Concrete Q&A: Compressive Strength of Cores and Specification Compliance

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Concrete Q&A: Compressive Strength of Cores and Specification Compliance

Author(s):

Publication: Concrete International

Volume: 42

Issue: 12

Appears on pages(s): 80

Keywords:

DOI: 10.14359/51730384

Date: 12/1/2020

Abstract:

Q: Last winter, we placed concrete grade beams for an industrial building. A technician from the owner’s testing agency took test cylinders but left them unprotected in the cold weather for a week. At 28 days, the average cylinder compressive strength was 2750 psi. Because this was far below the specified fc of 6000 psi, the engineer required three cores to be taken to evaluate the in-place concrete strength. The individual core compressive strengths were 4940, 4970, and 5370 psi, resulting in an average strength of 5090 psi (84.8% of fc). The engineer rejected the concrete on the basis that the ACI 318-19 Code1 requires the average core strength to equal 85% of the specified strength. In this case, 0.85 fc = 5100 psi, so isn’t the average core strength of 5090 psi close enough?

Related References:

1. ACI Committee 318, “Building Code Requirements for Structural Concrete (ACI 318-19) and Commentary (ACI 318R-19),” American Concrete Institute, Farmington Hills, MI, 2019, 623 pp.

2. Suprenant, B.A., “Understanding Concrete Core Testing,” NRMCA Publication No. 185, National Ready Mixed Concrete Association, Alexandria, VA, 19 pp.

3. ACI Technical Activities Committee, “Technical Committee Manual (ACI TCM-20),” American Concrete Institute, Farmington Hills, MI, 2020, 72 pp.