Neural Network for Mixture Design Optimization of Geopolymer Concrete

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Neural Network for Mixture Design Optimization of Geopolymer Concrete

Author(s): Ankur Bhogayata, Sneh Kakadiya, and Rinkesh Makwana

Publication: Materials Journal

Volume: 118

Issue: 4

Appears on pages(s): 91-96

Keywords: artificial neural network (ANN); compressive strength; geopolymer concrete; optimization; splitting tensile strength

DOI: 10.14359/51732711

Date: 7/1/2021

Abstract:
The paper discusses the development and application of the artificial neural network (ANN) model for predicting the compressive and splitting tensile strength of the geopolymer-based concrete composites (GPC). The strength properties of GPC are influenced by the proportions of the constituents—namely, the alkaline solution, fly ash, aggregates, and sand and water—and require optimization for the desired quality of the composite. The optimum mixture may be obtained by using modern techniques; namely ANN modeling. The ANN models have been developed by training and validating the input data using the sigmoid function and the feed-forward backpropagation algorithm in the hidden layers. The ANN layer is the functional part of the model consisting of the operators to carry out the specific task largely based on mathematical calculations. A five-layered ANN model has been developed and used to predict the strength to optimize the mixture design. The predicted values have been compared with the experimental strength values, and the effects of the most significant constituents have been studied.

Related References:

1. Zhang, G.; Patuwo, B. E.; and Hu, M. Y., “Forecasting with Artificial Neural Networks: The State of The Art,” International Journal of Forecasting, V. 14, No. 1, 1998, pp. 35-62. doi: 10.1016/S0169-2070(97)00044-7

2. Khademi, F.; Akbari, M.; Jamal, S. M.; and Nikoo, M., “Multiple Linear Regression, Artificial Neural Network, and Fuzzy Logic Prediction of 28 Days Compressive Strength of Concrete,” Frontiers of Structural and Civil Engineering, V. 11, No. 1, 2017, pp. 90-99. doi: 10.1007/s11709-016-0363-9

3. Lai, S., and Serra, M., “Concrete Strength Prediction by Means of Neural Network,” Construction and Building Materials, V. 11, No. 2, 1997, pp. 93-98. doi: 10.1016/S0950-0618(97)00007-X

4. Saad, S.; Ishtiyaque, M.; and Malik, H., “Selection of Most Relevant Input Parameters Using WEKA for Artificial Neural Network Based Concrete Compressive Strength Prediction Model,” 7th Power India International Conference (PIICON) 2016, pp. 1-6.

5. Yeh, I. C., “Modeling of Strength of High-Performance Concrete Using Artificial Neural Networks,” Cement and Concrete Research, V. 28, No. 12, 1998, pp. 1797-1808. doi: 10.1016/S0008-8846(98)00165-3

6. Kewalramani, M. A., and Gupta, R., “Concrete Compressive Strength Prediction Using Ultrasonic Pulse Velocity Through Artificial Neural Networks,” Automation in Construction, V. 15, No. 3, 2006, pp. 374-379. doi: 10.1016/j.autcon.2005.07.003

7. Barbuta, M.; Diaconescu, R. M.; and Harja, M., “Using Neural Networks for Prediction of Properties of Polymer Concrete With Fly Ash,” Journal of Materials in Civil Engineering, ASCE, V. 24, No. 5, 2011, pp. 523-528. doi: 10.1061/(ASCE)MT.1943-5533.0000413

8. Öztaş, A.; Pala, M.; Özbay, E.; Kanca, E.; Caglar, N.; and Bhatti, M. A., “Predicting the Compressive Strength and Slump of High Strength Concrete Using Neural Network,” Construction and Building Materials, V. 20, No. 9, 2006, pp. 769-775. doi: 10.1016/j.conbuildmat.2005.01.054

9. Altun, F.; Kişi, Ö.; and Aydin, K., “Predicting the Compressive Strength of Steel Fiber Added Lightweight Concrete Using Neural Network,” Computational Materials Science, V. 42, No. 2, 2008, pp. 259-265. doi: 10.1016/j.commatsci.2007.07.011

10. Nehdi, M.; Djebbar, Y.; and Khan, A., “Neural Network Model for Preformed-Foam Cellular Concrete,” ACI Materials Journal, V. 98, No. 5, Sept. 2001, pp. 402-409.

