Modeling Early-Age Rheology of Cement-Silica Fume Pastes

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Modeling Early-Age Rheology of Cement-Silica Fume Pastes

Author(s): Jedadiah F. Burroughs, Charles A. Weiss Jr., John E. Haddock, and W. Jason Weiss

Publication: Materials Journal

Volume: 117

Issue: 4

Appears on pages(s): 133-139

Keywords: absorbed moisture; cement paste; silica fume; specific surface; surface moisture; ultra-high-performance concrete; workability

DOI: 10.14359/51724626

Date: 7/1/2020

Abstract:
This study presents the application of an analytical model to describe the rheological behavior of cement pastes containing silica fume at replacement rates of up to 30% by mass. The analytical model hypothesizes how water interacts with particles in a cementitious system. The coating thickness of water surrounding each particle in the system is estimated. This coating thickness is shown to correlate strongly with measured rheological properties when fit to the Herschel-Bulkley model. To calculate coating thickness, it is necessary to account for the water absorbed by nonhydraulic components in the system, whether aggregate, supplementary cementitious materials, or mineral. The results suggest that silica fume particles may be absorptive, and this absorption capacity, although small, must be considered when designing water-starved cementitious materials. The experimental investigation involved the rheological testing of three water-binder ratios (0.20, 0.30, 0.45), three silica fume replacement levels (10%, 20%, 30%), and eight different silica fume products.

Related References:

1. Russell, H. G., and Graybeal, B. A., “Ultra-High-Performance Concrete: A State-of-the-Art Report for the Bridge Community,” Federal Highway Administration, McLean, VA, 2013.

2. Burroughs, J. F.; Rushing, T. S.; Scott, D. A.; and Williams, B. A., “Analyzing Effects of Varied Silica Fume Sources within Baseline UHPC,” Proceedings of the First International Interactive Symposium on UHPC, Des Moines, IA, 2016.

3. Ferraris, C. F., and de Larrard, F., “Modified Slump Test to Measure Rheological Parameters of Fresh Concrete,” Cement, Concrete and Aggregates, V. 20, No. 2, 1998, pp. 241-247. doi: 10.1520/CCA10417J

4. Nehdi, M., and Rahman, M.-A., “Estimating Rheological Properties of Cement Pastes Using Various Rheological Models for Different Test Geometry, Gap and Surface Friction,” Cement and Concrete Research, V. 34, No. 11, 2004, pp. 1993-2007. doi: 10.1016/j.cemconres.2004.02.020

5. ASTM C143/C143M-15a, “Standard Test Method for Slump of Hydraulic-Cement Concrete,” ASTM International, West Conshohocken, PA, 2015, 4 pp.

6. ASTM C939/C939M-16a, “Standard Test Method for Flow of Grout for Preplaced-Aggregate Concrete (Flow Cone Method),” ASTM International, West Conshohocken, PA, 2016, 3 pp.

7. ASTM C1437-15, “Standard Test Method for Flow of Hydraulic Cement Mortar,” ASTM International, West Conshohocken, PA, 2015, 2 pp.

8. Ferraris, C. F., “Measurement of Rheological Properties of Cement Paste: A New Approach,” Proceedings of Role of Admixtures in High Performance Concrete, RILEM International Symposium, Monterrey, Mexico, 1999.

9. Senff, L.; Hotza, D.; Repette, W.; Ferreira, V.; and Labrincha, J., “Rheological Characterisation of Cement Pastes with Nanosilica, Silica Fume and Superplasticizer Additions,” Advances in Applied Ceramics, V. 109, No. 4, 2010, pp. 213-218. doi: 10.1179/174367510X12663198542621

10. Mei, G.; Yang, H.; and Lu, C., “Coupled Effects of Silica Fume and Time after Water Addition on Rheology of Fresh Concrete,” Magazine of Concrete Research, V. 67, No. 14, 2015, pp. 762-770. doi: 10.1680/macr.14.00291

11. Vipulanandan, C., and Mohammed, A., “Hyperbolic Rheological Model with Shear Stress Limit for Acrylamide Polymer Modifed Bentonite Drilling Muds,” Journal of Petroleum Science Engineering, V. 122, 2014, pp. 38-47. doi: 10.1016/j.petrol.2014.08.004

12. Mohammed, A. S., “Vipulanandan Model for the Rheological Properties with Ultimate Shear Stress of Oil Well Cement Modified with Nanoclay,” Egyptian Journal of Petroleum, V. 27, No. 3, 2018, pp. 335-347. doi: 10.1016/j.ejpe.2017.05.007

13. Vikan, H.; Justnes, H.; Winnefeld, F.; and Figi, R., “Correlating Cement Characteristics with Rheology of Paste,” Cement and Concrete Research, V. 37, No. 11, 2007, pp. 1502-1511. doi: 10.1016/j.cemconres.2007.08.011

14. Kwan, A., and Wong, H., “Effects of Packing Density, Excess Water and Solid Surface Area on Flowability of Cement Paste,” Advances in Cement Research, V. 20, No. 1, 2008, pp. 1-11. doi: 10.1680/adcr.2008.20.1.1

15. Chen, J.; Fung, W.; and Kwan, A., “Effects of CSF on Strength, Rheology and Cohesiveness of Cement Paste,” Construction and Building Materials, V. 35, 2012, pp. 979-987. doi: 10.1016/j.conbuildmat.2012.04.037

16. Burroughs, J. F.; Weiss, J.; and Haddock, J. E., “Influence of High Volumes of Silica Fume on the Rheological Behavior of Oil Well Cement Pastes,” Construction and Building Materials, V. 203, 2019, pp. 401-407. doi: 10.1016/j.conbuildmat.2019.01.027

17. Lu, G.; Wang, K.; and Rudolphi, T. J., “Modeling Rheological Behavior of Highly Flowable Mortar Using Concepts of Particle and Fluid Mechanics,” Cement and Concrete Composites, V. 30, No. 1, 2008, pp. 1-12. doi: 10.1016/j.cemconcomp.2007.06.002

18. ASTM D854-14, “Standard Test Methods for Specific Gravity of Soil Solids by Water Pycnometer,” ASTM International, West Conshohocken, PA, 2014, 8 pp.

19. ASTM C1240-15, “Standard Specification for Silica Fume Used in Cementitious Mixtures,” ASTM International, West Conshohocken, PA, 2015, 7 pp.