Study on Assessment of Pozzolanic Activity: Slate Cutting Waste

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Study on Assessment of Pozzolanic Activity: Slate Cutting Waste

Author(s): S. C. L. Lima, L. C. B. Costa, K. C. S. Defáveri, J. M. Franco de Carvalho, R. A. F. Peixoto, and G. J. Brigolini

Publication: Materials Journal

Volume: 117

Issue: 3

Appears on pages(s): 3-10

Keywords: filler; pozzolan; slate cutting waste; strength activity index; supplementary cementitious material

DOI: 10.14359/51724611

Date: 5/1/2020

Abstract:
The mining industry is responsible for various environmental problems, including the extraction of natural resources and the generation of a significant volume of waste. The use of such residues in the construction industry as supplementary cementitious material (SCM) is one possible solution to minimize its disposal and a way for both industries to improve their eco-efficiency. This research aims to study the pozzolanic potential of the residue generated in slate cutting, as well as to compare the current standard methods applied to verify the pozzolanic activity (strength activity index) and direct methods based on calcium hydroxide consumption. A milling study in a planetary ball mill was carried out to evaluate the effects of particle size distribution on reactivity. The pozzolanic activity was investigated based on current standard methods (strength activity index) and analytical evaluations. The results of calcium hydroxide consumption were obtained from simultaneous thermal analysis (thermogravimetric and thermal differential analysis) and X-ray diffraction. Conflicting results between the current standard and direct methods were observed. The tested specimens with low or inexpressive calcium hydroxide consumption presented a high-strength activity index, while the specimens that presented a higher calcium hydroxide consumption showed a strength activity index below the minimum values required by the current standards. The results pointed to the potential use of slate cutting waste and contributes to the discussions about the phenomena neglected by the current strength activity index standard.

Related References:

1. Massazza, F., “Pozzolanic Cements,” Cement and Concrete Composites, V. 15, No. 4, 1993, pp. 185-214. doi: 10.1016/0958-9465(93)90023-3

2. Aprianti, E.; Shafigh, P.; Bahri, S.; and Farahani, J., “Supplementary Cementitious Materials Origin from Agricultural Wastes—A Review,” Construction and Building Materials, V. 74, 2015, pp. 176-187. doi: 10.1016/j.conbuildmat.2014.10.010

3. ASTM C595/C595M-17, “Standard Specification for Blended Hydraulic Cements,” ASTM International, West Conshohocken, PA, 2017, 8 pp

4. Damtoft, J.; Lukasik, J.; Herfort, D.; Sorrentino, D.; and Gartner, E., “Sustainable Development and Climate Change Initiatives,” Cement and Concrete Research, V. 38, No. 2, 2008, pp. 115-127. doi: 10.1016/j.cemconres.2007.09.008

5. Donatello, S.; Tyrer, M.; and Cheeseman, C., “Comparison of Test Methods to Assess Pozzolanic Activity,” Cement and Concrete Composites, V. 32, No. 2, 2010, pp. 121-127. doi: 10.1016/j.cemconcomp.2009.10.008

6. Frías, M.; Villar-Cocina, E.; Sanchez de Rojas, M.; and Valencia-Morales, E., “The Effect That Different Pozzolanic Activity Methods Has on the Kinetic Constants of the Pozzolanic Reaction in Sugar Cane Straw-Clay Ash/Lime Systems: Application of a Kinetic-Diffusive Model,” Cement and Concrete Research, V. 35, No. 11, 2005, pp. 2137-2142. doi: 10.1016/j.cemconres.2005.07.005

7. McCarter, W., and Tran, D., “Monitoring Pozzolanic Activity by Direct Activation with Calcium Hydroxide,” Construction and Building Materials, V. 31, 2001, pp. 41-49.

