Behavior of High-Strength Concrete and Normal-Strength Concrete Columns under Blast Loading

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Behavior of High-Strength Concrete and Normal-Strength Concrete Columns under Blast Loading

Author(s): Amer Hammoud and Hassan Aoude

Publication: Symposium Paper

Volume: 341

Issue:

Appears on pages(s): 1-26

Keywords: High-strength concrete, Columns, Blast, Shock Tube

DOI: 10.14359/51727020

Date: 6/30/2020

Abstract:
This paper presents the results from tests examining the performance of high-strength concrete (HSC) and normal-strength concrete (NSC) columns subjected to blast loading. As part of the study six columns built with varying concrete strengths were tested under simulated blast loads using a shock-tube. In addition to the effect of concrete strength, the effects of longitudinal steel ratio and transverse steel detailing were also investigated. The experimental results demonstrate that the HSC and NSC columns showed similar blast performance in terms of overall displacement response, blast capacity, damage and failure mode. However, when considering the results at equivalent blasts, doubling the concrete strength from 40 MPa to 80 MPa (6 to 12 ksi) resulted in 10%-20% reductions in maximum displacements. On the other hand, increasing the longitudinal steel ratio from ρ = 1.7% to 3.4% was found to increase blast capacity, while also reducing maximum displacements by 40-50%. The results also show that decreasing the tie spacing (from d/2 to d/4, where d is the section depth) improved blast performance by reducing peak displacements by 20-40% at equivalent blasts. The use of seismic ties also prevented bar buckling and reduced the extent of damage at failure. As part of the analytical study the response of the HSC columns was predicted using single-degree-of-freedom (SDOF) analysis. The resistance functions were developed using dynamic material properties, sectional analysis and a lumped inelasticity approach. The SDOF procedure was able to predict the blast response of HSC columns with reasonable accuracy, with an average error of 14%. A numerical parametric study examining the effects of concrete strength, steel ratio and tie spacing in larger-scale columns with 350 mm x 350 mm (14 in. x 14 in.) section was also conducted. The results of the numerical study confirm the conclusions from the experiments but indicate the need for further blast research on the effect of transverse steel detailing in larger-scale HSC columns.

Related References:

1. ACI Committee 363, "Report on High-Strength Concrete," ACI 363R-10, American Concrete Institute, Farmington Hills, MI, 2010, pp. 65.

2. ACI Committee 441, "Report on High-Strength Concrete Columns," ACI 441R-96, American Concrete Institute, Farmington Hills, MI, 1996, pp. 13.

3. Paultre P, Mitchell D, "Code Provisions for High Strength Concrete—An International Perspective," Concrete international, V. 25, No. 5. 2003, pp. 76-90.

4. Astarlioglu S, Krauthammer T, Morency D, Tran TP, "Behavior of reinforced concrete columns under combined effects of axial and blast-induced transverse loads," Engineering Structures, V. 55. 2013, pp. 26-34.

5. Reinschmidt KF, Hansen RJ, Yang CY, "Dynamic tests of reinforced concrete columns," ACI Structural Journal, V. 61, No. 3. 1964, pp. 317-334.

6. Louw M, "The behaviour of RC columns under impact loading," The Civil Engineer in South Africa, V. 34, No. 11. 1992, pp. 371-378.

7. Remennikov A, Kaewunruen S, "Impact resistance of reinforced concrete columns: experimental studies and design considerations," 19th Australasian Conference on the Mechanics of Structures and Materials, Christchurch, New Zealand, 2006.

8. Huynh L, Foster S, Valipour H, Randall R, "High strength and reactive powder concrete columns subjected to impact: experimental investigation," Construction and Building Materials, V. 78. 2015, pp. 153-171.

9. Saatcioglu M, Ozbakkaloglu T, Naumoski N, Lloyd A, "Response of earthquake-resistant reinforcedconcrete buildings to blast loadingThis article is one of a selection of papers published in the Special Issue on Blast Engineering," Canadian Journal of Civil Engineering, V. 36, No. 8. 2009, pp. 1378-1390.

10. Hayes JR, Woodson SC, Pekelnicky RG, Poland CD, Corley WG, Sozen M, "Can Strengthening for Earthquake Improve Blast and Progressive Collapse Resistance?," Journal of Structural Engineering, V. 131, No. 8. 2005, pp. 1157-1177.

11. Bao X, Li B, "Residual strength of blast damaged reinforced concrete columns," International Journal of Impact Engineering, V. 37, No. 3. 2010, pp. 295-308.

12. Kyei C, Braimah A, "Effects of transverse reinforcement spacing on the response of reinforced concrete columns subjected to blast loading," Engineering Structures, V. 142. 2017, pp. 148-164.

13. Fujikura S, Bruneau M, "Experimental Investigation of Seismically Resistant Bridge Piers under Blast Loading," Journal of Bridge Engineering, V. 16, No. 1. 2011, pp. 63-71.

14. Fujikura S, Bruneau M, Lopez-Garcia D, "Experimental Investigation of Multihazard Resistant Bridge Piers Having Concrete-Filled Steel Tube under Blast Loading," Journal of Bridge Engineering, V. 13, No. 6. 2008, pp. 586-594.

15. Williamson EB, Bayrak O, Davis C, Williams GD, "Performance of Bridge Columns Subjected to Blast Loads. I: Experimental Program," Journal of Bridge Engineering, V. 16, No. 6. 2011, pp. 693-702.

