Title:
Freezing-and-Thawing Behavior of Cementitious Materials Containing Superabsorbent Polymers at Early Ages
Author(s):
Ming Jin, Rita Maria Ghantous, Jiayin Tao, and Jason Weiss
Publication:
Materials Journal
Volume:
117
Issue:
6
Appears on pages(s):
243-252
Keywords:
cement paste; freezing and thawing; internal curing; residual strain; superabsorbent polymers (SAP)
DOI:
10.14359/51728130
Date:
11/1/2020
Abstract:
This paper examines the relationship between the curing time and freezing-and-thawing (F-T) resistance of internally cured (IC) cement paste using superabsorbent polymers (SAP). The degree of saturation (DOS), the amount of freezable water, and F-T damage resistance of plain and IC cement paste at different ages were assessed. For cement paste with a water-cement ratio (w/c) of 0.50 and higher, IC increased the DOS, and the DOS remained higher than the critical DOS even after 28 days of curing, thereby making these mixtures susceptible to F-T damage. For mixtures with a lower w/c, IC increased the DOS at early ages, but the DOS was similar to or less than that of plain cement paste at later ages. IC slightly increases the susceptibility of low w/c mixtures to F-T damage only at very early ages; this susceptibility decreases after 7 days of curing. It is recommended that care be taken to avoid F-T damage during the first few days when IC is used for mixtures with a higher w/c (that is, above 0.42).
Related References:
1. Fagerlund, G., “The Significance of Critical Degrees of Saturation at Freezing of Porous and Brittle Materials,” Durability of Concrete, SP-47, American Concrete Institute, Farmington Hills, MI, 1975, pp. 13-66.
2. Fagerlund, G., “A Service Life Model for Internal Frost Damage in Concrete,” Report TVBM, V. 3119, Division of Building Materials, LTH, Lund University, Lund, Sweden, 2004.
3. Litvan, G. G., “Freeze-Thaw Durability of Porous Building Materials,” Durability of Building Materials and Components, P. Sereda and G. Litvan, eds., ASTM International, West Conshohocken, PA, 1980, pp. 455-463.
4. Hall, C., “Water Sorptivity of Mortars and Concretes: A Review,” Magazine of Concrete Research, V. 41, No. 147, 1989, pp. 51-61. doi: 10.1680/macr.1989.41.147.51
5. Fagerlund, G., “The International Cooperative Test of the Critical Degree of Saturation Method of Assessing the Freeze/Thaw Resistance of Concrete,” Materiales de Construcción, V. 10, 1977, pp. 231-253.
6. Li, W.; Pour-Ghaz, M.; Castro, J.; and Weiss, J., “Water Absorption and Critical Degree of Saturation Relating to Freeze-Thaw Damage in Concrete Pavement Joints,” Journal of Materials in Civil Engineering, ASCE, V. 24, No. 3, 2012, pp. 299-307. doi: 10.1061/(ASCE)MT.1943-5533.0000383
7. Fagerlund, G., “The Critical Degree of Saturation Method of Assessing the Freeze/Thaw Resistance of Concrete,” Materiales de Construcción, V. 10, 1977, pp. 217-229.
8. Fagerlund, G., “Degré Critique de Saturation un Outil pour l’estimation de la Résistance au gel des Matériaux de Construction,” Materiales de Construcción, V. 4, Sept, 1971, pp. 271-285.
9. Todak, H.; Lucero, C.; and Weiss, J., “Why Is the Air There? Thinking about Freeze-Thaw in Terms of Saturation,” Concrete in Focus, Spring 2015, pp. OC3-OC7.
10. Farnam, Y.; Todak, H.; Spragg, R.; and Weiss, J., “Electrical Response of Mortar with Different Degrees of Saturation and Deicing Salt Solutions during Freezing and Thawing,” Cement and Concrete Composites, V. 59, May, 2015, pp. 49-59. doi: 10.1016/j.cemconcomp.2015.03.003
11. Todak, H.; Tsui, M.; Ley, T.; and Weiss, J., “Freeze-Thaw Resistance of Concrete: The Influence of Air Entrainment, Water to Cement Ratio, and Saturation,” Proceedings, Eleventh International Symposium on Brittle Matrix Composites, Warsaw, Poland, 2015.
