Effect of Particle Size Distribution of Sand on Mechanical Properties of Cement Mortar Modified with Microsilica

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Effect of Particle Size Distribution of Sand on Mechanical Properties of Cement Mortar Modified with Microsilica

Author(s): Kawan Ghafor, Wael Mahmood, Warzer Qadir, and Ahmed Mohammed

Publication: Materials Journal

Volume: 117

Issue: 1

Appears on pages(s): 47-60

Keywords: curing time; microsilica; modeling; statistical analysis; strengths; water-cement ratio (w/c)

DOI: 10.14359/51719070

Date: 1/1/2020

Abstract:
Despite the many research studies on the effect of the particle size distribution (PSD) of sand and microsilica content on the mechanical properties of cement mortar, there has not been a comprehensive study investigating the effect of the PSD curve corresponding to 10% of fines, microsilica content, curing time, and watercement ratio (w/c) on the compressive, tensile, and flexural strengths of cement mortar. Therefore, this study investigates the subject, which could be beneficial for geotechnical, building, and construction fields. In this study, more than 1000 data on the mechanical properties of the cement mortar modified with different percentages of microsilica, varied from 5 to 55% (by dry weight of the cement), were collected from the literature. The statistical analysis, modeling, and nonlinear regression analysis were performed on the collected data. The w/c ranged between 0.2 and 0.8. The Vipulanandan p-q Model was used and compared to the Logistic Growth Model to predict the PSD of sands used in cement mortar. The Vipulanandan Correlation Model was also used and compared with the Hoek-Brown Model to correlate the mechanical properties of cement mortar modified with microsilica. The Vipulanandan Correlation Model has a lower root mean square error (RMSE) compared to the Hoek-Brown Model. The results of the present study showed that there is a good relationship between the compressive strength with flexural strength and tensile strength for cement mortar modified with microsilica. Based on the coefficient of determination (R2) and RMSE, the compressive strength, flexural strength, and tensile strength of cement mortar quantified well as a function of w/c, the microsilica content (MS %), curing time, and effective diameter d10 using nonlinear relationship.

Related References:

Aköz, F.; Türker, F.; Koral, S.; and Yüzer, N., 1999, “Effects of Raised Temperature of Sulfate Solutions on the Sulfate Resistance of Mortars with and without Silica Fume,” Cement and Concrete Research, V. 29, No. 4, pp. 537-544. doi: 10.1016/S0008-8846(98)00251-8

Al-Khalaf, M. N., and Yousif, H. A., 1984, “Use of Rice Husk Ash in Concrete,” International Journal of Cement Composites and Lightweight Concrete, V. 6, No. 4, pp. 241-248. doi: 10.1016/0262-5075(84)90019-8

Almeida, A. E. D. S., and Sichieri, E. P., 2007, “Experimental Study on Polymer-Modified Mortars with Silica Fume Applied to Fix Porcelain Tile,” Building and Environment, V. 42, No. 7, pp. 2645-2650. doi: 10.1016/j.buildenv.2006.07.002

Alwash, J. J. H., 2013, “Use of Rice Husk Ash in Cement Mortar,” Journal of University of Babylon, V. 21, No. 2, pp. 582-590.

Biricik, H., and Sarier, N., 2014, “Comparative Study of the Characteristics of Nano Silica-, Silica Fume- and Fly Ash-Incorporated Cement Mortars,” Materials Research, V. 17, No. 3, pp. 570-582. doi: 10.1590/S1516-14392014005000054

Çakır, Ö., and Sofyanlı, Ö. Ö., 2015, “Influence of Silica Fume on Mechanical and Physical Properties of Recycled Aggregate Concrete,” HBRC Journal, V. 11, No. 2, pp. 157-166. doi: 10.1016/j.hbrcj.2014.06.002

Cong, X.; Gong, S.; Darwin, D.; and McCabe, S. L., 1990, “Role of Silica Fume in Compressive Strength of Cement Paste, Mortar, and Concrete,” University of Kansas Center for Research, Inc., Lawrence, KS, 37 pp.

