Micromechanical Properties of Self-Healing Concrete with Crystalline Admixture and Silica Fume

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Micromechanical Properties of Self-Healing Concrete with Crystalline Admixture and Silica Fume

Author(s): T. Chandra Sekhara Reddy, A. Ravitheja, and C. Sashidhar

Publication: Materials Journal

Volume: 117

Issue: 3

Appears on pages(s): 63-74

Keywords: calcium carbonate (CaCO3); crystalline admixtures; durability properties; Fourier-transform infrared spectroscopy (FTIR); mechanical properties; pH; scanning electron microscopy with energy dispersive X-ray spectroscopy (SEM-EDS); self-healing; silica fu

DOI: 10.14359/51722395

Date: 3/1/2020

Abstract:
The study aimed at examining the capacity of diverse add-ons in improving the self-healing ability of fiber-reinforced concrete through low water-cement ratios (w/c) and exposure to wide cracks. The self-healing capacities of crystalline admixture (CA) and silica fume (SF) were assessed by mechanical and durability performance. The effect of various exposure periods (7 to 42 days) in four different exposure conditions—namely, water immersion, wetting-and-drying cycles, water contact, and air exposure (AE)—on self-healing was evaluated by application of through-crack compressive stress. Compressive strength and durability analysis showed that CA with 10% SF was excellent in all four environments. Fourier transform infrared spectroscopy and scanning electron microscope results showed significant bond formation contributing to the self-healing property of the CAs. Therefore, concrete mixture with CA and 10% SF is recommended for use to increase the self-healing of concrete.

Related References:

1. Choi, H.; Inoue, M.; Kwon, S.; Choi, H.; and Lim, M., “Effective Crack Control of Concrete by Self-Healing of Cementitious Composites Using Synthetic Fiber,” Materials, V. 9, No. 4, 2016, 248 pp. doi: 10.3390/ma9040248

2. Jiang, Z.; Li, W.; Yuan, Z.; and Yang, Z., “Self-Healing of Cracks in Concrete with Various Crystalline Mineral Additives in Underground Environment,” Journal of Wuhan University of Technology-Materials Science, V. 29, No. 5, Oct. 2014, pp. 938-944. doi: 10.1007/s11595-014-1024-2

3. Nishiwaki, T.; Kwon, S.; Homma, D.; Yamada, M.; and Mihashi, H., “Self-Healing Capability of Fiber-Reinforced Cementitious Composites for Recovery of Watertightness and Mechanical Properties,” Materials (Basel), V. 7, No. 3, 2014, pp. 2141-2154. doi: 10.3390/ma7032141

4. van der Zwaag, S.; Alexander, J.; Schmets, M.; and van der Zaken., G., “Self-Healing Materials,” Springer, Dordrecht, the Netherlands, 2007.

5. Orosz, K., “Early Age Autogenous Deformation and Cracking of Cementitious Materials—Implications on Strengthening of Concrete Structures,” PhD thesis, Luleå University of Technology, Luleå, Sweden, 2017.

6. Alhhalabi, Z. S., and Dopuga, D., “Self-Healing Concrete: Definition, Mechanism and Application in Different Types of Structures,” International Research Journal, V. 59, No. 5, May 2017, pp. 55-57. doi: 10.23670/IRJ.2017.59.087

7. Van Tittelboom, K., and De Belie, N., “Self-Healing in Cementitious Materials—A Review,” Materials (Basel), V. 6, No. 6, 2013, pp. 2182-2217. doi: 10.3390/ma6062182

8. Ravitheja, A.; Reddy, T. C. S.; and Sashidhar, C., “Self-Healing Concrete with Crystalline Admixture—A Review,” Journal of Wuhan University of Technology-Materials Science, V. 34, No. 5, Oct. 2019, pp. 1143-1154. doi: 10.1007/s11595-019-2171-2

9. Meharie, M. G.; Kaluli, J. W.; Abiero-Gariy, Z.; and Kumar, N. D., “Factors Affecting the Self-Healing Efficiency of Cracked Concrete Structures,” American Journal of Applied Scientific Research, V. 3, No. 6, Nov. 2017, pp. 80-86. doi: 10.11648/j.ajasr.20170306.12

10. Huang, H.; Ye, G.; Qian, C.; and Schlangen, E., “Self-Healing in Cementitious Materials: Materials, Methods and Service Conditions,” Materials and Design, V. 92, Feb. 2016, pp. 499-511. doi: 10.1016/j.matdes.2015.12.091

