Parametric Service Load-Deflection Analyses of Reinforced Concrete Beams with Recycled Concrete Aggregates

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Parametric Service Load-Deflection Analyses of Reinforced Concrete Beams with Recycled Concrete Aggregates

Author(s): Adam M. Knaack and Yahya C. Kurama

Publication: Structural Journal

Volume: 117

Issue: 5

Appears on pages(s): 301-313

Keywords: immediate and time-dependent deflections; recycled concrete aggregates; reinforced concrete beams; sustained service loads

DOI: 10.14359/51725846

Date: 9/1/2020

Abstract:
This paper describes a numerical parametric investigation on the effects of coarse recycled concrete aggregates (RCAs) on the time-dependent sustained service-load deflections of reinforced concrete beams. The varied parameters are the volumetric replacement of coarse aggregate, concrete compressive strength, beam geometry (length, depth, width), rotational restraint at beam ends, top and bottom longitudinal steel areas, ultimate shrinkage strain, ultimate creep coefficient, and ambient relative humidity. In addition, RCA quality is quantified and varied through the water absorption and deleterious material content (for example, wood and asphalt). The beams were analyzed using a time-dependent concrete material model that can capture cracking, shrinkage, and creep behavior. The results show that the deflections of beams with good-quality RCA (with low water absorption and deleterious material content) are not much greater than those for beams with natural aggregate (NA). Importantly, RCA amount and quality have larger effects on the deflections of beams with less cracking (that is, shorter and/or deeper beams) and for beams with increased rotational restraint, for which allowable deflection limits would be less likely to govern design. There are significant differences between the ACI 318 time-dependent deflection factor and the numerical simulation results, with ACI 318 generally providing overly conservative estimates of the time-dependent factor, except for beams with minimal or no cracking. It is also found that RCA has a greater effect on the time-dependent deflections than on the initial deflection.

Related References:

ACI Committee 209, 1992, “Prediction of Creep, Shrinkage, and Temperature Effects in Concrete Structures (ACI 209R-92) (Reapproved 2008),” American Concrete Institute, Farmington Hills, MI, 47 pp.

ACI Committee 318, 2019, “Building Code Requirements for Structural Concrete (ACI 318-19) and Commentary (ACI 318R-19),” American Concrete Institute, Farmington Hills, MI, 624 pp.

Ajdukiewicz, A., and Kliszczewicz, A., 2011, “Long-Term Behavior of Reinforced-Concrete Beams and Columns Made of Recycled Aggregate Concrete,” fib Symposium, Prague, Czech Republic, pp. 479-482.

ASTM C33/C33M-08, 2008, “Standard Specification for Concrete Aggregates,” ASTM International, West Conshohocken, PA, 11 pp.

Azúa, G.; Gonzalez, M.; Arroyo, P.; and Kurama, Y., 2019, “Recycled Coarse Aggregates from Precast Plant and Building Demolitions: Environmental and Economic Modeling through Stochastic Simulations,” Journal of Cleaner Production, V. 210, pp. 1425-1434. doi: 10.1016/j.jclepro.2018.11.049

Brandes, M., and Kurama, Y., 2018a, “Effect of Recycled Concrete Aggregates on Strength and Stiffness Gain of Concrete and on Bond Strength of Steel Prestressing Strand,” PCI Journal, V. 63, No. 2, pp. 87-105. doi: 10.15554/pcij63.2-03

Brandes, M., and Kurama, Y., 2018b, “Behavior of Shear-Critical Prestressed Concrete Beams with Recycled Concrete Aggregates under Ultimate Loads,” Engineering Structures, V. 165, pp. 237-246. doi: 10.1016/j.engstruct.2018.03.029

Brandes, M., and Kurama, Y., 2018c, “Service-Load Behavior of Precast/Prestressed Concrete Beams with Recycled Concrete Aggregates,” ACI Structural Journal, V. 115, No. 3, May, pp. 861-873. doi: 10.14359/51702133

Brandes, M., and Kurama, Y., 2019, “Ultimate Behavior of Flexure-

Critical Prestressed Concrete Beams with Recycled Concrete Aggregates,” ACI Structural Journal, V. 116, No. 2, Mar., pp. 15-28. doi: 10.14359/51713287

Choi, W., and Yun, H., 2013, “Long-Term Deflection and Flexural Behavior of Reinforced Concrete Beams with Recycled Aggregate,” Materials & Design, V. 51, pp. 742-750. doi: 10.1016/j.matdes.2013.04.044

Domingo-Cabo, A.; Lazaro, C.; Lopez-Gayarre, F.; Serrano-Lopez, M. A.; Serna, P.; and Castano-Tabares, J. O., 2010, “Creep and Shrinkage of Recycled Aggregate Concrete,” Construction and Building Materials, V. 23, No. 3, pp. 2545-2553.

Etxeberria, M.; Vázquez, E.; Marí, A.; and Barra, M., 2007, “Influence of Amount of Recycled Coarse Aggregates and Production Process on Properties of Recycled Aggregate Concrete,” Cement and Concrete Research, V. 37, No. 5, pp. 735-742. doi: 10.1016/j.cemconres.2007.02.002

Fathifazl, G.; Razaqpur, A.; Isgor, O.; Abbas, A.; Fournier, B.; and Foo, S., 2010, “Shear Strength of Reinforced Recycled Concrete Beams with Stirrups,” Magazine of Concrete Research, V. 62, No. 10, pp. 685-699. doi: 10.1680/macr.2010.62.10.685

INDOT, 2012, “Standard Specifications,” Indiana Department of Transportation, Indianapolis, IN.

Kamara, M. E., and Novak, L. C., 2011, Simplified Design of Reinforced Concrete Buildings, fourth edition, Portland Cement Association, Skokie, IL.

