Design Approach for Flexural Strength of Reinforced Ultra- High-Performance Concrete Members Considering Size Effect

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Design Approach for Flexural Strength of Reinforced Ultra- High-Performance Concrete Members Considering Size Effect

Author(s): Fei Peng, Weijian Yi, and Zhi Fang

Publication: Structural Journal

Volume: 119

Issue: 1

Appears on pages(s): 281-294

Keywords: design equations; flexural strength; moment-curvature; size effect; ultra-high-performance concrete (UHPC)

DOI: 10.14359/51734140

Date: 1/1/2022

Abstract:
A new simplified method considering size effect was proposed to calculate the flexural strength of reinforced ultra-high performance concrete (UHPC) members in this paper. First, an iterative numerical procedure was developed to predict the moment-curvature behavior of reinforced UHPC sections. Based on the developed procedure and available experimental results, the performance of three constitutive models for UHPC under tension was evaluated. It was found that the size-dependent stress-strain model could provide accurate and consistent predictions of the flexural strength of reinforced UHPC members, while the size-independent model overestimated the flexural strength of largescale members. A parametric study was then conducted to evaluate the contribution of fibers and the size effect. An equivalent rectangular stress block was proposed to simplify the tensile stress distribution of UHPC. On this basis, a simplified yet rational design approach for predicting flexural strength was proposed based on a regression analysis of parametric analysis results. Finally, the accuracy of the proposed approach was verified based on the available experimental results of 117 reinforced UHPC members.

Related References:

Aaleti, S.; Petersen, B.; and Sritharan, S., 2013, “Design Guide for Precast UHPC Waffle Deck Panel System, Including Connections,” FHWA-HIF-13-032, U.S. Department of Transportation, Federal Highway Administration, Washington, DC, 127 pp.

ACI Committee 239, 2018, “Ultra-High-Performance Concrete: An Emerging Technology Report (ACI 239R-18),” American Concrete Institute, Farmington Hills, MI, 21 pp.

AFGC, 2013, “Bétons Fibrés Á Ultra-Hautes Performances: Recommendations,” Association Française de Génie Civil, Paris, France, 357 pp.

Baby, F.; Marchand, P.; and Toutlemonde, F., 2017, “Analytical Modeling of Ultra-High-Performance Fiber-Reinforced Concrete Behavior in Ribbed Plates,” ACI Structural Journal, V. 114, No. 1, Jan.-Feb., pp. 3-13. doi: 10.14359/51689246

Chen, S.; Zhang, R.; Jia, L.-J.; and Wang, J.-Y., 2018, “Flexural Behaviour of Rebar-Reinforced Ultra-High-Performance Concrete Beams,” Magazine of Concrete Research, V. 70, No. 19, pp. 997-1015. doi: 10.1680/jmacr.17.00283

Deng, Z.; Wang, Y.; Xiao, R.; Lan, M.; and Chen, X., 2015, “Flexural Test and Theoretical Analysis of UHPC Beams with High Strength Rebars,” Journal of Basic Science and Engineering, V. 23, No. 1, pp. 68-78. (in Chinese) doi: 10.16058/j.issn.1005-0930.2015.01.006

Fang, Z.; Liu, M.; and Zheng, H., 2015, “Experiment on Flexural Behaviors of Prestressed Reactive Powder Concrete Box Girders,” Journal of Architecture and Civil Engineering, V. 32, No. 6, pp. 8-16. (in Chinese) doi: 10.3969/j.issn.1673-2049.2015.06.002

Gowripalan, N., and Gilbert, I. R., 2000, “Design Guidelines for Ductal Prestressed Concrete Beams,” University of New South Wales, Sydney, Australia, 54 pp.

Graybeal, B. A., 2008, “Flexural Behavior of an Ultrahigh-Performance Concrete I-Girder,” Journal of Bridge Engineering, ASCE, V. 13, No. 6, pp. 602-610. doi: 10.1061/(ASCE)1084-0702(2008)13:6(602)

Graybeal, B. A., and Baby, F., 2019, “Tension Testing of Ultra-High Performance Concrete,” FHWA-HRT-17-053, U.S. Department of Transportation, Federal Highway Administration, Washington, DC, 186 pp.

Haldar, A., and Mahadevan, S., 2000, Probability, Reliability and Statistical Method in Engineering Design, John Wiley & Sons, Inc., New York, 304 pp.

Hasgul, U.; Turker, K.; Birol, T.; and Yavas, A., 2018, “Flexural Behavior of Ultra-High-Performance Fiber Reinforced Concrete Beams with Low and High Reinforcement Ratios,” Structural Concrete, V. 19, No. 6, pp. 1577-1590. doi: 10.1002/suco.201700089

JSCE, 2008, “Recommendations for Design and Construction of High-Performance Fibre Reinforced Cement Composites with Multiple Fine Cracks (HPFRCC),” Concrete Engineering Series 82, Japanese Society of Civil Engineers, Tokyo, Japan, 113 pp.

Kodur, V.; Solhmirzaei, R.; Agrawal, A.; Aziz, E. M.; and Soroushian, P., 2018, “Analysis of Flexural and Shear Resistance of Ultra High Performance Fiber Reinforced Concrete Beams without Stirrups,” Engineering Structures, V. 174, pp. 873-884. doi: 10.1016/j.engstruct.2018.08.010

Li, L.; Fan, X.; Shi X.; and Shao, X., 2018, “Experimental Study on Flexural Behavior of Large-Scale Prestressed UHPC T-Shaped Beam,” China Civil Engineering Journal, V. 51, No. 5, pp. 84-94. (in Chinese) doi: 10.15951/j.tmgcxb.2018.05.01010.15951/j.tmgcxb.2018.05.010

Liang, X.; Wang, P.; Xu, M.; Wang Z.; Yu, J.; and Li, L., 2019, “Investigation on Flexural Capacity of Reinforced Ultra High Performance Concrete Beams,” Engineering Mechanics, V. 36, No. 5, pp. 113-122. (in Chinese) doi: 10.6052/j.issn.1000-4750.2018.03.0164

Liu, C.; Zhang, Y.; Yao, Y.; and Huang, Y., 2019, “Calculation Method for Flexural Capacity of High Strain-Hardening Ultra-High Performance Concrete T-Beams,” Structural Concrete, V. 20, No. 1, pp. 405-419. doi: 10.1002/suco.201800151

MCS-EPFL, 2016, “Recommendation: Ultra-High Performance Fibre Reinforced Cement-Based Composites (UHPFRC),” Maintenance, Construction and Safety of Structures (MCS)- École polytechnique fédérale de Lausanne (EPFL), Lausanne, Switzerland, 37 pp.

Nguyen, D. L.; Kim, D. J.; Ryu, G. S.; and Koh, K. T., 2013, “Size Effect on Flexural Behavior of Ultra-High-Performance Hybrid Fiber-Reinforced Concrete,” Composites Part B: Engineering, V. 45, No. 1, pp. 1104-1116. doi: 10.1016/j.compositesb.2012.07.012

Peng, F.; Xue, W.; and Xue, W., 2020, “Database Evaluation of Shear Strength of Slender Fiber-Reinforced Polymer-Reinforced Concrete Members,” ACI Structural Journal, V. 117, No. 3, May, pp. 273-281. doi: 10.14359/51723504

Pourbaba, M.; Sadaghian, H.; and Mirmiran, A., 2019, “Flexural Response of UHPFRC Beams Reinforced with Steel Rebars,” Advances in Civil Engineering Materials, V. 8, No. 3, pp. 411-430. doi: 10.1520/ACEM20190129

Qi, J.; Wang, J.; and Ma, Z. J., 2018, “Flexural Response of High-Strength Steel-Ultra-High- Performance Fiber Reinforced Concrete Beams Based on a Mesoscale Constitutive Model: Experiment and Theory,” Structural Concrete, V. 19, No. 3, pp. 719-734. doi: 10.1002/suco.201700043

Qiu, M.; Shao, X.; Wille, K.; Yan, B.; and Wu, J., 2020a, “Experimental Investigation on Flexural Behavior of Reinforced Ultra High Performance Concrete Low-Profile T-Beams,” International Journal of Concrete Structures and Materials, V. 14, No. 1, pp. 1-20. doi: 10.1186/s40069-019-0380-x

Qiu, M.; Shao, X.; Zhu, Y.; Zhan, J.; Yan, B.; and Wang, Y., 2020b, “Experimental Investigation on Flexural Cracking Behavior of Ultrahigh Performance Concrete Beams,” Structural Concrete, V. 21, No. 5, pp. 2134-2153. doi: 10.1002/suco.201900339

Randl, N.; Simon, C.; and Mészöly, T., 2013, “Experimental Investigations on UHP(FR)C Beams with High Strength Reinforcement,” RILEM-fib-AFGC International Symposium on Ultra-High-Performance Fibre-Reinforced Concrete, Marseille, France, pp. 557-566.

Sim, C.; Tadros, M.; Gee, D.; and Asaad, M., 2020, “Flexural Design of Precast, Prestressed Ultra-High-Performance Concrete Members,” PCI Journal, V. 65, No. 6, pp. 35-61. doi: 10.15554/pcij65.6-02

Singh, M.; Sheikh, A. H.; Mohamed Ali, M. S.; Visintin, P.; and Griffith, M. C., 2017, “Experimental and Numerical Study of the Flexural Behaviour of Ultra-High Performance Fibre Reinforced Concrete Beams,” Construction and Building Materials, V. 138, pp. 12-25. doi: 10.1016/j.conbuildmat.2017.02.002

Steinberg, E., 2010, “Structural Reliability of Prestressed UHPC Flexure Models for Bridge Girders,” Journal of Bridge Engineering, ASCE, V. 15, No. 1, pp. 65-72. doi: 10.1061/(ASCE)BE.1943-5592.0000039

Sturm, A. B.; Visintin, P.; Seracino, R.; Lucier, G. W.; and Oehlers, D. J., 2020, “Flexural Performance of Pretensioned Ultra-High Performance Fibre Reinforced Concrete Beams with CFRP Tendons,” Composite Structures, V. 243, p. 112223. doi: 10.1016/j.compstruct.2020.112223

Su, J.; Fu, Y.; Huang, Q.; Chen, B.; and Wei, J., 2017, “Flexural Test and Finite Element Analysis of Reinforced UHPC Beams,” Journal of China & Foreign Highway, V. 37, No. 6, pp. 99-105. (in Chinese) doi: 10.14048/j.issn.1671-2579.2017.06.022

Su, J.; Ma, X.; Chen, B.; and Sennah, K., 2020, “Full-Scale Bending Test and Parametric Study on a 30-m Span Prestressed Ultra-High Performance Concrete Box Girder,” Advances in Structural Engineering, V. 23, No. 7, pp. 1276-1289. doi: 10.1177/1369433219894244

Turker, K.; Hasgul, U.; Birol, T.; Yavas, A.; and Yazici, H., 2019, “Hybrid Fiber Use on Flexural Behavior of Ultra High Performance Fiber Reinforced Concrete Beams,” Composite Structures, V. 229, p. 111400. doi: 10.1016/j.compstruct.2019.111400

Wahba, K., 2012, “Mechanical and Structural Properties of Ultra High Performance Fiber Reinforced Concrete,” master’s dissertation, Ryerson University, Toronto, ON, Canada, 79 pp.

Wang, Y.; Shao, X.; Cao J.; Deng, S.; and Li, Y., 2020, “Research on Flexural Performance of UHPPC Deck Panel Containing Small Coarse Aggregates,” China Civil Engineering Journal, V. 53, No. 3, pp. 67-79. (in Chinese) doi: 10.15951/j.tmgcxb.2020.03.009

Wille, K., and Parra-Montesinos, G. J., 2012, “Effect of Beam Size, Casting Method, and Support Conditions on Flexural Behavior of Ultra-High-Performance Fiber-Reinforced Concrete,” ACI Materials Journal, V. 109, No. 3, May-June, pp. 379-388.

Xia, J.; Chan, T.; Mackie, K. R.; Saleem, M. A.; and Mirmiran, A., 2018, “Sectional Analysis for Design of Ultra-High Performance Fiber Reinforced Concrete Beams with Passive Reinforcement,��� Engineering Structures, V. 160, pp. 121-132. doi: 10.1016/j.engstruct.2018.01.035

Xu, H., and Deng, Z., 2014, “Experimental Research on Flexural Behavior of Prestressed Ultra-High Performance Steel Fiber Concrete Beams,” Journal of Building Structures, V. 35, No. 12, pp. 58-64. (in Chinese). doi: 10.14006/j.jzjgxb.2014.12.008

Xue, W.; Peng, F.; and Xue, W., 2020, “Calibration of Strength Reduction Factor for Reinforced Ultra-High-Performance Concrete Bridge Girders in Flexure,” Journal of Bridge Engineering, ASCE, V. 25, No. 10, p. 04020086. doi: 10.1061/(ASCE)BE.1943-5592.0001621

Yang, J., and Fang, Z., 2009, “Research on Flexural Behaviors of Prestressed Ultra High Performance Concrete Beams,” China Journal of Highway and Transport, V. 22, No. 1, pp. 39-46. (in Chinese) doi: 10.19721/j.cnki.1001-7372.2009.01.007

Yang, I. H.; Joh, C.; and Kim, B.-S., 2010, “Structural Behavior of Ultra High Performance Concrete Beams Subjected to Bending,” Engineering Structures, V. 32, No. 11, pp. 3478-3487. doi: 10.1016/j.engstruct.2010.07.017

Yang, I.-H.; Joh, C.; and Kim, B.-S., 2011, “Flexural Strength of Large-Scale Ultra High Performance Concrete Prestressed T-Beams,” Canadian Journal of Civil Engineering, V. 38, No. 11, pp. 1185-1195. doi: 10.1139/l11-078

Yang, I.-H.; Park, J.; Bui, T. Q.; Kim, K.-C.; Joh, C.; and Lee, H., 2020, “An Experimental Study on the Ductility and Flexural Toughness of Ultrahigh-Performance Concrete Beams Subjected to Bending,” Materials (Basel), V. 13, No. 10, p. 2225. doi: 10.3390/ma13102225

Yoo, D.-Y.; Banthia, N.; Kang, S.-T.; and Yoon, Y.-S., 2016, “Size Effect in Ultra-High-Performance Concrete Beams,” Engineering Fracture Mechanics, V. 157, pp. 86-106. doi: 10.1016/j.engfracmech.2016.02.009

Yoo, D.-Y.; Banthia, N.; and Yoon, Y.-S., 2017, “Experimental and Numerical Study on Flexural Behavior of Ultra-High-Performance Fiber-Reinforced Concrete Beams with Low Reinforcement Ratios,” Canadian Journal of Civil Engineering, V. 44, No. 1, pp. 18-28. doi: 10.1139/cjce-2015-0384

Yoo, D.-Y., and Yoon, Y.-S., 2015, “Structural Performance of Ultra-High-Performance Concrete Beams with Different Steel Fibers,” Engineering Structures, V. 102, pp. 409-423. doi: 10.1016/j.engstruct.2015.08.


ALSO AVAILABLE IN:

Electronic Structural Journal



  

Edit Module Settings to define Page Content Reviewer