Time-Dependent Shear Strength Behavior of Superfıne Cement-Stabilized Clayey Soil

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Time-Dependent Shear Strength Behavior of Superfıne Cement-Stabilized Clayey Soil

Author(s): Murat Mollamahmutoglu and Eyubhan Avcı

Publication: Materials Journal

Volume: 117

Issue: 2

Appears on pages(s): 251-258

Keywords: clayey soil; shear strength; stabilization; superfine cement

DOI: 10.14359/51722403

Date: 3/1/2020

Abstract:
In this study, the goal was to investigate the shear strength properties of superfine cement (SC) stabilized clayey soil (CS). In this regard, standard compaction tests were run on the clayey soil specimens stabilized with 8, 10, and 12% SC to determine their optimum moisture contents and the maximum dry densities. Thereafter, unconsolidated undrained (UU) triaxial tests were conducted on them to find out their shear strength parameters and stress-strain characteristics at different time intervals under wet-cured and air-dried conditions. The shear strength parameters—namely the cohesion intercept and the internal friction angle of CS—increased with the stabilization of SC under both curing conditions. Additionally, the shear strength parameters of SC-stabilized CS were increased more with the increase of SC content and time under both curing conditions. The internal friction angles of air-dried specimens were higher than those of wet-cured specimens. On the other hand, the cohesion intercepts of wet-cured specimens were greater than those of air-dried specimens. The stress-strain behavior of CS was also influenced with the stabilization of SC such that as the stresses of CS were increased with the increase of SC content and time their strains decreased and they experienced brittle failures under both wet-cured and air-dried conditions.

Related References:

1. Cong, M.; Longzhu, C.; and Bing, C., “Analysis of Strength Development in Soft Clay Stabilized with Cement-Based Stabilizer,” Construction and Building Materials, V. 71, Nov, 2014, pp. 354-362. doi: 10.1016/j.conbuildmat.2014.08.087

2. Jahandari, S.; Li, S.; Saberian, M.; and Shahsavarigoughari, M., “Experimental Study of the Effects of Geogrids on Elasticity Modulus, Brittleness, Strength, and Stress-Strain Behavior of Lime Stabilized Kaolinitic clay,” GeoResJ, V. 13, June, 2017, pp. 49-58. doi: 10.1016/j.grj.2017.02.001

3. Prusinski, J., and Bhattacharja, S., “Effectiveness of Portland Cement and Lime in Stabilizing Clay Soils,” Transportation Research Record: Journal of the Transportation Research Board, V. 1652, No. 1, 1999, pp. 215-227. doi: 10.3141/1652-28

4. Bergado, D. T.; Anderson, L. R.; Miura, N.; and Balasubramaniam, A. S., Soft Ground Improvement in Lowland and Other Environments, ASCE Press, New York, 1996, 427 pp.

5. Chew, S. H.; Kamruzzaman, A. H. M.; and Lee, F. H., “Physicochemical and Engineering Behavior of Cement Treated Clays,” Journal of Geotechnical and Geoenvironmental Engineering, ASCE, V. 130, No. 7, 2004, pp. 696-706. doi: 10.1061/(ASCE)1090-0241(2004)130:7(696)

6. Sasanian, S., and Newson, T. A., “Basic Parameters Governing the Behavior of Cement-Treated Clays,” Soil and Foundation, V. 54, No. 2, 2014, pp. 209-224. doi: 10.1016/j.sandf.2014.02.011

7. Zhang, T.; Yue, X.; Deng, Y.; Zhang, D.; and Liu, S., “Mechanical Behaviour and Microstructure of Cement-Stabilized Marine Clay with a Metakaolin Agent,” Construction and Building Materials, V. 73, Oct, 2014, pp. 51-57. doi: 10.1016/j.conbuildmat.2014.09.041

8. Wong, L. S.; Mousavi, S.; Sobhani, S.; Kong, S. Y.; Birima, A. H.; and Mohd Pauzi, N. I., “Comparative Measurement of Compaction Impact of Clay Stabilized with Cement, Peat Ash and Silica Sand,” Measurement, V. 94, Dec, 2016, pp. 498-504. doi: 10.1016/j.measurement.2016.08.029

9. Mollamahmutoğlu, M., and Avcı, E., “Cement Type Effect on Improvement of Clayey Soil Properties,” ACI Materials Journal, V. 115, No. 6, Nov. 2018, pp. 855-866. doi: 10.14359/51702347

10. Chew, S. H.; Lee, F. H.; and Lee, Y., “Jet Grouting in Singapore Marine Clay,” Proceedings of the 3rd Asian Young Geotechnology Engineering Conference, Singapore, 1997, pp. 231-238.

