Utilization of Reclaimed Asphalt Pavement Aggregates in Portland Cement Concrete for Concrete Pavement

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Utilization of Reclaimed Asphalt Pavement Aggregates in Portland Cement Concrete for Concrete Pavement

Author(s): Anol Mukhopadhyay and Xijun Shi

Publication: Symposium Paper

Volume: 334

Issue:

Appears on pages(s): 13-32

Keywords: reclaimed asphalt pavement, portland cement concrete, microstructure, durability, life cycle assessment

DOI: 10.14359/51720251

Date: 9/30/2019

Abstract:
Potential issues associated with depletion of good aggregate sources and management of excess RAP stockpiles increasingly motivate use of RAP in PCC as a coarse aggregate replacement. Texas has shown great interest in disposing excess RAP stockpiles and a systematic study on using RAP in PCC for Texas pavement applications was conducted by the authors recently. This paper provides a concise summary of the findings from this study. The major conclusions are (1) PCC mixture with dense aggregate gradation can be achieved by adding coarse RAP with adequate intermediate sized particles, which offers better overall performance in terms of workability and mechanical properties, (2) RAP-PCC with coarse RAP replacement up to 40% showed considerable reduction for modulus of rupture. Asphalt cohesive failure (crack passing through the asphalt layer) was found to be the main mechanism responsible for the strength reductions, (3) the addition of allowable amounts of RAP into PCC provides equivalent durability performance relative to plain PCC, and (4) constructing pavements with RAP-PCC yields economic, environmental and social benefits.