Title: 
            Development of High-Strength Nano-Cementitious Composites Using Copper Slag
        
        
            Author(s): 
            S. Lavanya Prabha, M. Gopalakrishnan, and M. Neelamegam
        
        
            
                Publication: 
                Materials Journal
            
            
                Volume: 
                117
            
            
                Issue: 
                4
            
            
                Appears on pages(s): 
                37-46
            
            
                Keywords: 
                chloride ion permeability test; copper slag; high-strength cementitious composites; nano-cementitious composites
            
            
                DOI: 
                10.14359/51725778
            
        
        
            Date: 
            7/1/2020
        
        
            Abstract:
            This investigation was carried out to develop high-strength cementitious composite mixtures of compressive strength greater than 90 MPa (13.05 ksi). The main aim of this study is to develop high-strength cementitious composites having high density with low void content. To achieve the requirement, cement, copper slag, quartz powder, and silica fume ingredient proportions were arrived by optimum partial packing as well as the Dewar and Larrard method. More than 60 cementitious composite mixtures with and without high-strength micro-steel fiber and chopped basalt fiber were prepared and their compressive strength at the age of 28 days cured under normal water curing was investigated. In all the investigated trial mixtures, 100% copper slag was used instead of normal river sand and a required quantity of high-range water-reducing admixture (HRWRA) was used to maintain workability. Based on the 28-day compressive strength (greater than 90 MPa [13.05 ksi]), four cementitious composite mixtures were selected as optimized mixtures and their mechanical and durability properties were evaluated as per Indian Standard IS 516 and ASTM C469, and their rapid chloride permeability was assessed by ASTM C1202. X-ray diffraction (XRD) and scanning electron microscope (SEM) analysis were also carried out on four optimized composite mixtures. This project aims to develop mixtures suitable for the construction of storage buildings for arms and ammunition of defense research and development organizations (DRDO), and also these composites can be used in many special applications where high mechanical and durability properties are required.
        
     
    
    
    
            Related References:
                
                        1. Sambhaji, Z. K., and Autade, P. B., “Effect of Copper Slag as a Fine Aggregate on Properties of Cementitious Composites,” International Journal of Innovative Research in Advanced Engineering, V. 3, No. 8, 2016, pp. 4325-4329.
                    
                        2. Ambily, P. S.; Gunasekaran, U.; Ravisankar, K.; Prem, P. R.; Bharatkumar, B. H.; and Iyer, N. R., “Studies on Ultra-High-Performance Cementitious Composites Incorporating Copper Slag as Fine Aggregate,” Construction and Building Materials, V. 77, 2015, pp. 233-240. doi: 10.1016/j.conbuildmat.2014.12.092
                    
                        3. Al-Jabri, K. S.; Al-Saidy, A. H.; and Taha, R., “Effect of Copper Slag as a Fine Aggregate on the Properties of Cement Mortar and Concrete,” Construction and Building Materials, V. 25, No. 2, 2011, pp. 933-938. doi: 10.1016/j.conbuildmat.2010.06.090
                    
                        4. Zhang, M.-H.; Islam, J.; and Peethamparan, S., “Use of Nano-Silica to Increase Early Strength and Reduce Setting Time of Concretes with High Volumes of Slag,” Cement and Concrete Composites, V. 34, 2012, pp. 650-662. doi: 10.1016/j.cemconcomp.2012.02.005
                    
                        5. Wille, K.; Naaman, A. E.; El-Tawil, S.; and Parra-Montesinos, G., “Ultra-High-Performance Concrete and Fiber Reinforced Concrete: Achieving Strength and Ductility without Heat Curing,” Materials and Structures, V. 45, 2012, pp. 309-324. doi: 10.1617/s11527-011-9767-0
                    
                        6. Allena, S., and Newtson, C. M., “Ultra-High Strength Concrete Mixtures using Local Materials,” Civil Engineering Department, New Mexico State University, Las Cruces, NM, Apr. 2010, pp. 322-330.
                    
                        7. Snoeck, D.; Dewanckele, J.; Cnudde, V.; and De Belie, N., “X-Ray Computed Microtomography to Study Autogenous Healing of Cementitious Materials Promoted by Superabsorbent Polymers,” Cement and Concrete Composites, V. 65, 2016, pp. 83-93. doi: 10.1016/j.cemconcomp.2015.10.016
                    
                        8. IS 516-1959, “Methods of Test for Strength of Concrete,” Bureau of Indian Standards, New Delhi, India, 2004.
                    
                        9. ASTM C469-14, “Standard Test Method for Static Modulus of Elasticity and Poisson’s Ratio of Concrete in Compression,” ASTM International, West Conshohocken, PA, 2014.
                    
                        10. IS 4031-6, “Methods of Physical Tests for Hydraulic Cement, Part 6: Determination of Compressive Strength of Hydraulic Cement (Other than Masonry Cement),” Bureau of Indian Standards, New Delhi, India, 1988.
                    
                        11. IS 383-2016, “Coarse and Fine Aggregate for Concrete Specification (Third Revision),” Bureau of Indian Standards, New Delhi, India, 2016.
                    
                        12. Srinivasan, C.; Dattatreya, J. K.; Neelamegam, M.; and Harish, K. V., “Studies on Packing Density of Powder Mixtures and Cementitious Composites,” CSIR-SERC Report, RR/OLP-11841/3-May, 2006.
                    
                        13. IS 10078-1982, “Specification of Testing Jolting Apparatus for Cement,” Bureau of Indian Standards, New Delhi, India.
                    
                        14. Lavanya Prabha, S.; Dattatreya, J. K.; and Neelamegam, M., “Study on Stress-Strain Properties of Reactive Powder Cementitious Composites under Uniaxial Compression,” International Journal of Engineering Science and Technology, V. 2, No. 11, 2010, pp. 6407-6415.
                    
                        15. ASTM C78-18, “Standard Test Method for Flexural Strength of Concrete,” ASTM International, West Conshohocken, PA, 2018.
                    
                        16. EN 1992-1-1, “Eurocode 2: Design of Concrete Structures,” European Committee for Standardization, Brussels, Belgium, 2004.
                    
                        17. Zhang, J. J., and Bentley, L. R., “Factors Determining Poisson’s Ratio,” CREWES Research Report, V. 17, 2005.
                    
                        18. ASTM C1202-19, “Standard Test Method for Electrical Indication of Concrete’s Ability to Resist Chloride Ion Penetration,” ASTM International, West Conshohocken, PA, 2019.