Experimental Study and Analytical Modeling on Fatigue Properties of Pervious Concrete Made with Natural and Recycled Aggregates

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Experimental Study and Analytical Modeling on Fatigue Properties of Pervious Concrete Made with Natural and Recycled Aggregates

Author(s): Xudong Chen, Dandan Shi, Nan Shen, Shengtao Li and Saisai Liu

Publication: IJCSM

Volume: 13

Issue:

Appears on pages(s):

Keywords: pervious concrete, recycled aggregate, fracture parameter, plastic strain, fatigue life prediction

DOI: 10.1186/s40069-018-0305-0

Date: 1/31/2019

Abstract:
As a solid pollutant, the recycled aggregate can be reused to replace the natural aggregate to cast pervious concrete, promoting resource recycling and reducing environmental pollution. Pervious concrete is usually applied to trans-portation engineering as pavements and decks, which are often subjected to fatigue loads in service. Therefore, it is essential to investigate the fatigue mechanical properties of pervious concrete. In this study, four-point cyclic bending loading test of natural aggregate pervious concrete and recycled aggregate pervious concrete were conducted under four different stress levels. By analyzing the experimental results, the mechanical performances, including hysteresis curve characteristics, damping ratio, dynamic elastic modulus and cyclic strain, of two kinds of pervious concrete under cyclic loading were revealed. Based on the improved EPF model, the relationship between fracture parameters, plastic strain and unloading strain were obtained. Besides, the relationship between the loading cycles and the ratio of plastic strain to unloading strain was received according to fatigue testing data under different stress levels. Further, the simplified fatigue model of pervious concrete was proposed and the experimental data was fitted with the model results. The fitting result reached a good agreement.