Title: Strain-based fatigue failure criterion for steel-fiber reinforced concrete

Author(s): Poveda, E.; Ruiz, G.; Cifuentes, H.; Yu, R.C.; Zhang, X.X.

Publication: Symposium Paper

Volume: 343

Issue:

Appears on pages(s): 302-309

Keywords: Secondary strain rate, steel-fiber reinforced concrete, fibers, compression fatigue.

DOI:

Date: 10/1/2020

Abstract:
This work proposes a new strain-based failure criterion for compression fatigue in steelfiber reinforced concrete. It is based on the Spark and Menzies’ relationship between the logarithm of the secondary strain rate per cycle and the specimen life expressed as the logarithm of the number of cycles until failure. This relationship permits calculating the critical strain at the failure of the specimen as the sum of two terms. The first one is the maximum strain in the first cycle due to the maximum compression stress. The second term is the increase of strain due to the remaining cycles until failure. Thus, failure occurs when the strain reaches a critical level during fatigue loading. On the contrary, the material continues resisting while its accumulated strain is lower than the critical one. This criterion is validated against a series of low-cycle fatigue tests in five types of concrete with different amounts of fiber that share the same concrete matrix. Besides, the experimental results show that the fibers delay the deformation and deterioration processes caused by fatigue. They also show that there is an optimum fiber content that maximizes fatigue life.




  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

Edit Module Settings to define Page Content Reviewer