8. Payá, J.; Borrachero, M.; Monzo, J.; Peris-Mora, E.; and Amahjour, F., “Enhanced Conductivity Measurement Techniques for Evaluation of Fly Ash Pozzolanic Activity,” Cement and Concrete Research, V. 31, No. 1, 2001, pp. 41-49. doi: 10.1016/S0008-8846(00)00434-8

9. Mostafa, N., and Brown, P., “Heat of Hydration of High Reactive Pozzolans in Blended Cements: Isothermal Conduction Calorimetry,” Thermochimica Acta, V. 435, No. 2, 2005, pp. 162-167. doi: 10.1016/j.tca.2005.05.014

10. Detwiler, R., and Mehta, P., “Chemical and Physical Effects of Silica Fume on the Mechanical Behavior of Concrete,” ACI Materials Journal, V. 86, No. 6, Nov.-Dec. 1989, pp. 609-614.

11. Franco de Carvalho, J. M.; Melo, T. V.; Fontes, W. C.; Batista, J. O. S.; Brigolini, G. J.; and Peixoto, R. A. F., “More Eco-Efficient Concrete: An Approach on Optimization in the Production and Use of Waste-Based Supplementary Cementing Materials,” Construction and Building Materials, V. 206, 2019, pp. 397-409. doi: 10.1016/j.conbuildmat.2019.02.054

12. Rukzon, S., and Chindaprasirt, P., “Strength, Porosity, and Chloride Resistance of Mortar Using the Combination of Two Kinds of Pozzolanic Materials,” International Journal of Minerals Metallurgy and Materials, V. 20, No. 8, 2013, pp. 808-814. doi: 10.1007/s12613-013-0800-x

13. Kizhakkumodom Venkatanarayanan, H., and Rangaraju, P. R., “Effect of Grinding of Low-Carbon Rice Husk Ash on the Microstructure and Performance Properties of Blended Cement Concrete,” Cement and Concrete Composites, V. 55, 2015, pp. 348-363. doi: 10.1016/j.cemconcomp.2014.09.021

14. Berodier, E., and Scrivener, K., “Understanding the Filler Effect on the Nucleation and Growth of C-S-H,” Journal of the American Ceramic Society, V. 97, No. 12, 2014, pp. 3764-3773. doi: 10.1111/jace.13177

15. Gutteridge, W., and Dalziel, J., “Filler Cement: The Effect of the Secondary Component on the Hydration of Portland Cement,” Cement and Concrete Research, V. 20, No. 5, 1990, pp. 778-782. doi: 10.1016/0008-8846(90)90011-L

16. Oey, T.; Kumar, A.; Bullard, J.; Neithalath, N.; and Sant, G., “The Filler Effect: The Influence of Filler Content and Surface Area on Cementitious Reaction Rates,” Journal of the American Ceramic Society, V. 96, No. 6, 2013, pp. 1978-1990. doi: 10.1111/jace.12264

17. Mehta, P. K., and Monteiro, P. J. M., Concrete: Microstructure, Properties, and Materials, IBRACON, São Paulo, Brazil, 2008.

18. Cordeiro, G.; Toledo Filho, R.; Tavares, L.; and Fairbairn, E., “Pozzolanic Activity and Filler Effect of Sugarcane Bagasse Ash in Portland Cement and Lime Mortars,” Cement and Concrete Composites, V. 30, No. 5, 2008, pp. 410-418. doi: 10.1016/j.cemconcomp.2008.01.001

19. Cheerarot, R.; Tangpagasit, J.; and Jaturapitakkul, C., “Compressive Strength of Mortars Due to Pozzolanic Reaction of Fly Ash,” Eighth CANMET/ACI International Conference on Fly Ash, Silica Fume, Slag and Natural Pozzolans in Concrete, SP-221, American Concrete Institute, Farmington Hills, MI, 2004, pp. 411-426.

20. Jaturapitakkul, C.; Tangpagasit, J.; Songmue, S.; and Kiattikomol, K., “Filler Effect of Fine Particle Sand on the Compressive Strength of Mortar,” International Journal of Minerals Metallurgy and Materials, V. 18, No. 2, 2011, pp. 240-246. doi: 10.1007/s12613-011-0429-6

21. Khan, M.; Jamil, M.; Karim, M.; Zain, M.; and Kaish, A., “Filler Effect of Pozzolanic Materials on the Strength and Microstructure Development of Mortar,” KSCE Journal of Civil Engineering, V. 21, No. 1, 2017, pp. 274-284. doi: 10.1007/s12205-016-0737-5

