Flexural Behavior of Post-Tensioned Normal- and High-Strength Concrete-Filled Fiber-Reinforced Polymer Tubes

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Flexural Behavior of Post-Tensioned Normal- and High-Strength Concrete-Filled Fiber-Reinforced Polymer Tubes

Author(s): Asmaa Abdeldaim Ahmed, Mohamed Hassan, and Radhouane Masmoudi

Publication: Structural Journal

Volume: 118

Issue: 2

Appears on pages(s): 73-88

Keywords: beams; concrete-filled FRP tubes (CFFT); confinement; fiber-reinforced polymer (FRP); high-strength concrete (HSC); post-tensioning; steel tendons

DOI: 10.14359/51728178

Date: 3/1/2021

Abstract:
This paper investigates the effect of using the post-tensioning (PT) on the flexural strength and ductility of rectangular concrete-filled fiber-reinforced polymer (FRP) tube (CFFT) beams. A total of eight PT CFFTs and two PT concrete beams, serving as control specimens, were tested up to failure under four-point static monotonic and cyclic loading. The effects of prestressed reinforcement, FRP tube versus steel stirrups, tube thickness, concrete type (normal- and high-strength concrete [NSC and HSC]), number of strands, and loading schemes were investigated. The test results revealed that the CFFTs post-tensioned with steel tendons could successfully improve serviceability and ultimate flexural capacity with good ductility behavior and energy absorption capacity compared to nonprestressed CFFT and PT concrete beams. PT CFFT beam achieved approximately 25% and 143% (on average) higher strength than those of CFFT and PT concrete specimens, respectively. Flexural capacities of PT CFFTs can be enhanced by increasing the concrete compressive strength without affecting their overall ductility. Increasing the number of strands had a slight effect on ultimate capacity and total energy absorption, but it did affect the cracking and deflection behavior. Furthermore, insignificant strength reduction occurred due to the cyclic loading of the PT CFFT beam compared to the monotonic loading specimen. Finally, a simple model was proposed to predict the flexural moment capacity of the tested PT CFFT beams as well as nonprestressed rectangular CFFT beams from the literature. The model yielded good yet conservative predictions with an average ratio (Mu(exp)/M(pred.)) of 1.06 ± 0.16 and a COV of 14.7%.

Related References:

AASHTO, 2012, “AASHTO LRFD Guide Specifications for Design of Concrete-Filled FRP Tubes for Flexural and Axial Members,” American Association of State Highway and Transportation Officials, Washington, DC.

Abouzied, A., and Masmoudi, R., 2015, “Structural Performance of New Fully and Partially Concrete-Filled Rectangular FRP-Tube Beams,” Construction and Building Materials, V. 101, pp. 652-660. doi: 10.1016/j.conbuildmat.2015.10.060

Abouzied, A., and Masmoudi, R., 2017, “Flexural Behavior of Rectangular FRP-Tubes Filled with Reinforced Concrete: Experimental and Theoretical Studies,” Engineering Structures, V. 133, pp. 59-73. doi: 10.1016/j.engstruct.2016.12.010

ACI Committee 374, 2013, “Guide for Testing Reinforced Concrete Structural Elements Under Slowly Applied Simulated Seismic Loads (ACI 374.2R-13),” American Concrete Institute, Farmington Hills, MI, 412 pp.

Ahmed, A. A.; Hassan, M.; Mohamed, H.; Ahmed, A.; and Masmoudi, R., 2018, “Axial Behavior of Circular CFFT Long Columns Internally Reinforced with Steel or Carbon and Glass FRP Longitudinal Bars,” Engineering Structures, V. 155, pp. 267-278. doi: 10.1016/j.engstruct.2017.11.037

ASTM D3039/D3039M-17, 2017, “Standard Test Method for Tensile Properties of Polymer Matrix Composite Materials,” ASTM International, West Conshohocken, PA, 2017.

ASTM C39/C39M-18, “Standard Test Method for Compressive Strength of Cylindrical Concrete Specimens,” ASTM International, West Conshohocken, PA, 2018.

ASTM D695-15, 2015, “Standard Test Method for Compressive Properties of Rigid Plastics,” ASTM International, West Conshohocken, PA. doi: 10.1520/D0695-1510.1520/D0695-15

Booker, A. J., 2008, “Performance of Continuous and Segmented Post-Tensioned Concrete Filled Fiber Tubes,” Master’s thesis, Department of Civil Engineering, Washington State University, Pullman, WA, 115 pp.

CAN/CSA S6-14, 2014, “Canadian Highway Bridge Design Code (CHBDC),” Canadian Standards Association, Rexdale, ON, Canada, 894 pp.

