JSCE-SF6 Limitations for Shear Tests and ASTM D5607 Shear Tests on Fiber-Reinforced Concrete

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: JSCE-SF6 Limitations for Shear Tests and ASTM D5607 Shear Tests on Fiber-Reinforced Concrete

Author(s): Fulvio Tonon

Publication: Materials Journal

Volume: 118

Issue: 3

Appears on pages(s): 91-100

Keywords: fiber-reinforced concrete (FRC); glass fibers; shear capacity; shear failure; shear strength; shear stress; steel fibers; synthetic fibers

DOI: 10.14359/51732599

Date: 5/1/2021

Abstract:
Although several JSCE-SF6 tests have established the strength improvements caused by fiber reinforcement, it is unknown whether the measured strength improvements are caused by shear strength improvements (that is, Mode II), or by tensile or flexural strength improvement (Mode I). This paper provides a basic understanding of the state of stress: 1) in a JSCE-SF6 test; and 2) in an ASTM D5607 direct shear test, which has never been used earlier to investigate the shear strength of fiber-reinforced concrete (FRC). It was found that the JSCE-SF6 standard does not test the shear strength of a material, and it cannot be used to obtain shear characteristics of FRC. On the other hand, the ASTM D5607 standard can be used effectively to obtain shear characteristics of FRC because it creates a stress field very close to pure shear. The addition of steel fibers to concrete does not increase the peak shear strength of concrete.

Related References:

1. Valle, M., and Buyukozturk, O., “Behavior of Fiber Reinforced High-Strength Concrete under Direct Shear,” ACI Materials Journal, V. 90, No. 2, Mar.-Apr. 1993, pp. 122-133.

2. ACI Committee 544, “Guide to Design with Fiber-Reinforced Concrete (ACI 544.4R-18),” American Concrete Institute, Farmington Hills, MI, 2018, 4 pp.

3. Soetens, T., and Matthys, S., “Shear-Stress Transfer across a Crack in Steel Fibre-Reinforced Concrete,” Cement and Concrete Composites, V. 82, Sept. 2017, pp. 1-13. doi: 10.1016/j.cemconcomp.2017.05.010

4. Qasim, O. A., “Comparison between the Behaviors of Different Concrete Types in Various Shear Tests,” Proceedings, The Fourth Postgraduate Engineering Conference, IOP Conference Series: Materials Science and Engineering, Baghdad, Iraq, V. 745, 2020, doi: 10.1088/1757-899X/745/1/012176

5. Japan Society of Civil Engineers, “Method of Test for Shear Strength of Steel Fiber Reinforced Concrete (SFRC) (JSCE-SF6),” JSCE, Tokyo, Japan, 2005.

6. Fédération Internationale de la Précontrainte, “Shear at the Interface of Precast and In-Situ Concrete,” FIP, Lausanne, Switzerland, 1978.

7. Mostafazadeh, M., “Shear Behavior of Synthetic Fiber Reinforced Concrete Box Culverts,” PhD dissertation, Department of Civil Engineering, The University of Texas at Arlington, Arlington, TX, 2017.

8. Mirsayah, A. A., and Banthia, N., “Shear Strength of Steel Fiber-Reinforced Concrete,” ACI Materials Journal, V. 99, No. 5, Sept.-Oct. 2002, pp. 473-479.

9. Malatesta, S. C., and Contreras, M. C., “Shear Behavior of Steel Fiber Reinforced Concretes,” Revista de Ingeniería de Construcción, V. 24, No. 1, 2009, pp. 74-94.

10. Carmona, S., and Maripangui, F., “Comportamiento del Hormigón Reforzado con Fibras Sometido a Esfuerzo de Corte,” Anales de las XVI Jornadas Chilenas del Hormigón, Talca, Chile, 2007, 10 pp.

11. Mostafazadeh, M., and Abolmaali, A., “Shear Behavior of Synthetic Fiber Reinforced Concrete,” Advances in Civil Engineering Materials, V. 5, No. 1, 2016, pp. 371-386. doi: 10.1520/ACEM20160005

12. European Committee for Standardization, “Eurocode 2: Design of Concrete Structures—Part 1-1: General Rules and Rules for Buildings (EN 1992-1-1),” CEN, Brussels, Belgium, 2005.

13. Cornelissen, H. A. W.; Hordijk, D. A.; and Reinhardt, H. W., “Experimental Determination of Crack Softening Characteristics of Normalweight and Lightweight Concrete,” HERON, V. 31, No. 2, 1986, pp. 45-56.

14. Thorenfeldt, E.; Tomaszewicz, A.; and Jensen, J. J., “Mechanical Properties of High Strength Concrete and Application to Design,” Proceedings, Symposium: Utilization of High Strength Concrete, Stavanger, Norway, 1987, pp. 149-159.

15. Al-Mahaidi, R. S. H., “Nonlinear Finite Element Analysis of Reinforced Concrete Deep Members,” PhD thesis, Technical Report 79-1, Department of Structural Engineering, Cornell University, Ithaca, NY, 1979.

16. Naaman, A. E., and Reinhardt, H. W., “Proposed Classification of HPFRC Composites Based on Their Tensile Response,” Materials and Structures, V. 39, No. 5, 2006, pp. 547-555. doi: 10.1617/s11527-006-9103-2

17. Mostafazadeh, M.; Abolmaali, A.; and Ghahremannejad, M., “Shear Strength of Synthetic Fiber-Reinforced Concrete Box Culverts,” Journal of Bridge Engineering, ASCE, V. 24, No. 6, 2019, p. 04019039. doi: 10.1061/(ASCE)BE.1943-5592.0001402

18. Kovács, I., and Balázs, G. L., “Structural Performance of Steel Fibre Reinforced Concrete,” Proceedings, Second International Conference on Fibre Reinforced Concrete—From Research to Practice, Budapest University of Technology and Economics, Hungary, Nov. 19, 2004.


ALSO AVAILABLE IN: