Title: 
            Assessment of Design Guidelines of Concrete Columns Reinforced with Glass Fiber-Reinforced Polymer Bars
        
        
            Author(s): 
            A. Hadhood, H. M. Mohamed, B. Benmokrane, A. Nanni, and C. K. Shield
        
        
            
                Publication: 
                Structural Journal
            
            
                Volume: 
                116
            
            
                Issue: 
                4
            
            
                Appears on pages(s): 
                193-207
            
            
                Keywords: 
                capacity; design guidelines; GFRP-RC column; GFRP reinforcement; stiffness; strength limit state
            
            
                DOI: 
                10.14359/51715663
            
        
        
            Date: 
            7/1/2019
        
        
            Abstract:
            Recent years have seen a great interest in testing concrete columns reinforced with glass fiber-reinforced-polymer bars (GFRP-RC). Yet, current codes and guidelines have not addressed the design of GFRP-RC columns. This paper aims at providing a set of recommendations and provisions based on analytical investigations, past knowledge about steel-reinforced concrete columns, and correlations with the experimental results from several studies of GFRP-RC columns. A database of 144 experiments was assembled; the results are reported and analyzed. The assembled database includes a selected number of parameters that can represent numerous practical cases. Based on this study, the calculation of the effective flexural stiffness (EIeff) was assessed with several equations and compared to experiments. As a result, a modified expression is recommended for EIeff at the factored load level. The design axial and flexural strengths were developed based on four approaches that were recently assessed with nominal and experimental results. It was found that the experimental-to-design strength ratio varied from 1.43 to 2.09. The minimum and maximum reinforcement limits were reviewed against the experimental results to ensure the integrity of the GFRP bars. In addition, the limits in the recent editions of ACI 318 and CSA A23.3 on steel transverse reinforcement (ties and spirals) were reviewed and modified to fulfill the performance requirements of GFRP tied and spirally reinforced columns.
        
     
    
    
    
            Related References:
                
                        ACI Committee 318, 2014, “Building Code Requirements for Structural Concrete (ACI 318-14) and Commentary (ACI 318R-14),” American Concrete Institute, Farmington Hills, MI, 520 pp.
                    
                        ACI Committee 440, 2015, “Guide for the Design and Construction of Concrete Reinforced with Fiber-Reinforced Polymer Bars (ACI 440.1R-15),” American Concrete Institute, Farmington Hills, MI, 88 pp.
                    
                        Afifi, M.; Mohamed, H. M.; and Benmokrane, B., 2014, “Axial Capacity of Circular Concrete Columns Reinforced with GFRP Bars and Spirals,” Journal of Composites for Construction, ASCE, V. 18, No. 1, p. 04013017 doi: 10.1061/(ASCE)CC.1943-5614.0000438
                    
                        Afifi, M. Z.; Mohamed, H. M.; and Benmokrane, B., 2015, “Theoretical Stress-Strain Model for Circular Concrete Columns Confined by GFRP Spirals and Hoops,” Engineering Structures, V. 102, No. 2015, pp. 202-213.
                    
                        Alsayed, S. H.; Al-Salloum, Y. A.; Almusallam, T. H.; and Amjad, M. A., 1999, “Concrete Columns Reinforced by GFRP Rods,” Fourth International Symposium on Fiber-Reinforced Polymer Reinforcement for Reinforced Concrete Structures, SP-188, C.W. Dolan, S. H. Rizkalla, and A. Nanni, eds., American Concrete Institute, Farmington Hills, MI, pp. 103-112.
                    
                        American Association of State Highway and Transportation Officials (AASHTO) LRFD, 2009, “Bridge Design Guide Specifications for GFRP-Reinforced Concrete Bridge Decks and Traffic Railings,” Washington, DC.
                    
                        CAN/CSA S6-06, 2014, “Canadian Highway Bridge Design Code,” Canadian Standards Association, Rexdale, ON, Canada.
                    
                        CAN/CSA S806-12, 2012, “Design and Construction of Building Components with Fiber Reinforced Polymers,” Canadian Standards Association, Rexdale, ON, Canada.
                    
                        Choo, C. C.; Harik, I. E.; and Gesund, H., 2006, “Minimum Reinforcement Ratio for Fiber-Reinforced Polymer-Reinforced Concrete Rectangular Columns,” ACI Structural Journal, V. 103, No. 3, May-June, pp. 460-466.
                    
                        De Luca, A.; Matta, F.; and Nanni, A., 2010, “Behavior of Full-Scale Glass Fiber-Reinforced Polymer Reinforced Concrete Columns under Axial Load,” ACI Structural Journal, V. 107, No. 5, Sept.-Oct., pp. 589-596.
                    
                        Elchalakani, M., and Ma, G., 2017, “Tests of Glass Fibre Reinforced Polymer Rectangular Concrete Columns Subjected to Concentric and Eccentric Axial Loading,” Engineering Structures, V. 151, pp. 93-104. doi: 10.1016/j.engstruct.2017.08.023
                    
                        Guérin, M.; Mohamed, H. M.; Benmokrane, B.; Nanni, A.; and Shield, C. K., 2018a, “Eccentric Behavior of Full-Scale Reinforced Concrete Columns with Glass Fiber-Reinforced Polymer Bars and Ties,” ACI Structural Journal, V. 115, No. 2, Mar., pp. 489-499. doi: 10.14359/51701107
                    
                        Guérin, M.; Mohamed, H. M.; Benmokrane, B.; Shield, C. K.; and Nanni, A., 2018b, “Effect of Glass Fiber-Reinforced Polymer Reinforcement Ratio on the Axial-Flexural Strength of Reinforced Concrete Columns,” ACI Structural Journal, V. 115, No. 4, July, pp. 1049-1062. doi: 10.14359/51701279
                    
                        Hadhood, A.; Mohamed, H. M.; and Benmokrane, B., 2017a, “Axial Load-Moment Interaction Diagram of Circular Concrete Columns Reinforced with CFRP Bars and Spirals: Experimental and Theoretical Investigations,” Journal of Composites for Construction, ASCE, V. 21, No. 2.
                    
                        Hadhood, A.; Mohamed, H. M.; and Benmokrane, B., 2017b, “Failure Envelope of Circular Concrete Columns Reinforced with GFRP Bars and Spirals,” ACI Structural Journal, V. 114, No. 6, Nov.-Dec., pp. 1417-1428. doi: 10.14359/51689498
                    
                        Hadhood, A.; Mohamed, H. M.; and Benmokrane, B., 2018a, “Assessing Stress-Block Parameters in Designing Circular High-Strength Concrete Members Reinforced with FRP Bars,” Journal of Structural Engineering, ASCE, V. 144, No. 10, p. 04018182 doi: 10.1061/(ASCE)ST.1943-541X.0002173
                    
                        Hadhood, A.; Mohamed, H. M.; and Benmokrane, B., 2018b, “Flexural Stiffness of GFRP- and CFRP-RC Circular Members under Eccentric Loads Based on Experimental and Curvature Analysis,” ACI Structural Journal, V. 115, No. 4, July, pp. 1185-1198. doi: 10.14359/51702235
                    
                        Hadhood, A.; Mohamed, H. M.; Ghrib, F.; and Benmokrane, B., 2017c, “Efficiency of Glass-Fiber Reinforced-Polymer (GFRP) Discrete Hoops and Bars in Concrete Columns under Combined Axial and Flexural Loads,” Composites. Part B, Engineering, V. 114, pp. 223-236. doi: 10.1016/j.compositesb.2017.01.063
                    
                        Hadi, M. N.; Karim, H.; and Sheikh, M. N., 2016, “Experimental Investigations on Circular Concrete Columns Reinforced with GFRP Bars and Helices under Different Loading Conditions,” Journal of Composites for Construction, ASCE, V. 20, No. 4, p. 04016009 doi: 10.1061/(ASCE)CC.1943-5614.0000670
                    
                        Hadi, M. N., and Youssef, J., 2016, “Experimental Investigation of GFRP-Reinforced and GFRP-Encased Square Concrete Specimens under Axial and Eccentric Load, and Four-Point Bending Test,” Journal of Composites for Construction, ASCE, V. 20, No. 5, p. 04016020 doi: 10.1061/(ASCE)CC.1943-5614.0000675
                    
                        Hales, T. A.; Pantelides, C. P.; Sankholkar, P.; and Reaveley, L. D., 2017, “Analysis-Oriented Stress-Strain Model for Concrete Confined with Fiber-Reinforced Polymer Spirals,” ACI Structural Journal, V. 114, No. 5, Sept.-Oct., pp. 1263-1272. doi: 10.14359/51689788
                    
                        Karim, H.; Sheikh, M. N.; and Hadi, M. N., 2017, “Longitudinal Reinforcement Limits for Fiber-Reinforced Polymer Reinforced Concrete Members,” ACI Structural Journal, V. 114, No. 3, May-June, pp. 687-696. doi: 10.14359/51689439
                    
                        Khorramian, K., and Sadeghian, P., 2017, “Experimental and Analytical Behavior of Short Concrete Columns Reinforced with GFRP Bars under Eccentric Loading,” Engineering Structures, V. 151, pp. 761-773. doi: 10.1016/j.engstruct.2017.08.064
                    
                        Mander, J. B.; Priestley, M. J.; and Park, R., 1988, “Theoretical Stress-Strain Model for Confined Concrete,” Journal of Structural Engineering, ASCE, V. 114, No. 8, pp. 1804-1826. doi: 10.1061/(ASCE)0733-9445(1988)114:8(1804)
                    
                        Mohamed, H. M.; Afifi, M.; and Benmokrane, B., 2014, “Performance Evaluation of Concrete Columns Reinforced Longitudinally with FRP Bars and Confined with FRP Hoops and Spirals under Axial Load,” Journal of Bridge Engineering, ASCE, V. 19, No. 7, p. 04014020 doi: 10.1061/(ASCE)BE.1943-5592.0000590
                    
                        Nanni, A.; De Luca, A.; and Zadeh, H., 2014, Reinforced Concrete with FRP Bars: Mechanics and Design, CRC Press, Boca Raton, FL.
                    
                        Pantelides, C. P.; Gibbons, M. E.; and Reaveley, L. D., 2013, “Axial Load Behavior of Concrete Columns Confined with GFRP Spirals,” Journal of Composites for Construction, ASCE, V. 17, No. 3, pp. 305-313. doi: 10.1061/(ASCE)CC.1943-5614.0000357
                    
                        Prachasaree, W.; Piriyakootorn, S.; Sangsrijun, A.; and Limkatanyu, S., 2015, “Behavior and Performance of GFRP Reinforced Concrete Columns with Various Types of Stirrups,” International Journal of Polymer Science, V. 2015, 9 pp.
                    
                        Richart, F. E., 1933, “Reinforced Concrete Column Investigation,” ACI Journal Proceedings, V. 29, No. 2, Feb., pp. 275-284.
                    
                        Saatcioglu, M., and Razvi, S. R., 1992, “Strength and Ductility of Confined Concrete,” Journal of Structural Engineering, ASCE, V. 118, No. 6, pp. 1590-1607. doi: 10.1061/(ASCE)0733-9445(1992)118:6(1590)
                    
                        Sankholkar, P. P.; Pantelides, C. P.; and Hales, T. A., 2018, “Confinement Model for Concrete Columns Reinforced with GFRP Spirals,” Journal of Composites for Construction, ASCE, V. 22, No. 3, p. 04018007 doi: 10.1061/(ASCE)CC.1943-5614.0000843
                    
                        Shield, C. K.; Galambos, T. V.; and Gulbrandsen, P., 2011, “On the History and Reliability of the Flexural Strength of FRP Reinforced Concrete Members in ACI 440.1 R,” Fiber-Reinforced Polymer Reinforcement for Concrete Structures—10th International Symposium, SP-275, American Concrete Institute, Farmington Hills, MI, pp. 1-18. 
                    
                        Szerszen, M. M., and Nowak, A. S., 2003, “Calibration of Design Code for Buildings (ACI 318): Part 2—Reliability Analysis and Resistance Factors,” ACI Structural Journal, V. 100, No. 3, May-June, pp. 383-391.
                    
                        Tikka, T.; Francis, M.; and Teng, B., 2010, “Strength of Concrete Beam-Columns Reinforced with GFRP Bars,” 2nd International Structures Specialty Conference, Winnipeg, MB, Canada, pp. 46.1-46.10.
                    
                        Tobbi, H.; Farghaly, A. S.; and Benmokrane, B., 2012, “Concrete Columns Reinforced Longitudinally and Transversally with Glass Fiber-Reinforced Polymers Bars,” ACI Structural Journal, V. 109, No. 4, July-Aug., pp. 551-558.
                    
                        Tobbi, H.; Farghaly, A. S.; and Benmokrane, B., 2014, “Behavior of Concentrically Loaded Fiber-Reinforced Polymer Reinforced Concrete Columns with Varying Reinforcement Types and Ratios,” ACI Structural Journal, V. 111, No. 2, Mar.-Apr., pp. 375-385.
                    
                        Xue, W.; Peng, F.; and Fang, Z., 2018, “Behavior and Design of Slender Rectangular Concrete Columns Longitudinally Reinforced with Fiber-Reinforced Polymer Bars,” ACI Structural Journal, V. 115, No. 2, Mar., pp. 311-322. doi: 10.14359/51701131
                    
                        Zadeh, H., and Nanni, A., 2013a, “Design of RC Columns Using Glass FRP Reinforcement,” Journal of Composites for Construction, ASCE, V. 17, No. 3, pp. 294-304. doi: 10.1061/(ASCE)CC.1943-5614.0000354
                    
                        Zadeh, H., and Nanni, A., 2013b, “Reliability Analysis of Concrete Beams Internally Reinforced with Fiber-Reinforced Polymer Bars,” ACI Structural Journal, V. 110, No. 6, pp. 1023-1032.
                    
                        Zadeh, H. J., and Nanni, A., 2017, “Flexural Stiffness and Second-Order Effects in Fiber-Reinforced Polymer-Reinforced Concrete Frames,” ACI Structural Journal, V. 114, No. 2, Mar.-Apr., pp. 533-544. doi: 10.14359/51689257