Nonlinear Analysis of Reinforced Concrete Members Subjected to Combined Torsion and Bending Moment

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Nonlinear Analysis of Reinforced Concrete Members Subjected to Combined Torsion and Bending Moment

Author(s): Hyunjin Ju and Deuckhang Lee

Publication: Structural Journal

Volume: 118

Issue: 4

Appears on pages(s): 55-70

Keywords: aggregate interlock; bending moment; concrete crushing; reinforced concrete; spalling; torsion; truss model

DOI: 10.14359/51732643

Date: 7/1/2021

Abstract:
This study aims to develop a torsional behavior model for reinforced concrete (RC) members subjected to torsional moment combined with flexure. In the suggested method, the cross section of an RC member is idealized by using a thin-walled tube consisting of shear panel elements, where the shear flow is developed along its perimeter zone. Those panels are further divided into the compression and tension zones considering the normal stresses induced by flexural moment. The panel elements subjected to combined shear and normal stresses induced by torsional and flexural moments, respectively, are then analyzed by using the softened truss model. The multiple failure criteria are addressed to identify the failure mode and determine the ultimate strength of an RC member. Based on the detailed verifications by comparisons of test results collected from literature with those estimated by the proposed method, it was concluded that the proposed method can capture the torsional responses of RC specimens with a high level of accuracy.

Related References:

1. Collins, M. P.; Walsh, P. F.; Archer, F. E.; and Hall, A. S., “Ultimate Strength of Reinforced Concrete Beams Subjected to Combined Torsion and Bending,” Torsion of Structural Concrete, SP-18, G. P. Fisher, ed., American Concrete Institute, Farmington Hills, MI, 1968, pp. 279-402.

2. Lampert, P., and Collins, M. P., “Torsion, Bending, and Confusion-An Attempt to Establish the Facts,” ACI Journal Proceedings, V. 69, No. 8, Aug. 1972, pp. 500-504.

3. Lampert, P., and Thürlimann, B., “Torsion,-Bending Tests of Reinforced Concrete Beams,” Report No. 6506-3, Institut fűr Baustatik, ETH, Zurich, Switzerland, 1969, 116 pp.

4. McMullen, A. E., and Warwaruk, J. M., “Concrete Beams in Bending, Torsion, and Shear,” Journal of Structural Engineering, ASCE, V. 96, 1970, pp. 885-903.

5. Onsongo, W. M., “The Diagonal Compression Field Theory for Reinforced Concrete Beams Subjected to Combined Torsion, Flexure and Axial Loads,” PhD thesis, Department of Civil Engineering, University of Toronto, Toronto, ON, Canada, 1978, 246 pp.

6. Cardenas, A., and Sozen, M. A., “Strength and Stiffness of Isotropically and 28 Nonisotropically Reinforced Concrete Slabs Subjected to Combinations of Flexural and Torsional Moments,” Structural Research Series, No. 336, 1968, 250 pp.

7. Lampert, P., and Thürlimann, B., “Ultimate Strength and Design of Reinforced Concrete Beams in Torsion and Bending,” International Association of Bridge and Structural Engineering, V. 31-I, 1971, pp. 107-131.

8. McMullen, A. E., and Warwaruk, J., The Torsional Strength of Rectangular Reinforced Concrete Beams Subjected to Combined Loading (Research Report, University of Alberta, Edmonton, AB, Canada), 1967, 162 pp.

9. Greene, G. G., “Behavior of Reinforced Concrete Girders under Cyclic Torsion and Torsion Combined with Shear: Experimental Investigation and Analytical Models,” PhD thesis, Department of Civil, Architectural, and Environmental Engineering, Missouri University of Science and Technology, Rolla, MO, 2006.

10. Rahal, K. N., “Combined Torsion and Bending in Reinforced and Prestressed Concrete Beams Using Simplified Method for Combined Stress-Resultants,” ACI Structural Journal, V. 104, No. 4, July-Aug. 2007, pp. 402-411.

11. Bredt, R., “Kritische Bemerkungen zur Drehungselastizitat. Z Vereines Deutscher Ingenieure,” Band, V. 40, No. 28, 1896, pp. 785-790.

12. Hsu, T. T. C., and Zhang, L. X., “Nonlinear Analysis of Membrane Elements by Fixed-Angle Softened-Truss Model,” ACI Structural Journal, V. 94, No. 5, Sept.-Oct 1997, pp. 483-492.

13. Ju, H.; Lee, D. H.; Cho, H. C.; Kim, K. S.; Yoon, S.; and Seo, S. Y., “Application of Hydrophilic Silanol-Based Chemical Grout for Strengthening Damaged Reinforced Concrete Flexural Members,” Materials (Basel), V. 7, No. 6, 2014, pp. 4823-4844.

14. Lee, D. H.; Han, S. J.; and Kim, K. S., “Dual Potential Capacity Model for Reinforced Concrete Beams Subjected to Shear,” Structural Concrete, V. 17, No. 3, 2016, pp. 443-456.

15. Lee, D. H.; Han, S. J.; Hwang, J. H.; Ju, H.; and Kim, K. S., “Simplification and Verification of Dual Potential Capacity Model For Reinforced Concrete Beams Subjected to Shear,” Structural Concrete, V. 18, No. 2, 2016, pp. 259-277.

