Behavior of Lightweight Self-Consolidating Concrete Columns Reinforced with Glass Fiber-Reinforced Polymer Bars and Spirals under Axial and Eccentric Loads

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Behavior of Lightweight Self-Consolidating Concrete Columns Reinforced with Glass Fiber-Reinforced Polymer Bars and Spirals under Axial and Eccentric Loads

Author(s): Abdoulaye Sanni B., Hamdy M. Mohamed, Ammar Yahia, and Brahim Benmokrane

Publication: Structural Journal

Volume: 118

Issue: 3

Appears on pages(s): 241-253

Keywords: analytical P-M interaction diagram; axial and eccentric loading; axial-flexural capacity; circular reinforced concrete columns; design codes; glass fiber-reinforced polymer (GFRP) bars and spirals; lightweight self-consolidating concrete (LWSCC); lightwe

DOI: 10.14359/51730530

Date: 5/1/2021

Abstract:
This paper presents the test results of an experimental investigation conducted on 14 full-scale circular lightweight self-consolidating concrete (LWSCC) columns reinforced with glass fiber-reinforced polymer (GFRP) bars and spirals. The 300 mm (12 in.) diameter columns were designed according to CAN/CSA S806-12 code requirements. The columns were constructed using new designed and developed LWSCC and tested under axial and eccentric loading. The test variables were the eccentricity-to-diameter ratio, longitudinal reinforcement ratio, and type of reinforcement (steel versus GFRP). Four eccentricity-to-diameter ratios were estimated and applied (8.2, 16.4, 32.8, and 65.6%) to develop the nominal failure envelope. Test results indicate that increasing the GFRP longitudinal-reinforcement ratio enhanced the post-peak performance of LWSCC columns. On the other hand, the failure mechanism of the tested LWSCC columns was similar to that reported previously for conventional reinforced normal-weight concrete columns. Based on the fundamentals of equilibrium of forces and compatibility of strains, the available equivalent stressblock parameters and design provisions in the literature were used to predict the axial-flexural capacity of the tested GFRP-reinforced LWSCC columns. The predicted i interaction diagrams are presented and discussed.

Related References:

ACI Committee 237, 2007, “Self-Consolidating Concrete (ACI 237R-07),” American Concrete Institute, Farmington Hills, MI, 30 pp.

ACI Committee 318, 2019, “Building Code Requirements for Structural Concrete (ACI 318-19) and Commentary (ACI 318R-19),” American Concrete Institute, Farmington Hills, MI, 624 pp.

ACI Committee 440, 2015, “Guide for the Design and Construction of Concrete Reinforced with FRP Bars (ACI 440.1R-15),” American Concrete Institute, Farmington Hills, MI, 88 pp.

Afifi, M. Z.; Mohamed, H. M.; and Benmokrane, B., 2014a, “Axial Capacity of Circular Concrete Columns Reinforced with GFRP Bars and Spirals,” Journal of Composites for Construction, ASCE, V. 18, No. 1, p. 04013017. doi: 10.1061/(ASCE)CC.1943-5614.0000438

Afifi, M. Z.; Mohamed, H. M.; and Benmokrane, B., 2014b, “Strength and Axial Behavior of Circular Concrete Columns Reinforced with CFRP Bars and Spirals,” Journal of Composites for Construction, ASCE, V. 18, No. 2, p. 04013035. doi: 10.1061/(ASCE)CC.1943-5614.0000430

Afifi, M. Z.; Mohamed, H. M.; and Benmokrane, B., 2015a, “Theoretical Stress-Strain Model for Circular Concrete Columns Confined by GFRP Spirals and Hoops,” Engineering Structures, V. 102, pp. 202-213. doi: 10.1016/j.engstruct.2015.08.020

Afifi, M. Z.; Mohamed, H. M.; Chaallal, O.; and Benmokrane, B., 2015b, “Confinement Model for Concrete Columns Internally Confined with Carbon FRP Spirals and Hoops,” Journal of Structural Engineering, ASCE, V. 141, No. 9, p. 04014219. doi: 10.1061/(ASCE)ST.1943-541X.0001197

AL-Eliwi, B. J. M.; Ekmekyapar, T.; AL-Samaraie, M. I. A.; and Doğru, M. H., AL-Eliwi, 2018, “Behavior of Reinforced Lightweight Aggregate Concrete-filled Circular Steel Tube Columns Under Axial Loading,” Structures, V. 16, pp. 101-111. doi: 10.1016/j.istruc.2018.09.001

Allington, C.; Bull, D.; Park, R.; and McSaveney, L., 1998, “Ductility of Lightweight Aggregate Concrete Columns,” Combined Concrete Industry Conference 1998 - Commerce Of Concrete – Source To Market, NZ Combined Concrete Industry Conference, 9 pp.

ASTM C150/C150M-18, 2018, “Standard Specification for Portland Cement,” ASTM International, West Conshohocken, PA, 9 pp.