12. Lura, P.; Jensen, O. M.; and Van Breugel, K., “Autogenous Shrinkage in High-Performance Cement Paste: An Evaluation of Basic Mechanisms,” Cement and Concrete Research, V. 33, No. 2, 2003, pp. 223-232. doi: 10.1016/S0008-8846(02)00890-6
13. Glosser, D.; Azad, V. J.; Suraneni, P.; Isgor, B.; and Weiss, J., “Extension of Powers-Brownyard Model to Pastes Containing Supplementary Cementitious Materials,” ACI Materials Journal, V. 116, No. 5, Sept. 2019, pp. 205-216. doi: 10.14359/51714466
14. Wyrzykowski, M.; Igarashi, S. I.; Lura, P.; and Mechtcherine, V., “Recommendation of RILEM TC 260-RSC: Using Superabsorbent Polymers (SAP) to Mitigate Autogenous Shrinkage,” Materials and Structures, V. 51, No. 5, 2018, p. 135 doi: 10.1617/s11527-018-1241-9
15. Kovler, K., and Zhutovsky, S., “Overview and Future Trends of Shrinkage Research,” Materials and Structures, V. 39, No. 9, 2006, pp. 827-847. doi: 10.1617/s11527-006-9114-z
16. Wu, L.; Farzadnia, N.; Shi, C.; Zhang, Z.; and Wang, H., “Autogenous Shrinkage of High Performance Concrete: A Review,” Construction and Building Materials, V. 149, 2017, pp. 62-75. doi: 10.1016/j.conbuildmat.2017.05.064
17. Tu, W.; Zhu, Y.; Fang, G.; Wang, X.; and Zhang, M., “Internal Curing of Alkali-Activated Fly Ash-Slag Pastes Using Superabsorbent Polymer,” Cement and Concrete Research, V. 116, 2019, pp. 179-190. doi: 10.1016/j.cemconres.2018.11.018
18. Almeida, F. C. R., and Klemm, A. J., “Efficiency of Internal Curing by Superabsorbent Polymers (SAP) in PC-GGBS Mortars,” Cement and Concrete Composites, V. 88, 2018, pp. 41-51. doi: 10.1016/j.cemconcomp.2018.01.002
19. Jones, T. R., and Stephenson, H. K., “Properties of Lightweight Concrete Related to Prestressing,” Texas Transportation Institute, College Station, TX, 1957.
20. Barrett, T. J., “Improving Service Life of Concrete Structures through the Use of Internal Curing: Impact on Practice,” PhD thesis, Civil Engineering, Purdue University, West Lafayette, IN, 2015, p. 483.
21. De la Varga, I.; Castro, J.; Bentz, D.; and Weiss, J., “Application of Internal Curing for Mixtures Containing High Volumes of Fly Ash,” Cement and Concrete Composites, V. 34, No. 9, 2012, pp. 1001-1008. doi: 10.1016/j.cemconcomp.2012.06.008
22. Jones, W. A., “Examining the Freezing and Thawing Behavior of Concretes with Improved Performance through Internal Curing and Other Methods,” MSCE thesis, Civil Engineering, Purdue University, West Lafayette, IN, 2014, p. 151.