Demir, İ.; Güzelkücük, S.; and Sevim, Ö., 2018, “Effects of Sulfate on Cement Mortar with Hybrid Pozzolan Substitution,” Engineering Science and Technology, an International Journal, V. 21, No. 3, pp. 275-283.

Eberhardt, E., 2012, “The Hoek–Brown Failure Criterion,” The ISRM Suggested Methods for Rock Characterization, Testing and Monitoring: 2007-2014, pp. 233-240.

Erdem, R. T.; Ozturk, A. U.; and Gücüyen, E., 2016, “Estimarea Rezistentei la Compresune a Mortarelor de Cement/Estimation of Compressive Strength of Cement Mortars,” Revista Româna de Materiale, V. 46, No. 3, p. 313.

Haach, V. G.; Vasconcelos, G.; and Lourenço, P. B., 2011, “Influence of Aggregates Grading and Water/Cement Ratio in Workability and Hardened Properties of Mortars,” Construction and Building Materials, V. 25, No. 6, pp. 2980-2987. doi: 10.1016/j.conbuildmat.2010.11.011

Jiang, C.; Zhou, X.; Huang, S.; and Chen, D., 2016, “Influence of Polyacrylic Ester and Silica Fume on the Mechanical Properties of Mortar for Repair Application,” Advances in Mechanical Engineering, V. 9, No. 1, pp. 1-10. doi: 10.1177/1687814016683856

Jo, B. W.; Kim, C. H.; Tae, G. H.; and Park, J. B., 2007, “Characteristics of Cement Mortar with Nano-SiO2 Particles,” Construction and Building Materials, V. 21, No. 6, pp. 1351-1355. doi: 10.1016/j.conbuildmat.2005.12.020

Mahmood, W., and Mohammed, A., 2019, “New Vipulanandan p-q Model for Particle Size Distribution and Groutability Limits for Sandy Soils,” Journal of Testing and Evaluation, V. 48, No. 5.

Mebarkia, S., and Vipulanandan, C., 1992, “Compressive Behavior of Glass-Fiber Reinforced Polymer Concrete,” Journal of Materials in Civil Engineering, ASCE, V. 4, No. 1, pp. 91-105. doi: 10.1061/(ASCE)0899-1561(1992)4:1(91)

Mishra, S., and Deodhar, S. V., 2013, “Effect of Rice Husk Ash on Cement Mortar and Concrete,” New Building Materials and Construction World, V. 13, pp. 224-227.

Mohamadien, H. A., 2012, “The Effect of Marble Powder and Silica Fume as Partial Replacement for Cement on Mortar,” International Journal of Civil and Structural Engineering, V. 3, No. 2, p. 418

Mohammed, A., and Mahmood, W., 2018a, “Vipulanandan Failure Models to Predict the Tensile Strength, Compressive Modulus, Fracture Toughness and Ultimate Shear Strength of Calcium Rocks,” International Journal of Geotechnical Engineering, pp. 1-11.

Mohammed, A., and Mahmood, W., 2018b, “Statistical Variations and New Correlation Models to Predict the Mechanical Behavior and Ultimate Shear Strength of Gypsum Rock,” Open Engineering, V. 8, No. 1, pp. 213-226. doi: 10.1515/eng-2018-0026

Mohammed, A., and Vipulanandan, C., 2019, “Magnetic Field Strength and Temperature Effects on the Behavior of Oil Well Cement Slurry Modified with Iron Oxide Nanoparticles and Quantified with Vipulanandan Models,” Journal of Testing and Evaluation, V. 48, No. 6.