ASTM C330/C330M-17a, 2017, “Standard Specification for Lightweight Aggregates for Structural Concrete,” ASTM International, West Conshohocken, PA, 4 pp.

ASTM C39/C39M-15a, 2015, “Standard Test Method for Compressive Strength of Cylindrical Concrete Specimens,” ASTM International, West Conshohocken, PA, 7 pp.

ASTM C567/C567M-14, 2014, “Standard Test Method for Determining Density of Structural Lightweight Concrete,” ASTM International, West Conshohocken, PA, 4 pp.

CAN/CSA A23.3, 2014, “Design of Concrete Structures,” Canadian Standards Association, Rexdale, ON, Canada.

CAN/CSA S806, 2012, “Design and Construction of Building Structures with Fibre Reinforced Polymers S806-12 (R2017),” Canadian Standards Association, Rexdale, ON, Canada.

Chandra, S., and Berntsson, L., 2002, Lightweight Aggregate Concrete: Science, Technology and Applications, first edition, 450 pp.

Chen, H. J.; Wu, K. C.; Tang, C. W.; and Huang, C. H., 2018, “Engineering Properties of Self-Consolidating Lightweight Aggregate Concrete and Its Application in Prestressed Concrete Members,” Sustainability, V. 10, No. 1, p. 142. doi: 10.3390/su11010142

Cui, H. Z.; Lo, T. Y.; Memon, S. A.; and Xu, W., 2012, “Effect of Lightweight Aggregates on the Mechanical Properties and Brittleness of Lightweight Aggregate Concrete,” Construction and Building Materials, V. 35, pp. 149-158. doi: 10.1016/j.conbuildmat.2012.02.053

Fillmore, B., and Sadeghian, P., 2018, “Contribution of Longitudinal Glass Fiber-Reinforced Polymer Bars in Concrete Cylinders under Axial Compression,” Canadian Journal of Civil Engineering, V. 45, No. 6, pp. 458-468. doi: 10.1139/cjce-2017-0481

Guérin, M.; Mohamed, H. M.; Benmokrane, B.; Nanni, A.; and Shield, C. K., 2018a, “Eccentric Behavior of Full-Scale Reinforced Concrete Columns with Glass Fiber-Reinforced Polymer Bars and Ties,” ACI Structural Journal, V. 115, No. 2, Mar., pp. 489-499. doi: 10.14359/51701107

Guérin, M.; Mohamed, H. M.; Benmokrane, B.; Shield, C. K.; and Nanni, A., 2018b, “Effect of Glass Fiber-Reinforced Polymer Reinforcement Ratio on Axial-Flexural Strength of Reinforced Concrete Columns,” ACI Structural Journal, V. 115, No. 4, July, pp. 1049-1061. doi: 10.14359/51701279

Hadhood, A.; Mohamed, H. M.; and Benmokrane, B., 2017a, “Strength of Circular HSC Columns Reinforced Internally with Carbon-Fiber-Reinforced Polymer Bars under Axial And Eccentric Loads,” Construction and Building Materials, V. 141, pp. 366-378. doi: 10.1016/j.conbuildmat.2017.02.117

Hadhood, A.; Mohamed, H. M.; and Benmokrane, B., 2017b, “Experimental Study of Circular High-Strength Concrete Columns Reinforced with GFRP Bars and Spirals under Concentric and Eccentric Loading,” Journal of Composites for Construction, ASCE, V. 21, No. 2, p. 04016078. doi: 10.1061/(ASCE)CC.1943-5614.0000734

Hadhood, A.; Mohamed, H. M.; and Benmokrane, B., 2017c, “Axial Load-Moment Interaction Diagram of Circular Concrete Columns Reinforced with CFRP Bars and Spirals: Experimental and Theoretical Investigations,” Journal of Composites for Construction, ASCE, V. 21, No. 2, p. 04016092. doi: 10.1061/(ASCE)CC.1943-5614.0000748

Hadhood, A.; Mohamed, H. M.; and Benmokrane, B., 2017d, “Failure Envelope of Circular Concrete Columns Reinforced with Glass Fiber-Reinforced Polymer Bars and Spirals,” ACI Structural Journal, V. 114, No. 6, Nov.-Dec., pp. 1417-1428. doi: 10.14359/51689498

Hadhood, A.; Mohamed, H. M.; and Benmokrane, B., 2018, “Flexural Stiffness of GFRP- and CFRP-RC Circular Members under Eccentric Loads Based on Experimental and Curvature Analysis,” ACI Structural Journal, V. 115, No. 4, July, pp. 1185-1198. doi: 10.14359/51702235

Hadhood, A.; Mohamed, H. M.; Benmokrane, B.; Nanni, A.; and Shield, C. K., 2019, “Assessment of Design Guidelines of Concrete Columns Reinforced with Glass Fiber-Reinforced Polymer Bars,” ACI Structural Journal, V. 116, No. 4, July, pp. 193-207. doi: 10.14359/51715663

