impact of hydrated lime, high-range water reducer, calcium chloride set accelerator, and polypropylene fibers. Fluidity and setting behavior were monitored with the ASTM C1437 mortar flow, ASTM C403 time of setting, modified C403, and ASTM C807 Modified Vicat Needle tests.


ALSO AVAILABLE IN:

Electronic Materials Journal



  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

Edit Module Settings to define Page Content Reviewer