Development Length of Deformed Reinforcing Bars—A Worldwide Review

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Development Length of Deformed Reinforcing Bars—A Worldwide Review

Author(s): Christoph Mahrenholtz and Akanshu Sharma

Publication: Materials Journal

Volume: 117

Issue: 5

Appears on pages(s): 125-134

Keywords: bond; design; development; reinforcement; reinforcing bar

DOI: 10.14359/51725782

Date: 9/1/2020

Abstract:
The world becomes ever smaller and thus the global construction industry moves closer together. For this reason, civil engineers are looking for possibilities to harmonize design—for example, in the field of reinforced concrete structures. The streamlining would ease working in an international context and could offer opportunities for optimization: harmonization allows the identification of the technically best and most economical solution. This also holds for the provisions to calculate the development length of deformed reinforcing bars which, to date, differ notably from code to code. It is not reasonable that local codes define different development lengths for identical situations in terms of geometry and material used. This paper analyzes the provisions for the calculation of the development lengths according to internationally selected national codes as a basis for this discussion.

Related References:

1. PD-UN WPP, World Population Prospects, Population Division United Nations, New York, 2019.

2. IMF WEOD, World Economic Outlook Database of GDP (PPP), International Monetary Fund, Washington, DC, 2018.

3. Peters, K., and Inaudi, D., “Fiber Optic Sensors for Assessing and Monitoring Civil Structures,” Sensor Technologies for Civil Infrastructures, 2014.

4. Shull, L., “Basic Circuits,” Strain Gage Users’ Manual, 1992.

5. Mahrenholtz, C., “Seismic Bond Model for Concrete Reinforcement and the Application to Column-to-Foundation Connections,” dissertation, University of Stuttgart, Stuttgart, Germany, 2012.

6. Shima, H.; Chou, L.-L.; and Okamura, H., “Micro and Macro Models for Bond in Reinforced Concrete,” Journal of the Faculty of Engineering, V. 34, No. 2, University of Tokyo, Tokyo, Japan, 1987, pp. 133-194.

7. Metelli, G., and Plizzari, G., “Influence of the Relative Rib Area on Bond Behaviour,” Magazine of Concrete Research, V. 66, No. 6, 2014, pp. 277-294. doi: 10.1680/macr.13.00198

8. fib Model Code 2010, “Design Code,” Fédération Internationale du Béton, Lausanne, Switzerland, 2013.

9. NSCP, Structural Concrete, Association of Structural Engineers of the Philippines (ASEP), Quezon City, Philippines, 2015.

10. AIJ, Standard for Structural Calculation of Reinforced Concrete Structures, Architectural Institute of Japan (AIJ), Tokyo, Japan, 2010.

11. Hong Kong Buildings Department, Code of Practice for Structural Use of Concrete, Hong Kong Buildings Department, Kowloon, Hong Kong, 2013.

12. Macau, C. E. L., Code of Reinforced and Prestressed Concrete Structures,” Civil Engineering Laboratory of Macau, Macau, Macao, 1996.

13. EIT 1007-34, “Standard for Reinforced Concrete Building by Working Stress,” Engineering Institute of Thailand (EIT), Bangkok, Thailand, 2010.

14. AS 3600, “Concrete Structures,” Standards Australia, Sydney, Australia, 2009.

15. NZS 3101, “Concrete Structures Standard, Part 1: The Design of Concrete Structure. Part 2: Commentary on the Design of Concrete Structures,” New Zealand Standard Council, Wellington, New Zealand, 2006.

16. ACI Committee 318, “Building Code Requirements for Structural Concrete (ACI 318-19) and Commentary (ACI 318R-19),” American Concrete Institute, Farmington Hills, MI, 2019, 624 pp.

17. CIRSOC 201, “Reglamento Argentino de Estructuras,” Instituto Nacional de Tecnología Industrial (INTI), Argentina, 2005.

18. CSA A23.3-14, “Design of Concrete Structures,” Canadian Standards Association (CSA), Mississauga, ON, Canada, 2014.

19. NCh430, “Reinforced Concrete – Design and Calculation Requirements,” Instituto Nacional de Normalization (INN-Chile), Santiago, Chile, 2007.

20. SNI 03-2847-2013, “The Procedure for Calculating Concrete Structures for Buildings,” Standardisasi Nasional Indonesia (SNI), 2013.

21. BIS 103, “Gaceta Oficial del Distrito Federal,” Gobierno del Distrito Federal México, Mexico City, Mexico, 2004.

22. KCI Code, “Korea Structural Concrete Design Code 2012,” Korea Concrete Institute (KCI), Korea, 2012.

23. CICHE 401, “Reinforced Concrete Design Code and Commentary,” Chinese Institute of Civil and Hydraulic Engineering, Taiwan, 2011.

24. JSCE Guideline No. 15, “Standard Specifications for Concrete Structures 2007,” Japan Society of Civil Engineers (JSCE), Japan, 2007.

25. GB 50010, “Code for Design of Concrete Structures,” Guo Biao, Standardization Administration of China (SAC), China, 2015.

26. SP 63.13330.2012, “Concrete and Reinforced Concrete Structures General,” National Building Codes of Russia (SNiP), 2003.

27. TCVN 5574, “Concrete and Reinforced Concrete Structures – Design Standard,” Tieu Chuan Viet Nam (TCVN), Hanoi, Vietnam, 2018.

28. IS 456, “Plain and Reinforced Concrete – Code of Practice,” Bureau of Indian Standards (IS), New Delhi, India, 2000.

29. EN 1992, “Eurocode 2: Design of Concrete Structures,” European Committee for Standardization (CEN), Brussels, Belgium, 2010.

30. AISBL, Steel Statistical Yearbook 2018, World Steel Association, Brussels, Belgium, 2018.


ALSO AVAILABLE IN:

Electronic Materials Journal