11. Keppert, M.; Urbanová, M.; Brus, J.; Čáchová, M.; Fořt, J.; Trník, A.; Scheinherrová, L.; Záleská, M.; and Černý, R., “Rational Design of Cement Composites Containing Pozzolanic Additions,” Construction and Building Materials, V. 148, Sept. 2017, pp. 411-418. doi: 10.1016/j.conbuildmat.2017.05.032

12. Lothenbach, B.; Scrivener, K.; and Hooton, R., “Supplementary Cementitious Materials,” Cement and Concrete Research, V. 41, No. 12, 2011, pp. 1244-1256. doi: 10.1016/j.cemconres.2010.12.001

13. Yang, K. H.; Jung, Y. B.; Cho, M. S.; and Tae, S. H., “Effect of Supplementary Cementitious Materials on Reduction of CO2 Emissions from Concrete,” Journal of Cleaner Production, V. 103, Sept. 2015, pp. 774-783. doi: 10.1016/j.jclepro.2014.03.018

14. Reddy, T. C. S., and Ravitheja, A., “Macro Mechanical Properties of Self-Healing Concrete with Crystalline Admixture under Different Environments,” Ain Shams Engineering Journal, V. 10, No. 1, 2019, pp. 23-32. doi: 10.1016/j.asej.2018.01.005

15. Reddy, T. C. S.; Theja, A. R.; and Sashidhar, C., “Self-Healing Ability of High-Strength Fibre-Reinforced Concrete with Fly Ash and Crystalline Admixture,” Civil Engineering Journal, V. 4, No. 5, 2018, pp. 971-979. doi: 10.28991/cej-0309149

16. Wang, Y.; Pham, D. T.; and Ji, C., “Self-Healing Composites: A Review,” Cogent Engineering, V. 2, No. 1, 2015, pp. 1-28. doi: 10.1080/23311916.2015.1075686

17. Pacheco-Torgal, F.; Barroso de Aguiar, J.; Ding, Y.; Tahri, W.; and Baklouti, S., “Performance of Alkali-Activated Mortars for the Repair and Strengthening of OPC Concrete,” Handbook of Alkali-Activated Cements, Mortars and Concretes, Elsevier, 2015, pp. 627-641. doi: 10.1533/9781782422884.4.627

18. Fang, Y.; Liu, J.; and Chen, Y.; “Effect of Magnesia on Properties and Microstructure of Alkali-Activated Slag Cement,” Water Science and Engineering journal, V. 4, No. 4, Dec. 2011, pp. 463-469. doi: 10.3882/j.issn.1674-2370.2011.04.010

19. Ferrara, L.; Krelani, V.; and Moretti, F., “On the Use of Crystalline Admixtures in Cement-Based Construction Materials: From Porosity Reducers to Promoters of Self Healing,” Smart Materials and Structures, V. 28, No. 8, July 2016, pp. 1-17. doi: 10.1088/0964-1726/25/8/084002

20. Qureshi, T. S., and Al-Tabbaa, A., “Self-Healing of Drying Shrinkage Cracks in Cement-Based Materials Incorporating Reactive MgO,” Smart Materials and Structures, V. 25, 2016, pp 1-16. doi: 10.1088/0964-1726/25/8/084004

21. ASTM C1202-17a, “Standard Test Method for Electrical Indication of Concrete’s Ability to Resist Chloride Ion Penetration,” ASTM International, West Conshohocken, PA, 2017, 8 pp. doi: 10.1520/C1202-17A

22. ASTM C642-13, “Standard Test Method for Density, Absorption, and Voids in Hardened Concrete,” ASTM International, West Conshohocken, PA, 2013, 3 pp. doi: 10.1520/C0642-1310.1520/C0642-13

23. ASTM C596-09, “Standard Test Method for Drying Shrinkage of Mortar Containing Hydraulic Cement,” ASTM International, West Conshohocken, PA, 2017, 4 pp. doi: 10.1520/C0596-09R17

24. Kim, H.; Liu, Z.; Cong, W.; and Zhang, H. C., “Tensile Fracture Behavior and Failure Mechanism of Additively-Manufactured AISI 4140 Low Alloy Steel by Laser Engineered Net Shaping,” Materials (Basel), V. 10, No. 11, 2017, 1283 pp. doi: 10.3390/ma10111283

25. García-Lodeiro, I.; Macphee, D.; Palomo, A.; and Fernández-Jiménez, A., “Effect of Alkalis on Fresh C–S–H Gels. FTIR Analysis,” Cement and Concrete Research, V. 39, Jan. 2009, pp. 147-153. doi: 10.1016/j.cemconres.2009.01.003.