Knaack, A., and Kurama, Y., 2013, “Design of Concrete Mixtures with Recycled Concrete Aggregates,” ACI Materials Journal, V. 110, No. 5, Sept.-Oct., pp. 483-493.

Knaack, A., and Kurama, Y., 2015a, “Creep and Shrinkage of Normal Strength Concrete with Recycled Concrete Aggregates,” ACI Materials Journal, V. 112, No. 3, May-June, pp. 451-462. doi: 10.14359/51687392

Knaack, A., and Kurama, Y., 2015b, “Sustained Service-Load Behavior of Concrete Beams with Recycled Concrete Aggregates,” ACI Structural Journal, V. 112, No. 5, Sept.-Oct., pp. 565-577. doi: 10.14359/51687799

Knaack, A., and Kurama, Y., 2018, “Modeling Time-Dependent Deformations: Application for Reinforced Concrete Beams with Recycled Concrete Aggregates,” ACI Materials Journal, V. 115, No. 1, Jan., pp. 175-190.

Lapko, A., and Grygo, R., 2010, “Long Term Deflection of Recycled Aggregate Concrete (RAC) Beams Made of Recycled Concrete,” 10th International Conference: Modern Building Materials, Structures and Techniques, Vilnius, Lithuania.

Li, X., 2009, “Recycling and Reuse of Waste Concrete in China Part II: Structural Behavior of Recycled Aggregate Concrete and Engineering Applications,” Resources, Conservation and Recycling, V. 53, No. 3, pp.  107-112. doi: 10.1016/j.resconrec.2008.11.005

Lye, C.; Dhir, R.; and Ghataora, G., 2016b, “Shrinkage of Recycled Aggregate Concrete,” Proceedings of the Institution of Civil Engineers. Structures and Buildings, V. 169, No. 12, pp. 867-891. doi: 10.1680/jstbu.15.00138

Lye, C.; Dhir, R.; Ghataora, G.; and Li, H., 2016a, “Creep Strain of Recycled Aggregate Concrete,” Construction and Building Materials, V. 102, pp. 244-259. doi: 10.1016/j.conbuildmat.2015.10.181

Marí, A.; Bairán, J.; and Duarte, N., 2010, “Long-Term Deflections in Cracked Reinforced Concrete Flexural Members,” Engineering Structures, V. 32, No. 3, pp. 829-842. doi: 10.1016/j.engstruct.2009.12.009

Maruyama, I.; Oka, Y.; and Sato, R., 2005, “Time-Dependent Behavior of Reinforced Recycled Concrete Beams,” CONCREEP 7, Nantes, France.

Maruyama, I.; Sogo, M.; Sogabe, T.; Sato, R.; and Kawai, K., 2004, “Flexural Properties of Reinforced Recycled Concrete Beams.” International RILEM Conference on the Use of Recycled Materials in Building Structures, Barcelona, Spain, pp. 526-535.

McGinnis, M.; Davis, M.; de la Rosa, A.; Weldon, B.; and Kurama, Y., 2017a, “Quantified Sustainability of Recycled Concrete Aggregates,” Magazine of Concrete Research, V. 69, No. 23, pp. 1203-1211. doi: 10.1680/jmacr.16.00338

McGinnis, M. J.; Davis, M.; de la Rosa, A.; Weldon, B. D.; and Kurama, Y. C., 2017b, “Strength and Stiffness of Concrete with Recycled Aggregate Concrete,” Construction & Building Materials, V. 154, pp. 258-269. doi: 10.1016/j.conbuildmat.2017.07.015

OpenSees, 2006, “The Open System for Earthquake Engineering Simulation,” Pacific Earthquake Engineering Research Center, Berkeley, CA, opensees.berkeley.edu. (last accessed Aug. 12, 2020)

Rahal, K., 2007, “Mechanical Properties of Concrete with Recycled Coarse Aggregates,” Building and Environment, V. 42, No. 1, pp. 407-415. doi: 10.1016/j.buildenv.2005.07.033

Sato, R.; Maruyama, I.; Sogabe, T.; and Sogo, M., 2007, “2007, “Flexural Behavior of Reinforced Recycled Concrete Beams,” Journal of Advanced Concrete Technology, V. 5, No. 1, pp. 43-61. doi: 10.3151/jact.5.43

Seara-Paz, S.; González-Fonteboa, B.; Martínez-Abella, F.; and Carro-López, D., 2018, “Long-Term Flexural Performance of Reinforced Concrete Beams with Recycled Coarse Aggregates,” Construction and Building Materials, V. 176, pp. 593-607. doi: 10.1016/j.conbuildmat.2018.05.069

Tošić, N.; Marinković, S.; and Ignjatović, I., 2016, “A Database on Flexural and Shear Strength of Reinforced Recycled Aggregate Concrete Beams and Comparison to Eurocode 2 Predictions,” Construction and Building Materials, V. 127, pp. 932-944. doi: 10.1016/j.conbuildmat.2016.10.058

Tošić, N.; Marinkovic, S.; Pecic, N.; Ignjatovic, I.; and Dragas, J., 2018, “Long-Term Behaviour of Reinforced Beams Made with Natural or Recycled Aggregate Concrete and High-Volume Fly Ash Concrete,” Construction and Building Materials, V. 176, pp. 344-358. doi: 10.1016/j.conbuildmat.2018.05.002

Xiao, J.; Li, J.; and Zhang, C., 2005, “Mechanical Properties of Recycled Aggregate Concrete under Uniaxial Loading,” Cement and Concrete Research, V. 35, No. 6, pp. 1187-1194. doi: 10.1016/j.cemconres.2004.09.020


ALSO AVAILABLE IN:

Electronic Structural Journal