23. Li, M.; Liu, J.; Tian, Q.; Wang, Y.; and Xu, W., “Efficacy of Internal Curing Combined with Expansive Agent in Mitigating Shrinkage Deformation of Concrete under Variable Temperature Condition,” Construction and Building Materials, V. 145, 2017, pp. 354-360. doi: 10.1016/j.conbuildmat.2017.04.021
24. Craeye, B.; Geirnaert, M.; and De Schutter, G., “Super Absorbing Polymers as an Internal Curing Agent for Mitigation of Early-Age Cracking of High-Performance Concrete Bridge Decks,” Construction and Building Materials, V. 25, No. 1, 2011, pp. 1-13. doi: 10.1016/j.conbuildmat.2010.06.063
25. Bentz, D. P., and Jensen, O. M., “Mitigation Strategies for Autogenous Shrinkage Cracking,” Cement and Concrete Composites, V. 26, No. 6, 2004, pp. 677-685. doi: 10.1016/S0958-9465(03)00045-3
26. Craeye, B.; Cockaerts, G.; and Kara De Maeijer, P., “Improving Freeze–Thaw Resistance of Concrete Road Infrastructure by Means of Superabsorbent Polymers,” Infrastructures, V. 3, No. 1, 2018, p. 4 doi: 10.3390/infrastructures3010004
27. Chatterji, S., “Freezing of Air-Entrained Cement-Based Materials and Specific Actions of Air-Entraining Agents,” Cement and Concrete Composites, V. 25, No. 7, 2003, pp. 759-765. doi: 10.1016/S0958-9465(02)00099-9
28. Mechtcherine, V.; Schrӧfl, C.; Wyrzykowski, M.; Gorges, M.; Lura, P.; Cusson, D.; Margeson, J.; De Belie, N.; Snoeck, D.; Ichimiya, K.; Igarashi, S.; Falikman, V.; Friedrich, S.; Bokern, J.; Kara, P.; Marciniak, A.; Reinhardt, H.; Sippel, S.; Ribeiro, A. B.; Custódio, J.; Ye, G.; Dong, H.; and Weiss, J., “Effect of Superabsorbent Polymers (SAP) on the Freeze–Thaw Resistance of Concrete: Results of a RILEM Interlaboratory Study,” Materials and Structures, V. 50, No. 1, 2017, p. 14 doi: 10.1617/s11527-016-0868-7
29. Jones, W.; House, M.; and Weiss, J., “Internal Curing of High Performance Concrete Using Lightweight Aggregates and Other Techniques,” Purdue University, West Lafeyette, IN, 2014, p. 129.
30. Suzuki, T.; Shiotani, T.; and Ohtsu, M., “Evaluation of Cracking Damage in Freeze-Thawed Concrete Using Acoustic Emission and X-Ray CT Image,” Construction and Building Materials, V. 136, 2017, pp. 619-626. doi: 10.1016/j.conbuildmat.2016.09.013
31. Ebrahimi, K.; Daiezadeh, M. J.; Zakertabrizi, M.; Zahmatkesh, F.; and Korayem, A. H., “A Review of the Impact of Micro- and Nanoparticles on Freeze-Thaw Durability of Hardened Concrete: Mechanism Perspective,” Construction and Building Materials, V. 186, 2018, pp. 1105-1113. doi: 10.1016/j.conbuildmat.2018.08.029
32. Trofimov, B. Y.; Kramar, L. Y.; and Schuldyakov, K., “On Deterioration Mechanism of Concrete Exposed to Freeze-Thaw Cycles,” IOP Conference Series. Materials Science and Engineering, V. 262, 2017, pp. 1-6. doi: 10.1088/1757-899X/262/1/012019
33. Beaudoin, J. J., and MacInnis, C., “Dimensional Changes of Hydrated Portland Cement Paste during Slow Cooling and Warming,” Cement and Concrete Research, V. 2, No. 2, 1972, pp. 225-240. doi: 10.1016/0008-8846(72)90044-0
34. Vuorinen, J., “On Use of Dilation Factor and Degree of Saturation in Testing Concrete for Frost Resistance,” Nordisk Betong, V. 14, No. 1, 1970, pp. 37-64.
35. Montanari, L.; Suraneni, P.; and Weiss, W. J., “Accounting for Water Stored in Superabsorbent Polymers in Increasing the Degree of Hydration and Reducing the Shrinkage of Internally Cured Cementitious Mixtures,” Advances in Civil Engineering Materials, V. 6, No. 1, 2017, pp. 583-599. doi: 10.1520/ACEM20170098
36. Montanari, L.; Suraneni, P.; Chang, M. T.; Villani, C.; and Weiss, J., “Absorption and Desorption of Superabsorbent Polymers for Use in Internally Cured Concrete,” Advances in Civil Engineering Materials, V. 7, No. 4, 2018, pp. 547-566. doi: 10.1520/ACEM20180008
37. ASTM C305-06, “Standard Practice for Mechanical Mixing of Hydraulic Cement Pastes and Mortars of Plastic Consistency,” ASTM International, West Conshohocken, PA, 2006, 3 pp.