Mohammed, A. S., 2017, “Effect of Temperature on the Rheological Properties with Shear Stress Limit of Iron Oxide Nanoparticle Modified Bentonite Drilling Muds,” Egyptian Journal of Petroleum, V. 26, No. 3, pp. 791-802. doi: 10.1016/j.ejpe.2016.10.018

Mohammed, A. S., 2018a, “Electrical Resistivity and Rheological Properties of Sensing Bentonite Drilling Muds Modified with Lightweight Polymer,” Egyptian Journal of Petroleum, V. 27, No. 1, pp. 55-63. doi: 10.1016/j.ejpe.2017.01.002

Mohammed, A. S., 2018b, “Vipulanandan Models to Predict the Electrical Resistivity, Rheological Properties and Compressive Stress-Strain Behavior of Oil Well Cement Modified with Silica Nanoparticles,” Egyptian Journal of Petroleum, V. 27, No. 4, pp. 1265-1273. doi: 10.1016/j.ejpe.2018.07.001

Mohammed, A. S., 2019, “Vipulanandan Models to Predict the Mechanical Properties, Fracture Toughness, Pulse Velocity and Ultimate Shear Strength of Shale Rocks,” Geotechnical and Geological Engineering, V. 37, No. 2, pp. 625-638. doi: 10.1007/s10706-018-0633-5

Mohammed, A. S., and Vipulanandan, C., 2014, “Compressive and Tensile Behavior of Polymer Treated Sulfate Contaminated CL Soil,” Geotechnical and Geological Engineering, V. 32, No. 1, pp. 71-83. doi: 10.1007/s10706-013-9692-9

Muttar, A. A., and Salman, M. M., 2011, “Mechanical Properties of Acrylic Mortar,” Journal of Engineering and Sustainable Development, V. 15, No. 3, pp. 152-162.

Ozgurel, H. G., and Vipulanandan, C., 2005, “Effect of Grain Size and Distribution on Permeability and Mechanical Behavior of Acrylamide Grouted Sand,” Journal of Geotechnical and Geoenvironmental Engineering, ASCE, V. 131, No. 12, pp. 1457-1465. doi: 10.1061/(ASCE)1090-0241(2005)131:12(1457)

Rai, B.; Kumar, S.; and Satish, K., 2014, “Effect of Fly Ash on Mortar Mixes with Quarry Dust as Fine Aggregate,” Advances in Materials Science and Engineering, V. 2014, 7 pp. doi: 10.1155/2014/62642510.1155/2014/626425

Rathish, K. P., 2010, “High Performance Superplasticized Silica Fume Mortars for Ferrocement Works,” Facta Universitatis-Series: Architecture and Civil Engineering, V. 8, No. 2, pp. 129-134.

Rucińska, T., 2018, “Sustainable Cement Mortars,” E3S Web of Conferences, V. 49, p. 00090.

Seeger, A.; Brickmann, J.; and Luft, G., 2009, “Penetration of Organic Liquids into Dry Portland cement Mortar under Ambient and High Pressure,” Chemical Engineering & Technology: Industrial Chemistry‐Plant Equipment‐Process Engineering‐Biotechnology, V. 32, No. 6, pp. 891-902. doi: 10.1002/ceat.200900049

Sezer, G. İ., 2012, “Compressive Strength and Sulfate Resistance of Limestone and/or Silica Fume Mortars,” Construction and Building Materials, V. 26, No. 1, pp. 613-618. doi: 10.1016/j.conbuildmat.2011.06.064

Siddique, R., 2003, “Effect of Fine Aggregate Replacement with Class F Fly Ash on the Mechanical Properties of Concrete,” Cement and Concrete Research, V. 33, No. 4, pp. 539-547. doi: 10.1016/S0008-8846(02)01000-1

Türkel, S., and Altuntaş, Y., 2009, “The Effect of Limestone Powder, Fly Ash and Silica Fume on the Properties of Self-Compacting Repair Mortars,” Sadhana, V. 34, No. 2, pp. 331-343. doi: 10.1007/s12046-009-0011-3