16. Lloyd A, "Performance of reinforced concrete columns under shock tube induced shock wave loading," PhD thesis, University of Ottawa, Civil Engineering, 2010.

17. Burrell RP, Aoude H, Saatcioglu M, "Response of SFRC columns under blast loads," Journal of Structural Engineering, V. 141, No. 9. 2014, pp. 04014209.

18. Astarlioglu S, Krauthammer T, "Response of normal-strength and ultra-high-performance fiberreinforced concrete columns to idealized blast loads," Engineering Structures, V. 61. 2014, pp. 1-12.

19. Xu J, Wu C, Xiang H, Su Y, Li Z-X, Fang Q, et al., "Behaviour of ultra high performance fibre reinforced concrete columns subjected to blast loading," Engineering Structures, V. 118. 2016, pp. 97-107.

20. Aoude H, Dagenais FP, Burrell RP, Saatcioglu M, "Behavior of ultra-high performance fiber reinforced concrete columns under blast loading," International Journal of Impact Engineering, V. 80. 2015, pp. 185-202.

21. Crawford JE, "State of the art for enhancing the blast resistance of reinforced concrete columns with fiber-reinforced plastic," Canadian Journal of Civil Engineering, V. 40, No. 11. 2013, pp. 1023-1033.

22. Carriere M, Heffernan PJ, Wight RG, Braimah A, "Behaviour of steel reinforced polymer (SRP) strengthened RC members under blast loadThis paper is one of a selection of papers in the Special Issue on Blast Engineering," Canadian Journal of Civil Engineering, V. 36, No. 8. 2009, pp. 1356-1365.

23. Canadian Standards Association (CSA), "Design of concrete structures," CAN/CSA A23.3-14, Mississauga, ON, 2014.

24. ASTM A370-19, "Standard Test Methods and Definitions for Mechanical Testing of Steel Products," ASTM International, West Conshohocken, PA, 2019, pp. 8.

25. Lloyd A, Jacques E, Saatcioglu M, Palermo D, Nistor I, Tikka T, "Capabilities and effectiveness of using a shock tube to simulate blast loading on structures and structural components," ACI SP-281: Behaviour of Concrete Structures Subjected to Blast and Impact Loadings. 2011, pp. 1-20.

26. Li Y, Algassem O, Aoude H, "Response of high-strength reinforced concrete beams under shock-tube induced blast loading," Construction and Building Materials, V. 189. 2018, pp. 420-437.

27. Luccioni B, Isla F, Codina R, Ambrosini D, Zerbino R, Giaccio G, et al., "Effect of steel fibers on static and blast response of high strength concrete," International Journal of Impact Engineering, V. 107. 2017, pp. 23-37.

28. Algassem O, Li Y, Aoude H, "Ability of steel fibers to enhance the shear and flexural behavior of highstrength concrete beams subjected to blast loads," Engineering Structures, V. 199. 2019, pp. 109611.

29. Légeron F, Paultre P, "Uniaxial Confinement Model for Normal- and High-Strength Concrete Columns," Journal of Structural Engineering, V. 129, No. 2. 2003, pp. 241-252.

30. Popovics S, "A numerical approach to the complete stress-strain curve of concrete," Cement and concrete research, V. 3, No. 5. 1973, pp. 583-599.

31. Soroushian P, Choi K-B, Alhamad A, "Dynamic Constitutive Behavior of Concrete," ACI Journal Proceedings, V. 83, No. 2. 1986.

32. Bischoff P, Perry S, "Compressive behaviour of concrete at high strain rates," Materials and structures, V. 24, No. 6. 1991, pp. 425-450.

33. Elfahal MM, Krauthammer T, Ohno T, Beppu M, Mindess S, "Size effect for normal strength concrete cylinders subjected to axial impact," International Journal of Impact Engineering, V. 31, No. 4. 2005, p. 461-481.

34. Guo YB, Gao GF, Jing L, Shim VPW, "Response of high-strength concrete to dynamic compressive loading," International Journal of Impact Engineering, V. 108. 2017, pp. 114-135.

35. CEB-FIP, "Model Code 1990," Comite Euro-International Du Beton, Paris. 1991, pp. 87-109.

36. Canadian Standards Association (CSA), "Design and assessment of buildings subjected to blast loads," CSA S850-12, Mississauga, ON, Canada, 2012, pp. 126.

37. Jacques E, Lloyd A, Saatcioglu M, "Predicting reinforced concrete response to blast loads," Canadian Journal of Civil Engineering, V. 40, No. 5. 2012, pp. 427-444.

38. Malvar LJ, "Review of static and dynamic properties of steel reinforcing bars," ACI Materials Journal, V. 95, No. 5. 1998, pp. 609-616.

39. Saatcioglu M, Lloyd A, Jacques E, Braimah A, Doudak G, "Focused research for development of a CSA standard on design and assessment of buildings subjected to blast loads," Interim report submitted to Public Works and Government Services Canada, Hazard Mitigation and Disaster Management Research Centre, University of Ottawa, Ottawa, Canada, 2011.

40. Yalcin C, Saatcioglu M, "Inelastic analysis of reinforced concrete columns," Computers & Structures, V. 77, No. 5. 2000, pp. 539-555.

41. Jacques E, "RCBLAST version. 0.5.1. http://www.rcblast.ca," 2014.

42. Biggs JM, "Introduction to structural dynamics." McGraw-Hill New York; 1964.