38. Ghantous, R. M.; Madland, H.; Kwong, J.; and Weiss, J., “Examining the Influence of the Degree of Saturation on Length Change and Freeze-Thaw Damage,” Advances in Civil Engineering Materials, V. 8, No. 1, 2019, pp. 365-374. doi: 10.1520/ACEM20190001
39. Hasholt, M. T., and Jensen, O. M., “Chloride Migration in Concrete with Superabsorbent Polymers,” Cement and Concrete Composites, V. 55, 2015, pp. 290-297. doi: 10.1016/j.cemconcomp.2014.09.023
40. Espinoza-Hijazin, G., and Lopez, M., “Extending Internal Curing to Concrete Mixtures with W/C Higher Than 0.42,” Construction and Building Materials, V. 25, No. 3, 2011, pp. 1236-1242. doi: 10.1016/j.conbuildmat.2010.09.031
41. Jensen, O. M., and Hansen, P. F., “Water-Entrained Cement-Based Materials: I. Principles and Theoretical Background,” Cement and Concrete Research, V. 31, No. 4, 2001, pp. 647-654. doi: 10.1016/S0008-8846(01)00463-X
42. Fagerlund, G., “ Chemically Bound Water as Measure of Degree of Hydration: Method and Potential Errors,” Report TVBM, V. 3150, Division of Building Materials, Lund Institute of Technology, Lund, Sweden, 2009, p. 28.
43. Snyder, K. A., and Bentz, D. P., “Suspended Hydration and Loss of Freezable Water in Cement Pastes Exposed to 90% Relative Humidity,” Cement and Concrete Research, V. 34, No. 11, 2004, pp. 2045-2056. doi: 10.1016/j.cemconres.2004.03.007
44. Suraneni, P.; Azad, V. J.; Isgor, B.; and Weiss, J., “Role of Supplementary Cementitious Material Type in the Mitigation of Calcium Oxychloride Formation in Cementitious Pastes,” Journal of Materials in Civil Engineering, ASCE, V. 30, No. 10, 2018, p. 04018248. doi: 10.1061/(ASCE)MT.1943-5533.0002425
45. Montanari, L.; Amirkhanian, A. N.; Suraneni, P.; and Weiss, J., “Design Methodology for Partial Volumes of Internal Curing Water Based on the Reduction of Autogenous Shrinkage,” Journal of Materials in Civil Engineering, ASCE, V. 30, No. 7, 2018, p. 04018137. doi: 10.1061/(ASCE)MT.1943-5533.0002331
46. Li, W.; Pour-Ghaz, M.; Castro, J.; and Weiss, J., “Water Absorption and Critical Degree of Saturation Relating to Freeze-Thaw Damage in Concrete Pavement Joints,” Journal of Materials in Civil Engineering, ASCE, V. 24, No. 3, 2012, pp. 299-307. doi: 10.1061/(ASCE)MT.1943-5533.0000383
47. Powers, T. C., “Basic Considerations Pertaining to Freezing- and-Thawing Tests,” ASTM Proceedings, V. 55, ASTM International, West Conshohocken, PA, 1955, pp. 1132-1155.
48. Fagerlund, G., “Effect of the Freezing Rate on the Frost Resistance of Concrete,” Nordic Concrete Research, Norsk Betongforening, Oslo, Norway, 1992, pp. 20-36.
49. Esmaeeli, H. S.; Farnam, Y.; Bentz, D. P.; Zavattieri, P. D.; and Weiss, J., “Numerical Simulation of the Freeze-Thaw Behavior of Mortar Containing Deicing Salt Solution,” Materials and Structures, V. 50, No. 1, 2017, p. 96 doi: 10.1617/s11527-016-0964-8
50. Powers, T. C., “Structure and Physical Properties of Hardened Portland Cement Paste,” Journal of the American Ceramic Society, V. 41, No. 1, 1958, pp. 1-6. doi: 10.1111/j.1151-2916.1958.tb13494.x
51. Powers, T. C., and Brownyard, T. L., “Studies of the Physical Properties of Hardened Portland Cement Paste,” ACI Journal Proceedings, V. 43, No. 9, Nov. 1946, pp. 249-336.
52. Sun, Z., and Scherer, G. W., “Effect of Air Voids on Salt Scaling and Internal Freezing,” Cement and Concrete Research, V. 40, No. 2, 2010, pp. 260-270. doi: 10.1016/j.cemconres.2009.09.027
53. Cai, H., and Liu, X., “Freeze-Thaw Durability of Concrete: Ice Formation Process in Pores,” Cement and Concrete Research, V. 28, No. 9, 1998, pp. 1281-1287. doi: 10.1016/S0008-8846(98)00103-3