11. Miura, N.; Horpibulsuk, S.; and Nagaraj, T. S., “Engineering Behavior of Cement Stabilized Clay at High Water Content,” Soil and Foundation, V. 41, No. 5, 2001, pp. 33-45. doi: 10.3208/sandf.41.5_33

12. Cokça, E., “Use of Class C Fly Ashes for the Stabilization of an Expansive Soil,” Journal of Geotechnical and Geoenvironmental Engineering, ASCE, V. 127, No. 7, 2001, pp. 568-573. doi: 10.1061/(ASCE)1090-0241(2001)127:7(568)

13. Nagaraj, T. S.; Miura, N.; Yamadera, A.; and Yaligar, P., “Strength Assessment of Cement Admixtures Soft Clays—Parametric Study,” Proceedings of the International Conference on Ground Improvement Techniques, Macau, 1997, pp. 379-386.

14. Mitchell, J. K., “Soil Improvement State of the Art Report,” Proceedings of the 10th International Conference on Soil Mechanics and Foundation Engineering, Stockholm, Sweden, 1981, pp. 509-565.

15. Tremblay, H.; Leroueil, S.; and Locat, J., “Mechanical Improvement and Vertical Yield Stress Prediction of Clayey Soils from Eastern Canada Treated with Lime or Cement,” Canadian Geotechnical Journal, V. 38, No. 3, 2001, pp. 567-579. doi: 10.1139/t00-119

16. Sarkar, G.; Islam, M. R.; Alamgir, M.; and Rokonuzzaman, M., “Study on the Geotechnical Properties of Cement-Based Composite Fine-grained Soil,” International Journal of Advanced Structures and Geotechnical Engineering, V. 1, No. 2, 2012, pp. 42-49.

17. Bell, F. G., Engineering Treatment of Soils, Chapman & Hall, London, UK, 1993, 316 pp.

18. ASTM D422-63(2002), “Standard Test Method for Particle-Size Analysis of Soils,” ASTM International, West Conshohocken, PA, 2002, 8 pp.

19. ASTM D4318-10e1, “Standard Test Methods for Liquid Limit, Plastic Limit, and Plasticity Index of Soils,” ASTM International, West Conshohocken, PA, 2010, 16 pp.

20. ASTM D854-02, “Standard Test Method for Specific Gravity of Soil Solids by Water Pycnometer,” ASTM International, West Conshohocken, PA, 2002, 7 pp.

21. ASTM D2487-00, “Standard Practice for Classification of Soils for Engineering Purposes (Unified Soil Classification System),” ASTM International, West Conshohocken, PA, 2000, 12 pp.

22. Das, B. M., and Sivakugan, N., Fundamentals of Geotechnical Engineering, Cengage Learning, Boston, MA, 2015, 315 pp.

23. ASTM D698-00a, “Standard Test Methods for Laboratory Compaction Characteristics of Soil Using Standard Effort (12,400 ft-lbf/ft3 (600 kN-m/m3)),” ASTM International, West Conshohocken, PA, 2000, 13 pp.

24. ASTM D2850-15, “Standard Test Method for Unconsolidated-Undrained Triaxial Compression Test on Cohesive Soils,” ASTM International, West Conshohocken, PA, 2015, 7 pp.

25. Locat, J.; Trembaly, H.; and Leroueil, S., “Mechanical and Hydraulic Behaviour of a Soft Inorganic Clay Treated with Lime,” Canadian Geotechnical Journal, V. 33, No. 4, 1996, pp. 654-669. doi: 10.1139/t96-090-311

26. Horpibulsuk, S.; Suddeepong, A.; Chinkulkijniwat, A.; and Liu, M. D., “Strength and Compressibility of Lightweight Cemented Clays,” Applied Clay Science, V. 69, Nov. 2012, pp. 11-21. doi: 10.1016/j.clay.2012.08.006

27. Richardson, D. N., “AASHTO Layer Coefficients for Cement-Stabilized Soil Bases,” Journal of Materials in Civil Engineering, ASCE, V. 8, No. 2, 1996, pp. 83-87. doi: 10.1061 (ASCE)0899-1561(1996)8:2(83)

28. Bhattacharja, S., and Bhatty, J., “Comparative Performance of Portland Cement and Lime in Stabilization of Moderate to High Plasticity Clay Soils,” PCA RD125, Portland Cement Association, Skokie, IL, 2003, pp. 1-21.

29. Lorenzo, G. A., and Bergado, D. T., “Fundamental Characteristics of Cement Admixed Clay in Deep Mixing,” Journal of Materials in Civil Engineering, ASCE, V. 18, No. 2, 2006, pp. 161-174. doi: 10.1061/(ASCE)0899-1561(2006)18:2(161)


ALSO AVAILABLE IN:

Electronic Materials Journal