16. Hsu, T. T. C., and Mo, Y. L., Unified Theory of Concrete Structures, Wiley & Sons, Inc.s, Chichester, UK, 2010, 500 pp.

17. Hsu, T. T. C., Torsion of Reinforced Concrete, Van Nostrand Reinhold, Inc., New York, 1984, 516 pp.

18. Collins, M. P., and Mitchell, D., Prestressed Concrete Structures, Prentice Hall, Hoboken, NJ, 1991, 766 pp.

19. Kim, K. S., and Lee, D. H., “Nonlinear Analysis Method for Continuous Post-Tensioned Concrete Members with Unbonded Tendons,” Engineering Structures, V. 40, No. 1, 2012, pp. 487-500.

20. Hsu, T. T. C., and Zhang, L. X., “Tension Stiffening in Reinforced Concrete Membrane Element,” ACI Structural Journal, V. 93, No. 1, Jan.-Feb. 1996, pp. 108-115.

21. Lee, J.-Y., and Mansour, M. Y., “New Algorithm for Fixed-Angle Softened-Truss Model,” Proceedings of the ICE – Structures and Buildings, Vol. 159, No. 6, 2006, pp. 349-359.

22. Ju, H.; Lee, D. H.; Hwang, J. H.; Kang, J. W.; Kim, K. S.; and Oh, Y. H., “Torsional Behavior Model of Steel Fiber-Reinforced Concrete Members Modifying Fixed-Angle Softened-Truss Model,” Composites. Part B, Engineering, V. 45, No. 1, 2013, pp. 215-231.

23. Lee, J.-Y., and Kim, S.-W., “Torsional Strength of RC Beams Considering Tension Stiffening Effect,” Journal of Structural Engineering, ASCE, V. 136, No. 11, 2010, pp. 1367-1378.

24. Belarbi, A., and Hsu, T. T. C., “Constitutive Laws of Concrete in Tension and Reinforcing Bars Stiffened by Concrete,” ACI Structural Journal, V. 91, No. 4, July-Aug. 1994, pp. 465-474.

25. Jeng, C. H., and Hsu, T. T. C., “A Softened Membrane Model for Torsion in Reinforced Concrete Members,” Engineering Structures, V. 32, No. 9, 2009, pp. 1944-1954.

26. Pang, X. B., and Hsu, T. T. C., “Fixed-Angle Softened-Truss Model for Reinforced Concrete,” ACI Structural Journal, V. 93, No. 2, Mar.-Apr. 1996, pp. 197-207.

27. ACI Committee 318, “Building Code Requirements for Structural Concrete (ACI 318-14) and Commentary (ACI 318R-14),” American Concrete Institute, Farmington Hills, MI, 2014, 520 pp.

28. Hsu, T. T. C., and Mo, Y. L., “Softening of Concrete in Torsional Members—Theory And Tests,” ACI Journal Proceedings, V. 82, No. 3, May-June 1985, pp. 290-303.

29. Mitchell, D., and Collins, M. P., “Diagonal Compression Field Theory—A Rational Model For Structural Concrete in Pure Torsion,” ACI Journal Proceedings, V. 71, No. 8, 1974, pp. 396-408.

30. Ju, H.; Han, S. J.; Kim, K. S.; Strauss, A.; and Wu, W., “Multi-Potential Capacity for Reinforced Concrete Members under Pure Torsion,” Structural Engineering and Mechanics, V. 75, No. 3, 2020, pp. 401-414.

31. Walrarven, J. C., “Fundamental Analysis of Aggregate Interlock,” Journal of the Structural Division, ASCE, V. 107, 1981, pp. 2245-2270.

32. Rahal, K. N., “Behavior of Reinforced Concrete Beams Subjected to Combined Shear and Torsion,” PhD thesis, University of Toronto, Toronto, ON, Canada, 1993, 175 pp.

33. Belarbi, A., and Hsu, T. T. C., “Constitutive Laws of Softened Concrete in Biaxial Tension-Compression,” ACI Structural Journal, V. 92, No. 5, Sept.-Oct. 1995, pp. 562-573.

34. Stevens, N. J.; Uzumeri, S. M.; Collins, M. P.; and Will, G. T., “Constitutive Model for Reinforced Concrete Finite Element Analysis,” ACI Structural Journal, V. 88, No. 1, Jan.-Feb. 1991, pp. 49-59.

35. Vecchio, F. J., and Collins, M. P., The Response of Reinforced Concrete to In-Plane Shear and Normal Stresses, No. 82-03, Department of Civil Engineering, University of Toronto, Toronto, CA, 1982, 332 pp.

36. Vecchio, F. J., and Collins, M. P., “Modified Compression Field Theory for Concrete Elements Subjected to Shear,” ACI Journal Proceedings, V. 83, No. 2, Mar.-Apr. 1986, pp. 219-231.

37. Rahal, K. N., and Collins, M. P., “Analysis of Sections Subjected to Combined Shear and Torsion-A Theoretical Model,” ACI Structural Journal, V. 92, No. 4, July-Aug. 1995, pp. 459-469.


ALSO AVAILABLE IN:

Electronic Structural Journal