Title: Structural Behavior of Precast Reinforced Concrete Shear Walls with Large-Diameter Bars

Author(s): Xin Chen, Ming Liu, Fabio Biondini, and Gianpaolo Rosati

Publication: Structural Journal

Volume: 116

Issue: 5

Appears on pages(s): 77-86

Keywords: experimental tests; large-diameter bars; nonlinear finite element analysis; precast shear walls; structural behavior

DOI: 10.14359/51715657

Date: 9/1/2019

Abstract:
A series of four precast concrete shear walls with large-diameter reinforcing steel bars or uniformly reinforced were assembled with grouting anchors and tested to failure under cyclic loading. Extensive experimental tests were performed to investigate bearing capacity and displacement ductility. Results show that the tested precast walls with few large-diameter reinforcing bars have more evident flag behavior with wider cycles and higher strength compared with small-diameter uniformly reinforced shear walls. Finite element analyses are performed to simulate the structural behavior of the investigated walls. The obtained skeleton curves are compared with the experimental results to validate the structural model. Finally, some suggestions for seismic design of precast shear wall structures assembled with large-diameter reinforcing bars are provided.


ALSO AVAILABLE IN:

Electronic Structural Journal



  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

Edit Module Settings to define Page Content Reviewer