11. Bui, D. K.; Nguyen, T.; Chou, J. S.; Nguyen-Xuan, H.; and Ngo, T. D., “A Modified Firefly Algorithm-Artificial Neural Network Expert System for Predicting Compressive and Tensile Strength of High-Performance Concrete,” Construction and Building Materials, V. 180, 2018, pp. 320-333. doi: 10.1016/j.conbuildmat.2018.05.201

12. Topçu, İ. B., and Sarıdemir, M., “Prediction of Rubberized Concrete Properties Using Artificial Neural Network and Fuzzy Logic,” Construction and Building Materials, V. 22, No. 4, 2008, pp. 532-540. doi: 10.1016/j.conbuildmat.2006.11.007

13. Khademi, F.; Jamal, S. M.; Deshpande, N.; and Londhe, S., “Predicting Strength of Recycled Aggregate Concrete Using Artificial Neural Network, Adaptive Neuro-Fuzzy Inference System and Multiple Linear Regression,” International Journal of Sustainable Built Environment, V. 5, No. 2, 2016, pp. 355-369. doi: 10.1016/j.ijsbe.2016.09.003

14. Mashhadban, H.; Kutanaei, S. S.; and Sayarinejad, M. A., “Prediction and Modeling of Mechanical Properties in Fiber Reinforced Self-Compacting Concrete Using Particle Swarm Optimization Algorithm and Artificial Neural Network,” Construction and Building Materials, V. 119, 2016, pp. 277-287. doi: 10.1016/j.conbuildmat.2016.05.034

15. Topcu, I. B., and Sarıdemir, M., “Prediction of Properties of Waste AAC Aggregate Concrete Using Artificial Neural Network,” Computational Materials Science, V. 41, No. 1, 2007, pp. 117-125. doi: 10.1016/j.commatsci.2007.03.010

16. Bondar, D., “Use of a Neural Network to Predict Strength and Optimum Compositions of Natural Alumina-Silica-Based Geopolymers,” Journal of Materials in Civil Engineering, ASCE, V. 26, No. 3, 2013, pp. 499-503. doi: 10.1061/(ASCE)MT.1943-5533.0000829

17. Lokuge, W.; Wilson, A.; Gunasekara, C.; Law, D. W.; and Setunge, S., “Design of Fly Ash Geopolymer Concrete Mix Proportions Using Multivariate Adaptive Regression Spline Model,” Construction and Building Materials, V. 166, 2018, pp. 472-481. doi: 10.1016/j.conbuildmat.2018.01.175

18. Bilgehan, M., and Turgut, P., “Artificial Neural Network Approach to Predict Compressive Strength of Concrete Through Ultrasonic Pulse Velocity,” Research in Nondestructive Evaluation, V. 21, No. 1, 2010, pp. 1-7. doi: 10.1080/09349840903122042

19. Mozumder, R. A., and Laskar, A. I., “Prediction of Unconfined Compressive Strength of Geopolymer Stabilized Clayey Soil Using Artificial Neural Network,” Computers and Geotechnics, V. 69, 2015, pp. 291-300. doi: 10.1016/j.compgeo.2015.05.021

20. Nagajothi, S., and Elavenil, S., Influence of Aluminosilicate for the Prediction of Mechanical Properties of Geopolymer Concrete–Artificial Neural Network, Silicon, New York, 2019.

21. Nazari, A.; Hajiallahyari, H.; Rahimi, A.; Khanmohammadi, H.; and Amini, M., “Prediction Compressive Strength of Portland Cement-Based Geopolymers by Artificial Neural Networks,” Neural Computing and Applications, V. 31, No. 2, 2019, pp. 733-741. doi: 10.1007/s00521-012-1082-3

22. Nazari, A., “Application of Gene Expression Programming to Predict the Compressive Damage of Lightweight Aluminosilicate Geopolymer,” Neural Computing and Applications, V. 31, No. 2, 2019, pp. 767-776. doi: 10.1007/s00521-012-1137-5

23. Nazari, A., and Torgal, F. P., “Predicting Compressive Strength of Different Geopolymers by Artificial Neural Networks,” Ceramics International, V. 39, No. 3, 2013, pp. 2247-2257. doi: 10.1016/j.ceramint.2012.08.070

24. Yadollahi, M. M.; Benli, A.; and Demirboga, R., “Application of Adaptive Neuro-Fuzzy Technique and Regression Models to Predict the Compressive Strength of Geopolymer Composites,” Neural Computing and Applications, V. 28, No. 6, 2017, pp. 1453-1461. doi: 10.1007/s00521-015-2159-6

25. Lau, C. K.; Lee, H.; Vimonsatit, V.; Huen, W. Y.; and Chindaprasirt, P., “Abrasion Resistance Behaviour of Fly Ash Based Geopolymer Using Nanoindentation and Artificial Neural Network,” Construction and Building Materials, V. 212, 2019, pp. 635-644. doi: 10.1016/j.conbuildmat.2019.04.021


ALSO AVAILABLE IN:

Electronic Materials Journal