22. Cerulli, T.; Pistolesi, C.; Maltese, C.; and Salvioni, D., “Durability of Traditional Plaster with Respect to Blast Furnace Slag-Based Plaster,” Cement and Concrete Research, V. 33, No. 9, 2003, pp. 1375-1383. doi: 10.1016/S0008-8846(03)00072-3

23. Li, G., and Wu, X., “Influence of Fly Ash and Its Mean Particle Size on Certain Engineering Properties of Cement Composite Mortars,” Cement and Concrete Research, V. 35, No. 6, 2005, pp. 1128-1134. doi: 10.1016/j.cemconres.2004.08.014

24. Silva, K.; Cordeiro, G.; Natalli, J.; Mendes, J.; Silva, G.; and Peixoto, R., “Rock Wool Waste as Supplementary Cementing Materials for Portland Cement-Based Composites,” ACI Materials Journal, V. 115, No. 5, Sept. 2018, pp. 653-661.

25. Papadakis, V., and Tsimas, S., “Supplementary Cementing Materials in Concrete Part I: Efficiency and Design,” Cement and Concrete Research, V. 32, No. 10, 2002, pp. 1525-1532. doi: 10.1016/S0008-8846(02)00827-X

26. Ihask, S., and Hashim, H., “Low Carbon Measures for Measures for Cement Plant - A Review,” Journal of Cleaner Production, V. 105, 2015, pp. 260-274.

27. Miller, S., “Supplementary Cementitious Materials to Mitigate Greenhouse Gas Emissions from Concrete: Can There Be Too Much of a Good Thing?,” Journal of Cleaner Production, V. 178, 2018, pp. 587-598. doi: 10.1016/j.jclepro.2018.01.008

28. Rodrigues, W.; Guimaraes, C.; and Silva, M., “Study of the Technical and Economic Feasibility of the Use of Slate Industrial Waste in Asphalt Mixture of the Pre-Mixed Cold Type,” Military Journal of Science and Technology, V. 31, 2014, pp. 34-50.

29. Oti, J.; Kinuthia, J.; Snelson, D.; and Bai, J., “Applications of Slate Waste Material in the UK,” Waste and Resource Management, V. 163, 2010, pp. 9-15.

30. Barluenga, G., and Hernández-Olivares, F., “Self-Levelling Cement Mortar Containing Grounded Slate from Quarrying Waste,” Construction and Building Materials, V. 24, No. 9, 2010, pp. 1601-1607. doi: 10.1016/j.conbuildmat.2010.02.033

31. Frias, M.; Villas, R.; Garcia, R.; Soto, I.; Medina, C.; and Rojas, M., “Scientific and Technical Aspects of Blended Cement Matrices Containing Activated Slate Wastes,” Cement and Concrete Composites, V. 48, 2014, pp. 19-25. doi: 10.1016/j.cemconcomp.2014.01.002

32. Frias, M.; Vigil de la Villa, R.; Garcia, R.; Sánchez de Rojas, M.; and Juan Valdés, A., “The Influence of Slate Waste Activation Conditions on Mineralogical Changes and Pozzolanic Behavior,” Journal of the American Ceramic Society, V. 96, No. 7, 2013, pp. 2276-2282. doi: 10.1111/jace.12387

33. ABNT, “NBR 5733 - High Early Strength Portland Cement - Specification,” Brazilian Association of Technical Standards - ABNT, Rio de Janeiro, Brazil, 1991.

34. Rietveld, H., “Profile Refinement Method for Nuclear and Magnetic Structure,” Journal of Applied Crystallography, V. 2, No. 2, 1969, pp. 65-71. doi: 10.1107/S0021889869006558

35. Scrivener, K.; Snellings, R.; and Lothenbach, B., A Practical Guide to Microstructural Analysis of Cementitious Materials, CRC Press, Boca Raton, FL, 2016.

36. ASTM C311/C311M-17, “Standard Test Methods for Sampling and Testing Fly Ash or Natural Pozzolans for Use in Portland-Cement Concrete,” ASTM International, West Conshohocken, PA, 2017.

37. ASTM C230/C230M-14, “Standard Specification for Flow Table for Use in Tests of Hydraulic Cement,” ASTM International, West Conshohocken, PA, 2014, 6 pp.