26. Nagaraj, H. B.; Sravan, M. V.; Arun, T. G.; and Jagadish, K. S., “Role of Lime with Cement in Long-Term Strength of Compressed Stabilized Earth Blocks,” International Journal of Sustainable Built Environment, V. 3, No. 1, 2014, pp. 54-61. doi: 10.1016/j.ijsbe.2014.03.001

27. Supe, J., and Gupta, M., “Role of Heat of Hydration in Attaining Early Strength Gain of Cement in Concrete,” International Journal of Pure and Applied Sciences and Technology, V. 3, No. 2, Oct. 2014, pp. 94-106.

28. Ghosh, S., and Handoo, S., “Infrared and Raman Spectral Studies in Cement and Concrete (review),” Cement and Concrete Research, V .10, No. 6, Nov. 1980, pp. 771-782. doi: 10.1016/0008-8846(80)90005-8

29. Huang, H., and Ye, G., “Self-Healing of Cracks in Cement Paste Affected by Additional Ca 2+ ions in the Healing Agent,” Journal of Intelligent Material Systems and Structures, V. 26, No. 3, 2015, pp .309-320. doi: 10.1177/1045389X14525490

30. Yu, P.; Kirkpatrick, R. J.; Poe, B.; McMillan, P.F.; and Cong, X., “Structure of Calcium Silicate Hydrate (C-S-H): Near-, Mid-, and Far-Infrared Spectroscopy,” Journal of the American Ceramic Society, V. 82, No. 3, Mar. 1999, pp 742-748. doi: 10.1111/j.1151-2916.1999.tb01826.x

31. Tambelli, C. E.; Schneider, J. F.; Hasparyk, N. P.; and Monteiro, P. J. M., “Study of the Structure of Alkali-Silica Reaction Gel by High-Resolution NMR Spectroscopy,” Journal of Non-Crystalline Solids, V. 352, No. 32-35, 2006, pp. 3429-3436. doi: 10.1016/j.jnoncrysol.2006.03.112

32. Sharma, T. K.; Alazhari, M.; Heath, A.; Paine, K.; and Cooper, R., “Alkaliphilic Bacillus Species Show Potential Application in Concrete Crack Repair by Virtue of Rapid Spore Production and Germination then Extracellular Calcite Formation,” Journal of Applied Microbiology, V. 122, No. 5, May 2017, pp. 1233-1244. doi: 10.1111/jam

33. Björnström, J.; Martinelli, A.; Matic, A.; Börjesson, L.; and Panas, I., “Accelerating Effects of Colloidal Nano-Silica for Beneficial Calcium-Silicate-Hydrate Formation in Cement,” Chemical Physics Letters, V. 392, No. 1-3, 2004, pp. 242-248. doi: 10.1016/j.cplett.2004.05.071

34. ASTM C348-08, “Standard Test Method for Flexural Strength of Hydraulic-Cement Mortars,” ASTM International, West Conshohocken, PA, 2008, 6 pp. doi: 10.1520/C0348-08

35. Varas, M. J.; Alvarez de Buergo, M.; and Fort, R., “Natural Cement as the Precursor of Portland Cement: Methodology for its Identification,” Cement and Concrete Research, V. 35, No. 11, 2005, pp. 2055-2065. doi: 10.1016/j.cemconres.2004.10.045

36. Fernández-Carrasco, L., and Vázquez, E., “Reactions of Fly Ash with Calcium Aluminate Cement and Calcium Sulphate,” Fuel, V. 88, No. 9, 2009, pp. 1533-1538. doi: 10.1016/j.fuel.2009.02.018

37. Parande, A. K.; Babu, B. R.; Pandi, K.; Karthikeyan, M. S.; and Palaniswamy, N., “Environmental Effects on Concrete Using Ordinary and Pozzolana Portland Cement,” Construction and Building Materials, V. 25, No. 1, 2011, pp. 288-297. doi: 10.1016/j.conbuildmat.2010.06.027


ALSO AVAILABLE IN:

Electronic Materials Journal