Venkatarama Reddy, B. V., and Gupta, A., 2008, “Influence of Sand Grading on the Characteristics of Mortars and Soil–Cement Block Masonry,” Construction and Building Materials, V. 22, No. 8, pp. 1614-1623. doi: 10.1016/j.conbuildmat.2007.06.014

Villagrán Zaccardi, Y. A.; Fullea García, J.; Huélamo, P.; and Di Maio, A. A., 2009, “Influence of Temperature and Humidity on Portland Cement Mortar Resistivity Monitored with Inner Sensors,” Materials and Corrosion, V. 60, No. 4, pp. 294-299. doi: 10.1002/maco.200805075

Vipulanandan, C., and Mohammed, A., 2015a, “Smart Cement Modified with Iron Oxide Nanoparticles to Enhance the Piezoresistive Behavior and Compressive Strength for Oil Well Applications,” Smart Materials and Structures, V. 24, No. 12, p. 125020 doi: 10.1088/0964-1726/24/12/125020

Vipulanandan, C., and Mohammed, A., 2015b, “Smart Cement Rheological and Piezoresistive Behavior for Oil Well Applications,” Journal of Petroleum Science Engineering, V. 135, pp. 50-58. doi: 10.1016/j.petrol.2015.08.015

Vipulanandan, C., and Mohammed, A., 2015c, “XRD and TGA, Swelling and Compacted Properties of Polymer Treated Sulfate Contaminated CL Soil,” Journal of Testing and Evaluation, V. 44, No. 6, pp. 2270-2284.

Vipulanandan, C., and Mohammed, A., 2017, “Rheological Properties of Piezoresistive Smart Cement Slurry Modified with Iron-Oxide Nanoparticles for Oil-Well Applications,” Journal of Testing and Evaluation, V. 45, No. 6, pp. 2050-2060. doi: 10.1520/JTE20150443

Vipulanandan, C., and Mohammed, A., 2018, “Smart Cement Compressive Piezoresistive, Stress-Strain, and Strength Behavior with Nanosilica Modification,” Journal of Testing and Evaluation, V. 47, No. 2, pp. 1479-1501.

Vipulanandan, C., and Mohammed, A. S., 2014, “Hyperbolic Rheological Model with Shear Stress Limit for Acrylamide Polymer Modified Bentonite Drilling Muds,” Journal of Petroleum Science Engineering, V. 122, pp. 38-47. doi: 10.1016/j.petrol.2014.08.004

Vipulanandan, C., and Ozgurel, H. G., 2009, “Simplified Relationships for Particle-Size Distribution and Permeation Groutability Limits for Soils,” Journal of Geotechnical and Geoenvironmental Engineering, ASCE, V.  135, No. 9, pp. 1190-1197. doi: 10.1061/(ASCE)GT.1943-5606.0000064

Vipulanandan, C., and Paul, E., 1990, “Performance of Epoxy and Polyester Polymer Concrete,” ACI Materials Journal, V. 87, No. 3, May-June, pp. 241-251.

Wong, Y. L.; Lam, L.; Poon, C. S.; and Zhou, F. P., 1999, “Properties of Fly Ash-Modified Cement Mortar-Aggregate Interfaces,” Cement and Concrete Research, V. 29, No. 12, pp. 1905-1913. doi: 10.1016/S0008-8846(99)00189-1

Xu, A.; Sarkar, S. L.; and Nilsson, L. O., 1993, “Effect of Fly Ash on the Microstructure of Cement Mortar,” Materials and Structures, V. 26, No. 7, pp. 414-424. doi: 10.1007/BF02472942

Zelić, J.; Rušić, D.; Veža, D.; and Krstulović, R., 2000, “The Role of Silica Fume in the Kinetics and Mechanisms during the Early Stage of Cement Hydration,” Cement and Concrete Research, V. 30, No. 10, pp. 1655-1662. doi: 10.1016/S0008-8846(00)00374-4


ALSO AVAILABLE IN: