Computational Determination of Interface Fracture Properties for Concrete by Inverse Analysis

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Computational Determination of Interface Fracture Properties for Concrete by Inverse Analysis

Author(s): Xun Xi, Shangtong Yang, Xiaofei Hu, and Chun-Qing Li

Publication: Materials Journal

Volume: 117

Issue: 6

Appears on pages(s): 43-53

Keywords: cohesive crack model; fracture energy; fracture mechanics; heterogeneous concrete; interfacial transition zone (ITZ); inverse analysis; meso-scale

DOI: 10.14359/51728123

Date: 11/1/2020

Abstract:
The interfacial transition zone (ITZ) between cement mortar and aggregate significantly affects the cracking behavior of concrete. However, the fracture properties including the tensile strength and fracture energy of ITZ are hard to obtain directly from experiments. This paper develops an inverse numerical method for determining the fracture properties of ITZ based on a meso-scale fracture model and artificial neural network. Concrete is considered a multi-phase material, mainly consisting of aggregates, cement mortar, and ITZ. In the fracture model, cohesive elements are inserted in the mesh to achieve arbitrary cracking. The tensile strength and fracture energy of ITZ are the targeted variables to be inversely attained. A neural network is created and trained based on the simulated results, by which the optimized values of the targeted variables are obtained. Experimental results from RILEM tests are used to validate the numerical method.