CSA-A23.3 M-14, 2014, “Design of Concrete Structures for Buildings,” Canadian Standards Association, Rexdale, ON, Canada, 240 pp.

ElGawady, M.; Booker, A.; and Dawood, H. M., 2010, “Seismic Behavior of Posttensioned Concrete-Filled Fiber Tubes,” Journal of Composites for Construction, ASCE, V. 14, No. 5, pp. 616-628. doi: 10.1061/(ASCE)CC.1943-5614.0000107

Fam, A., and Mandal, S. K., 2006, “Prestressed Concrete–Filled Fiber-Reinforced Polymer Circular Tubes Tested in Flexure,” PCI Journal, V. 51, No. 4, pp. 42-54. doi: 10.15554/pcij.07012006.42.54

Fam, A., and Rizkalla, S., 2002, “Flexural Behavior of Concrete Filled Fiber-Reinforced Polymer Circular Tubes,” Journal of Composites for Construction, ASCE, V. 6, No. 2, pp. 123-132. doi: 10.1061/(ASCE)1090-0268(2002)6:2(123)

Fam, A.; Schnerch, D.; and Rizkalla, S., 2005, “Rectangular Filament-Wound Glass Fiber Reinforced Polymer Tubes Filled with Concrete under Flexural and Axial loading: Experimental Investigation,” Journal of Composites for Construction, ASCE, V. 9, No. 1, pp. 25-33. doi: 10.1061/(ASCE)1090-0268(2005)9:1(25)

Grace, N. F.; Soliman, A. K.; Abdel-Sayed, G.; and Saleh, K. R., 1998, “Behavior and Ductility of Simple and Continuous FRP Reinforced Beams,” Journal of Composites for Construction, ASCE, V. 2, No. 4, pp. 186-194. doi: 10.1061/(ASCE)1090-0268(1998)2:4(186)

Idris, Y., and Ozbakkaloglu, T., 2014, “Flexural Behavior of FRP-HSC-Steel Composite Beams,” Thin-walled Structures, V. 80, pp. 207-216. doi: 10.1016/j.tws.2014.03.011

Jaeger, L.; Mufti, A.; and Tadros, G., 1997, “The Concept of the Overall Performance Factor in Rectangular-Section Reinforced Concrete Beams,” Proceedings of the 3rd International Symposium on Non-Metallic (FRP) Reinforcement for Concrete Structures, Japan Concrete Institute, Tokyo, Japan, pp. 551-558.

Mandal, S., and Fam, A., 2006, “Modeling of Prestressed Concrete-Filled Circular Composite Tubes Subjected to Bending and Axial Loads,” Journal of Structural Engineering, ASCE, V. 132, No. 3, pp. 449-459. doi: 10.1061/(ASCE)0733-9445(2006)132:3(449)

Masmoudi, R., and Abouzied, A., 2018, “2018, “Flexural Performance and Deflection Prediction of Rectangular FRP-Tube Beams Fully or Partially Filled with Reinforced Concrete,” Journal of Structural Engineering, ASCE, V. 144, No. 6, p. 04018067 doi: 10.1061/(ASCE)ST.1943-541X.0002055

Mirmiran, A., and Shahawy, M., 1999, “Partially Prestressed Concrete Filled Fiber-Reinforced Polymer FRP Tubes,” Proc., Advances in Composite Materials and Mechanics, ASCE, Reston, VA, pp. 85-94.

Naaman, A. E., and Jeong, S. M., 1995, “Structural Ductility of Concrete Beams Prestressed with FRP Tendons,” Non-Metallic (FRP) Reinforcement for Concrete Structures, L. Taewre, ed., E & FN Spon, London, UK, pp. 379-386.

Park., R., 1989, “Evaluation of Ductility of Structures and Structural Assemblages From Laboratory Testing.” Bulletin of the New Zealand National Society for Earthquake Engineering, V. 22, No. 3.

Rosenboom, O. A., and Kowalsky, M. J., 2004, “Reversed in-Plane Cyclic Behavior of Posttensioned Clay Brick Masonry Walls,” Journal of Structural Engineering, ASCE, V. 130, No. 5, pp. 787-798. doi: 10.1061/(ASCE)0733-9445(2004)130:5(787)

Xue, W.; Tan, Y.; and Peng, F., Jan. 2020, “Experimental Study on Damaged Prestressed Concrete Beams Using External Post-Tensioned Tendons,” ACI Structural Journal, V. 117, No. 1, Jan., pp. 159-168. doi: 10.14359/51718019


ALSO AVAILABLE IN:

Electronic Structural Journal