Internally Cured High-Performance Concrete Slabs Reinforced with Glass Fiber-Reinforced Polymer

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Internally Cured High-Performance Concrete Slabs Reinforced with Glass Fiber-Reinforced Polymer

Author(s): Yail J. Kim and Junhao Gao

Publication: Structural Journal

Volume: 116

Issue: 5

Appears on pages(s): 43-54

Keywords: fiber-reinforced polymer (FRP); internal curing; one-way slab; performance

DOI: 10.14359/51715574

Date: 9/1/2019

Abstract:
This paper presents a new concept of high-performance structures composed of internally cured concrete and glass fiber-reinforced polymer (GFRP) reinforcement. The former addresses autogenous shrinkage that leads to premature cracking of concrete, and the latter provides a noncorrosive service environment. Presaturated superabsorbent polymer (SAP) is mixed with concrete at 0 to 0.4% of the cement mass to facilitate a hydration process. The swelling kinetics of SAP due to water absorption is quantified, and its releasing rate with time is determined. A total of 15 one-way slabs are tested in flexure to examine the effects of SAP inclusions. The behavior of the slabs is assessed by deterministic and stochastic models with an emphasis on tension stiffening and performance reliability. The amount of the internal curing agent affects the strength of the concrete and the response of the slabs. Various cracks are observed when the slabs are loaded, including flexural, horizontal splitting, and diagonal tension cracks. As the amount of SAP increases, the cracks become localized and expedite the failure of the slabs. The tension stiffening of control slabs (0%SAP) is more pronounced than that of the slabs with SAP. The cumulative degradation probability and the risk level of the slabs made of the internally cured concrete are controlled by the amount of SAP.

Related References:

1. American Concrete Institute, “ACI Concrete Terminology (ACI CT-16),” American Concrete Institute, Farmington Hills, MI, 2016, 80 pp.

2. Cusson, D.; Lounis, Z.; and Daigle, L., “Benefits of Internal Curing on Service Life and Life-Cycle Cost of High-Performance Concrete Bridge Decks—A Case Study,” Cement and Concrete Composites, V. 32, No. 5, 2010, pp. 339-350. doi: 10.1016/j.cemconcomp.2010.02.007

3. Zhutovsky, S., and Kovler, K., “Effect of Internal Curing on Durability-Related Properties of High-Performance Concrete,” Cement and Concrete Research, V. 42, No. 1, 2012, pp. 20-26. doi: 10.1016/j.cemconres.2011.07.012

4. Soliman, A. M., and Nehdi, M. L., “Effects of Shrinkage Reducing Admixture and Wollastonite Microfiber on Early-Age Behavior of Ultra-High-Performance Concrete,” Cement and Concrete Composites, V. 46, 2014, pp. 81-89. doi: 10.1016/j.cemconcomp.2013.11.008

5. RILEM, “Internal Curing of Concrete: State-of-the-Art Report of RILEM Technical Committee 196-ICC,” International Union of Laboratories and Experts in Construction Materials, Systems, and Structures, Paris, France, 2007.

6. ACI Committees 213 and 308, “Report on Internally Cured Concrete Using Prewetted Absorptive Lightweight Aggregate (ACI 308-213R-13),” American Concrete Institute, Farmington Hills, MI, 2013, 12 pp.

7. Jensen, O. M., and Hansen, P. F., “Water-Entrained Cement-Based Materials—II. Experimental Observations,” Cement and Concrete Research, V. 32, No. 6, 2002, pp. 973-978. doi: 10.1016/S0008-8846(02)00737-8

8. Pourjavadi, A.; Fakoorpoor, S. M.; Khaloo, A.; and Hosseini, P., “Improving the Performance of Cement-Based Composites Containing Superabsorbent Polymers by Utilization of Nano-SiO2 particles,” Materials and Design, V. 42, 2012, pp. 94-101. doi: 10.1016/j.matdes.2012.05.030

9. Craeye, B.; Geirnaert, M.; and De Schutter, G., “Super Absorbing Polymer as an Internal Curing Agent for Mitigation of Early-Age Cracking of High-Performance Concrete Bridge Decks,” Construction and Building Materials, V. 25, No. 1, 2011, pp. 1-13. doi: 10.1016/j.conbuildmat.2010.06.063

10. Mechtcherine, V., and Reinhardt, H.-W., Application of Superabsorbent Polymers (SAP) in Concrete Construction, Springer, Dordrecht, the Netherlands, 2012.

11. Nkurunziza, G.; Debaiky, A.; Cousin, P.; and Benmokrane, B., “Durability of GFRP Bars: A Critical Review of the Literature,” Progress in Structural Engineering and Materials, V. 7, No. 4, 2005, pp. 194-209. doi: 10.1002/pse.205

12. Ahmed, E. A.; El-Salakawy, E. F.; and Benmokrane, B., “Performance Evaluation of Glass Fiber-Reinforced Polymer Shear Reinforcement for Concrete Beams,” ACI Structural Journal, V. 107, No. 1, Jan.-Feb. 2010, pp. 53-62.

13. Kharal, Z., and Sheikh, S., “Tension Stiffening and Cracking Behavior of Glass Fiber-Reinforced Polymer Reinforced Concrete,” ACI Structural Journal, V. 114, No. 2, Mar.-Apr. 2017, pp. 299-310.

14. AASHTO, “Guide Specifications for GFRP-Reinforced Concrete Bridge Decks and Traffic Railing,” American Association of State Highway Transportation Officials, Washington, DC, 2009.

15. ACI Committee 440, “Guide for the Design and Construction of Structural Concrete Reinforced with Fiber-Reinforced Polymer (FRP) Bars (ACI 440.1R-15),” American Concrete Institute, Farmington Hills, MI, 2015, 88 pp.

16. Zhutovsky, S.; Kovler, K.; and Bentur, A., “Efficiency of Lightweight Aggregates for Internal Curing of High Strength Concrete to Eliminate Autogenous Shrinkage,” Materials and Structures, V. 35, No. 2, 2002, pp. 97-101. doi: 10.1007/BF02482108

17. Bentz, D. P., “Influence of Internal Curing Using Lightweight Aggregates on Interfacial Transition Zone Percolation and Chloride Ingress in Mortars,” Cement and Concrete Composites, V. 31, No. 5, 2009, pp. 285-289. doi: 10.1016/j.cemconcomp.2009.03.001

18. Koch, G. H.; Brongers, M. P. H.; Thompson, N. G.; Virmani, Y. P.; and Payer, J. H., “Corrosion Cost and Preventive Strategies in the United States,” Report No. FHWA-RD-01-156, Federal Highway Administration, Washington, DC, 2002.

19. ASTM C192/C192M-16a, “Standard Practice For Making and Curing Concrete Test Specimens In The Laboratory,” ASTM International, West Conshohocken, PA, 2016, 8 pp.

20. Ferreira, T., and Rashband, W., The ImageJ User Guide, National Institute of Health, Bethesda, MD, 2012.

21. Buchholz, F. L., Absorbency and Superabsorbency: Modern Superabsorbent Polymer Technology, Wiley, New York, 1998, pp. 1-18.

22. Kinney, A. B., and Scranton, A. B., “Formation and Structure of Cross-linked Polyacrylates,” ACS Symposium Series, 1994, pp. 2-26.

23. Hu, W., Polymer Physics: A Molecular Approach, Springer, Berlin, Germany, 2013.

24. Zhu, Q.; Barney, C. W.; and Erk, K. A., “Effect of Ionic Crosslinking on the Swelling and Mechanical Response of Model Superabsorbent Polymer Hydrogels for Internally Cured Concrete,” Materials and Structures, V. 48, No. 7, 2015, pp. 2261-2276. doi: 10.1617/s11527-014-0308-5

25. Esteves, L. P., “Superabsorbent Polymers: On Their Interaction with Water and Pore Fluid,” Cement and Concrete Composites, V. 33, No. 7, 2011, pp. 717-724. doi: 10.1016/j.cemconcomp.2011.04.006

26. Shen, C. H., and Springer, G. S., “Moisture Absorption and Desorption of Composite Materials,” Journal of Composite Materials, V. 10, No. 1, 1976, pp. 2-20. doi: 10.1177/002199837601000101

27. Britton, L. N.; Ashman, R.-B.; Aminahhavi, T. M.; and Cassidy, P. E., “Prediction of Transport Properties of Permeants through Polymer Films,” Journal of Chemical Education, V. 65, No. 4, 1988, pp. 368-370. doi: 10.1021/ed065p368

28. Neville, A. M., Properties of Concrete, fourth edition, Prentice Hall, Essex, UK, 1995.

29. Wood, S. L., “Evaluation of the Long-Term Properties of Concrete,” ACI Materials Journal, V. 88, No. 6, Nov.-Dec. 1991, pp. 630-643.

30. El-Sayed, A.; El-Salakawy, E.; and Benmokrane, B., “Shear Strength of One-Way Concrete Slabs Reinforced with Fiber-Reinforced Polymer Composite Bars,” Journal of Composites for Construction, ASCE, V. 9, No. 2, 2005, pp. 147-157. doi: 10.1061/(ASCE)1090-0268(2005)9:2(147)

31. ACI Committee 318, “Building Code Requirements for Structural Concrete (ACI 318-14) and Commentary (ACI 318R-14),” American Concrete Institute, Farmington Hills, MI, 2014, 520 pp.

32. McKay, M. D.; Beckman, R. J.; and Conover, W. J., “A Comparison of Three Methods for Selecting Values of Input Variables in the Analysis of Output from a Computer Code,” Technometrics, V. 21, No. 2, 1979, pp. 239-245.

33. Bischoff, P. H., “Deflection Calculation of FRP Reinforced Concrete Beams Based on Modifications to the Existing Branson Equation,” Journal of Composites for Construction, ASCE, V. 11, No. 1, 2007, pp. 4-14. doi: 10.1061/(ASCE)1090-0268(2007)11:1(4)

34. Madsen, H. O.; Krenk, S.; and Lind, N. C., Methods of Structural Safety, Dover Publications, Mineola, NY, 2006.

35. Weibull, W., “A Statistical Theory of the Strength of Materials,” The Royal Swedish Institute, Stockholm, Sweden, 1939.

36. Foster, S. J.; Stewart, M. G.; Loo, M.; Ahammed, M.; and Sirivivatnanon, V., “Calibration of Australian Standard AS3600 Concrete Structures: Part I Statistical Analysis of Material Properties and Model Error,” Australian Journal of Structural Engineering, V. 17, No. 4, 2016, pp. 242-253. doi: 10.1080/13287982.2016.1246793

37. Okeil, A. M.; El-Tawil, S.; and Shahawy, M., “Flexural Reliability of Reinforced Concrete Bridge Girders Strengthened with Carbon Fiber-Reinforced Polymer Laminates,” Journal of Bridge Engineering, ASCE, V. 7, No. 5, 2002, pp. 290-299. doi: 10.1061/(ASCE)1084-0702(2002)7:5(290)

38. Hamutçuoğlu, O. M., and Scott, M. H., “Finite Element Reliability Analysis of Bridge Girders Considering Moment-Shear Interaction,” Structural Safety, V. 31, No. 5, 2009, pp. 356-362. doi: 10.1016/j.strusafe.2009.02.003

39. Kulkarni, S. N., “Calibration of Flexural Design of Concrete Members Reinforced with FRP Bars,” MS thesis, Louisiana State University, Baton Rouge, LA, 2006.

40. Neocleous, K.; Pilakoutas, K.; and Waldron, P., “Flexural Behaviour of Over-Reinforced FRP RC Beams: Effect of Design Parameters and Material Partial Safety Factors,” Fibre-reinforced Plastics for Reinforced Concrete Structures (FRPRCS-5), 2001, pp. 71-78.


ALSO AVAILABLE IN:

Electronic Structural Journal