38. El-Jazairi, B., and Illston, J., “The Hydration of Cement Paste Using the Semi-Isothermal Method of Derivative Thermogravimetry,” Cement and Concrete Research, V. 10, 2010, pp. 487-493.

39. ASTM C618-17a, “Standard Specification for Coal Fly Ash and Raw or Calcined Natural Pozzolan for Use in Concrete,” ASTM International, West Conshohocken, PA, 2017, 5 pp.

40. Juenger, M., and Siddique, R., “Recent Advances in Understanding the Role of Supplementary Cementitious Materials in Concrete,” Cement and Concrete Research, V. 78, 2015, pp. 71-80. doi: 10.1016/j.cemconres.2015.03.018

41. Palaniandy, S.; Azizli, K.; Hussin, H.; and Hashim, S., “Study on Mechanochemical Effect of Silica for Short Grinding Period,” International Journal of Mineral Processing, V. 82, No. 4, 2007, pp. 195-202. doi: 10.1016/j.minpro.2006.10.008

42. de F. Souza, L. P., and Mansur, H. S., “Production and Characterization of Ceramic Pieces Obtained by Slip Casting Using Powder Wastes,” Journal of Materials Processing Technology, V. 145, 2004, pp. 14-20. doi: 10.1016/S0924-0136(03)00857-4

43. Bakolas, A.; Aggelakopoulou, E.; Moropoulou, A.; and Anagnostopoulou, A., “Evaluation of Pozzolanic Activity and Physic-Mechanical Characteristics in Metakaolin-Lime Pastes,” Journal of Thermal Analysis and Calorimetry, V. 84, No. 1, 2006, pp. 157-163. doi: 10.1007/s10973-005-7262-y

44. Lim, S., and Mondal, P., “Efffects of Nanosilica Addition on Increased Thermal Stability of Cement-Based Composite,” ACI Materials Journal, V. 112, No. 2, Mar.-Apr. 2015, pp. 305-315. doi: 10.14359/51687177

45. Kaminskas, R.; Cesnauskas, V.; and Kubiliute, R., “Influence of Different Artificial Additives on Portland Cement Hydration and Hardening,” Construction and Building Materials, V. 95, No. 1, 2015, pp. 537-544. doi: 10.1016/j.conbuildmat.2015.07.113

46. Mitrović, A., and Zdujić, M., “Preparation of Pozzolanic Addition by Mechanical Treatment of Kaolin Clay,” International Journal of Mineral Processing, V. 132, 2014, pp. 59-66. doi: 10.1016/j.minpro.2014.09.004

47. Souri, A.; Kazemi-Kamyab, H.; Snellings, R.; Naghizadeh, R.; Golestani-Fard, F.; and Scrivener, K., “Pozzolanic Activity of Mechanochemically and Thermally Activated Kaolin in Cement,” Cement and Concrete Research, V. 77, Nov. 2015, pp. 47-59.

48. Burris, L. E., and Juenger, M. C., “Milling as a Pretreatment Method for Increasing the Reactivity of Natural Zeolites for Use as Supplementary Cementitious Materials,” Cement and Concrete Composites, V. 65, 2016, pp. 163-170. doi: 10.1016/j.cemconcomp.2015.09.008

49. Cordeiro, G. C.; Tavares, L.; and Toledo Filho, R. D., “Improved Pozzolanic Activity of Sugar Cane Bagasse Ash by Selective Grinding and Classification,” Cement and Concrete Research, V. 89, 2016, pp. 269-275. doi: 10.1016/j.cemconres.2016.08.020

50. Choudhary, A.; Shah, V.; and Bishnoi, S., “Effect of Low Cost Fillers on Cement Hydration,” Construction and Building Materials, V. 124, 2016, pp. 533-543. doi: 10.1016/j.conbuildmat.2016.07.088

51. Frías, M., and Cabrera, J., “Pore Size Distribution and Degree of Hydration of Metakaolin-Cement Pastes,” Cement and Concrete Research, V. 30, No. 4, 2000, pp. 561-569. doi: 10.1016/S0008-8846(00)00203-9


ALSO AVAILABLE IN:

Electronic Materials Journal