Abstract:
The article presents a recently completed preliminary study of the effects of finishing and surface treatments on durability of decorative concrete. It discusses results of water-absorption testing per RILEM Test Method 11.4 and modified ASTM C1585, as well as abrasion resistance testing per ASTM C944/C944M and with a Chaplin Abrasion Tester, conducted on specimens representing hard-troweled, stamped, and exposed aggregate finishes with various surface treatments.

Related References:

1. Farny, J., and Rowland, L., “Concrete Q&A: Setting a Standard for Decorative Concrete,” Durability + Design, Aug. 2014, pp. 42-50.

2. ACI Committee 308, “Guide to External Curing of Concrete (ACI 308R-16),” American Concrete Institute, Farmington Hills, MI, 2016, 36 pp.

3. Dhir, R.; Hewlett, P.; and Chan, Y., “Near-Surface Characteristics of Concrete: Abrasion Resistance,” Materials and Structures, V. 24, No. 140, Mar. 1991, pp. 122-128.

4. ASTM C944/C944M-99(2005), “Standard Test Method for Abrasion Resistance of Concrete or Mortar Surfaces by the Rotating-Cutter Method,” ASTM International, West Conshohocken, PA, 1999, 4 pp.

5. Amini, K.; Sadati, S.; Ceylan, H.; and Taylor, P.C., “Effects of Mixture Proportioning, Curing, and Finishing on Concrete Surface Hardness,” ACI Materials Journal, V. 116, No. 2, Mar. 2019, pp. 119-126.

6. Shen, P.; Chen, W.; Lu, L.; Geng, H.; and Li, Q., “Effect of Aggregate Exposing and Curing Agent on the Performance of Exposed Aggregate Concrete,” Construction and Building Materials, V. 156, Sept. 2017, pp. 675-683.

7. RILEM Test Method 11.4, “Measurement of Water Absorption Under Low Pressure,” RILEM, Paris, France, Sept. 1987, 3 pp.

8. ASTM C1585-11, “Standard Test Method for Measurement of Rate of Absorption of Water by Hydraulic-Cement Concretes,” ASTM International, West Conshohocken, PA, 2011, 6 pp.