Influence of Fiber Geometry and Type on Creep Rupture of Cracked Fiber-Reinforced Shotcrete Mixtures

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Influence of Fiber Geometry and Type on Creep Rupture of Cracked Fiber-Reinforced Shotcrete Mixtures

Author(s): Erik Stefan Bernard

Publication: Materials Journal

Volume: 118

Issue: 2

Appears on pages(s): 3-12

Keywords: creep; fiber-reinforced shotcrete; macrosynthetic fibers; pullout; rupture; slippage; steel fibers; testing; time-dependent behavior

DOI: 10.14359/51730410

Date: 3/1/2021

Abstract:
It is well known that creep can affect the serviceability of concrete structures, including tunnel linings made using fiber-reinforced shotcrete (FRS). However, the possible effect of creep on the strength of structures is seldom explicitly considered in design. For cracked FRS loaded in tension or flexure, creep rupture of the fiber-concrete composite, either by pullout or rupture of fibers, can lead to structural collapse, at least when no alternative load path exists. In the present investigation, the influence of fiber geometry and surface roughness on creep rupture (expressed as the time-to- collapse) of FRS panel specimens subjected to a sustained flexural-tensile load has been assessed. The results suggest that geometric aspects of fiber design influence the propensity of the fiber composite to suffer creep rupture at a crack, and that collapse primarily occurs as a result of fiber pullout rather than tertiary creep of individual fibers. For the fibers presently investigated, geometric aspects of fiber design appear to exert a greater influence on creep rupture of the fiber composite than the properties of the material comprising the fibers.

Related References:

1. Wittman, F. H., “Creep and Shrinkage Mechanisms,” Creep and Shrinkage of Concrete Structures, Z. P. Bažant, and F. H. Wittman, eds., Wiley, Chichester, UK, 1982, pp. 129-161.

2. Bažant, Z. P., ed., Mathematical Modeling of Creep and Shrinkage of Concrete, Wiley, Chichester, UK, 1988.

3. Rusch, H., “Researches toward a General Flexural Theory for Structural Concrete,” ACI Journal Proceedings, V. 57, No. 1, Jan. 1960, pp. 1-28.

4. Gossla, U., and Rieder, K.-A., “Time Dependent Behaviour of Fibre Reinforced Concrete—Fundamentals and Applications,” Proceedings, Fifth Central European Congress on Concrete Engineering, Baden, Austria, September 24-25, 2009, pp. 109-114.

5. Bernard, E. S., “Influence of Fiber Type on Creep Deformation of Cracked Fiber-Reinforced Shotcrete Panels,” ACI Materials Journal, V. 107, No. 5, Sept.-Oct. 2010, pp. 474-480.

6. Zerbino, R. L., and Barragan, B. E., “Long-Term Behavior of Cracked Steel Fiber-Reinforced Concrete Beams under Sustained Loading,” ACI Materials Journal, V. 109, No. 2, Mar.-Apr. 2012, pp. 215-224.

7. Kurtz, S., and Balaguru, P., “Postcrack Creep of Polymeric Fiber-Reinforced Concrete in Flexure,” Cement and Concrete Research, V. 30, No. 2, 2000, pp. 183-190. doi: 10.1016/S0008-8846(99)00228-8

8. Buratti, N., and Mazzotti, C., “Experimental Tests on the Effect of Temperature on the Long-Term Behaviour of Macrosynthetic Fibre Reinforced Concretes,” Construction and Building Materials, V. 95, Oct, 2015, pp. 133-142. doi: 10.1016/j.conbuildmat.2015.07.073

9. Kusterle, W., “Flexural Creep Tests on Unnotched Beams—9 Years of Experience with Synthetic Macro Fibers,” Symposium, BEFIB 2016—Ninth RILEM International Symposium on Fiber Reinforced Concrete, Vancouver, BC, Canada, Sept. 19-21, 2016.

10. Reid, S. G., and Bernard, E. S., “De-Bonding of Shotcrete Linings at the Substrate Boundary,” Proceedings, World Tunnel Congress 2019, Naples, Italy, May 3-9, 2019.

11. Bernard, E. S., “Creep Rupture of Steel Fibre Reinforced Shotcrete Loaded in Flexure,” Symposium, Seventh International Symposium on Sprayed Concrete, Modern Use of Wet Mix Sprayed Concrete for Underground Support, Sandefjord, Norway, June 16-19, 2014.

12. Turner, S., “Creep of Polymeric Materials,” Encyclopedia of Materials: Science and Technology, K. H. J. Buschow, M. C. Flemings, E. J. Kramer, and P. Veyssière, eds., Elsevier Science, New York, 2001, pp. 1813-1817.

13. Boshoff, W. P., and Nieuwoudt, P. D., “Tensile Creep of Cracked Steel Fibre Reinforced Concrete: Mechanisms on the Single Fibre and at the Macro Level,” Proceedings of the International RILEM Workshop FRC-Creep 2016, Valencia, P. Serna, A. Llano-Torre, and S. H. P. Cavalaro, eds., Springer, Dordrecht, The Netherlands, 2017, pp. 63-75.

14. Parmentier, B.; Vandewalle, L.; and Van Rickstal, F., “Evaluation of the Scatter of the Postpeak Behaviour of Fibre Reinforced Concrete in Bending: A Step towards Reliability,” BEFIB 2008: Seventh International Symposium on Fibre Reinforced Concrete, R. Gettu, ed., RILEM, 2008, pp. 133-143.

15. Cavalaro, S. H. P., and Aguado, A., “Intrinsic Scatter of FRC: An Alternative Philosophy to Estimate Characteristic Values,” Materials and Structures, V. 48, No. 11, 2015, pp. 3537-3555. doi: 10.1617/s11527-014-0420-6

16. ASTM C1550, “Standard Test Method for Flexural Toughness of Fiber Reinforced Concrete (Using Centrally Loaded Round Panel),” ASTM International, West Conshohocken, PA.

17. Barton, N., and Grimstad, E., “The Q-System Following Thirty Years of Development and Application in Tunneling Projects,” Symposium, Rock Engineering—Theory and Practice, Proceedings of the ISRM Regional Symposium EUROCK 2004, Salzburg, Austria, 2004, pp. 15-18.

18. Conforti, A.; Minelli, F.; Plizzari, G. A.; and Tiberti, G., “Comparing Test Methods for the Mechanical Characterization of Fiber Reinforced Concrete,” Structural Concrete—fib, V. 19, No. 3, 2018, pp. 656-669.

19. Bernard, E. S., and Xu, G. G., “Crack Widths in ASTM C1550 Panels,” Shotcrete: Elements of a System, E. S. Bernard, ed., Taylor & Francis, London, 2010, pp. 21-28.

20. Tyler, D., and Clements, M. J. K., “High Toughness Shotcrete for Large Deformation Control at Perseverance Mine,” Shotcrete: More Engineering Developments, E. S. Bernard, ed., Taylor & Francis, London, UK, 2004, pp. 259-266.

21. Bjøntegaard, O.; Myren, S. A.; Klemetsrud, K.; and Kompen, R., “Fibre Reinforced Sprayed Concrete (FRSC): Energy Absorption Capacity from 2 Days Age to One Year,” Symposium, Seventh International Symposium on Sprayed Concrete, Sandefjord, Norway, June 16-19, 2014, pp. 88-97.

22. Bernard, E. S., “Age-Dependent Changes in Post-Crack Performance of Fibre Reinforced Shotcrete Linings,” Tunnelling and Underground Space Technology, V. 49, Jun, 2015, pp. 241-248. doi: 10.1016/j.tust.2015.05.006

23. Zhou, F. P., “Time-Dependent Crack Growth and Fracture in Concrete,” Doctoral thesis TVBM-1011, Division of Building Materials, Lund Institute of Technology, Lund, Sweden, 1992.

24. Davis, J. R., “Concise Metals Engineering Data Book,” ASM International, Materials Park, OH, 1997.


ALSO AVAILABLE IN:

Electronic Materials Journal