Hadhood, A.; Mohamed, H. M.; Ghrib, F.; and Benmokrane, B., 2017e, “Efficiency of Glass-Fiber Reinforced-Polymer (GFRP) Discrete Hoops and Bars in Concrete Columns under Combined Axial and Flexural Loads,” Composites. Part B, Engineering, V. 114, pp. 223-236. doi: 10.1016/j.compositesb.2017.01.063

Hadi, M. N. S.; Karim, H.; and Sheikh, M. N., 2016, “Experimental Investigations on Circular Concrete Columns Reinforced with GFRP Bars and Helices under Different Loading Conditions,” Journal of Composites for Construction, ASCE, V. 20, No. 4, p. 04016009. doi: 10.1061/(ASCE)CC.1943-5614.0000670

Maranan, G. B.; Manalo, A. C.; Benmokrane, B.; Karunasena, W.; and Mendis, P., 2016, “Behavior of Concentrically Loaded Geopolymer-Concrete Circular Columns Reinforced Longitudinally and Transversely with GFRP Bars,” Engineering Structures, V. 117, pp. 422-436. doi: 10.1016/j.engstruct.2016.03.036

Meng, W.; Samaranayake, V. A.; and Khayat, K. H., 2018, “Factorial Design and Optimization of Ultra-High-Performance Concrete with Lightweight Sand,” ACI Materials Journal, V. 115, No. 1, Jan., pp. 129-138. doi: 10.14359/51700995

Mohamed, H. M.; Afifi, M. Z.; and Benmokrane, B., 2014, “Performance Evaluation of Concrete Columns Reinforced Longitudinally with FRP Bars and Confined with FRP Hoops and Spirals under Axial Load,” Journal of Bridge Engineering, ASCE, V. 19, No. 7, p. 04014020. doi: 10.1061/(ASCE)BE.1943-5592.0000590

Mousa, A.; Mahgoub, M.; and Hussein, M., 2018, “Lightweight Concrete in America: Presence and Challenges,” Sustainable Production and Consumption, V. 15, pp. 131-144. doi: 10.1016/j.spc.2018.06.007

Pultrall Inc, 2017, “Composite Reinforcing Rods Technical Data Sheet,” Thetford Mines, QC, Canada, www.pultrall.com.

Qian, J.; Luo, H.; and Huang, J., 1998, “The Effect of Brittleness on Strength of Concrete,” Proceedings of FraMCoS-3, Gifu, Japan. Aedificatio Publishers, Freiburg, Germany, pp. 2031-2040.

Salah-Eldin, A.; Mohamed, H. M.; and Benmokrane, B., 2019a, “Structural Performance of High-Strength-Concrete Columns Reinforced with GFRP Bars and Ties Subjected to Eccentric Loads,” Engineering Structures, V. 185, pp. 286-300. doi: 10.1016/j.engstruct.2019.01.143

Salah-Eldin, A.; Mohamed, H. M.; and Benmokrane, B., 2019b, “Axial-Flexural Performance of High-Strength-Concrete Bridge Compression Members Reinforced with Basalt-FRP Bars and Ties: Experimental and Theoretical Investigation,” Journal of Bridge Engineering, ASCE, V. 24, No. 7, p. 04019069. doi: 10.1061/(ASCE)BE.1943-5592.0001448

Short, A., and Kinniburgh, W., 1978, Lightweight Concrete, third edition, Applied Science Publishers Ltd., London, UK, 464 pp.

Tobbi, H.; Farghaly, A. S.; and Benmokrane, B., 2012, “Concrete Columns Reinforced Longitudinally and Transversally with Glass Fiber-Reinforced Polymer Bars,” ACI Structural Journal, V. 109, No. 4, July-Aug., pp. 551-558.

Wu, T.; Wei, H.; Zhang, Y.; and Liu, X., 2018, “Axial Compressive Behavior of Lightweight Aggregate Concrete Columns Confined with Transverse Steel Reinforcement,” Advances in Mechanical Engineering, V. 10, No. 3, p. 1687814018766632 doi: 10.1177/1687814018766632

Yahia, A., and Khayat, K. H., 2012, “Statistical Modelling of the Coupled Effect of Mix Design and Rebar Spacing on Restricted Flow Characteristics of SCC,” Construction and Building Materials, V. 37, Dec., pp. 699-706.

Yahia, A.; Khayat, K. H.; and Bizien, G., 2011, “Use of Self-Consolidating Concrete to Cast Large Concrete Pipes,” Canadian Journal of Civil Engineering, V. 38, No. 10, pp. 1112-1121. doi: 10.1139/l11-065

Zadeh, H. J., and Nanni, A., 2013, “Design of RC Columns Using Glass FRP Reinforcement,” Journal of Composites for Construction, ASCE, V. 17, No. 3, pp. 294-304. doi: 10.1061/(ASCE)CC.1943-5614.0000354


ALSO AVAILABLE IN:

Electronic Structural Journal