Title: Experimental Behaviour of Precast Tunnel Segments in Steel Fiber Reinforcement with GFRP Rebars

Author(s): Meda, A.; Rinaldi, Z.; Spagnuolo, S.; De Rivaz, B.; Giamundo, N.

Publication: Symposium Paper

Volume: 343

Issue:

Appears on pages(s): 153-162

Keywords: Tunnel segments, hybrid solution, Fiber reinforced concrete, GFRP reinforcement, full scale tests.

DOI:

Date: 10/1/2020

Abstract:
The interest in using fiber reinforced concrete (FRC) for the production of precast segments in tunnel lining, installed with Tunnel Boring Machines (TBMs), is continuously growing, as witnessed by the studies available in literature and by the actual applications. The possibility of adopting a hybrid solution of FRC tunnel segments with Glass Fiber Reinforced Polymer (GFRP) reinforcement is investigated herein. Full-scale tests were carried out on FRC segments with and without GFRP cage, with a typical geometry of metro tunnels. In particular, both flexural and point load full-scale tests were carried out, for the evaluation of the structural performances (both in terms of structural capacity and crack pattern evolution) under bending, and under the TBM thrust. Finally, the obtained results are compared, in order to judge the effectiveness of the proposed technical solution.




  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

Edit Module Settings to define Page Content Reviewer